Review of Key Parameters Affecting Punching Shear Strength of Post-Tensioned Slabs

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Review of Key Parameters Affecting Punching Shear Strength of Post-Tensioned Slabs

Author(s): Madhura Sanjay Chavan and Mary Beth Hueste

Publication: Symposium Paper

Volume: 357

Issue:

Appears on pages(s): 41-61

Keywords: Direct shear, experimental database, flat slabs, post-tensioned concrete, punching shear, reinforcement ratio, slab-column connections

DOI: 10.14359/51738758

Date: 4/1/2023

Abstract:
Experimental tests have been performed on interior post-tensioned (PT) slab-column (SC) connections over the past several decades. This paper presents a comprehensive database of 92 such tests performed on interior PT SC connections without shear reinforcement under direct shear. The data was then analyzed to compare the accuracy of the punching shear provisions of ACI 318-19, Eurocode 2 (2004), and CSA A23-19. Several key parameters were evaluated for the PT SC specimens including the concrete compressive strength, specimen geometry, bonded flexural reinforcement ratio, and minimum area of bonded flexural reinforcement; and their influence on the two-way shear strength of these connections was studied. Recommendations are made for possible modifications to the provisions of ACI 318-19 including the limit on the value of the concrete compressive strength f_c^'. Areas for further study, including size effect and bonded flexural reinforcement requirements, are highlighted.

Related References:

ACI Committee 318, 2019, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary,” American Concrete Institute, Farmington Hill, MI, 623 pp.

ACI-ASCE Committee 423, 2017, “Recommendations for Concrete Members Prestressed with Unbonded Tendons (423.3R-17),” American Concrete Institute, Farmington Hill, MI.

ACI-ASCE Committee 423, 1974, “Tentative Recommendations for Prestressed Concrete Flat Plates,” ACI Journal Proceedings, 71(2), Feb., pp. 67-71.

ACI-ASCE Committee 423, 1958, “Tentative Recommendations for Prestressed Concrete,” ACI Journal Proceedings, 54(7), Jan., pp. 545-578.

BS EN 1992-1-1-:2004, 2004, “Design of Concrete Structures—Part 1-1: General Rules and Rules for Buildings,” Eurocode 2, British Standards Institution, London.

Burns, N. H.; and Hemakom, R., 1977, “Test of Scale Model Post-Tensioned Flat Plate,” Journal of Structural Engineering, ASCE, 103(6), pp. 1237-1255.

Canadian Standards Association (CSA), 2019, “Design of Concrete Structures (CSA A23.3-19),” CSA Group, Rexdale, ON, Canada, 298 pp.

Corrêa, G. S., 2001, “Puncionamento em Lajes Cogumelo Protendidas com Cabos Não Aderentes,” MSc dissertation, Department of Civil and Environmental Engineering, University of Brasília, Brasília, Brazil, 153 pp.

Franklin, S. O.; and Long, A. E., 1982, “The Punching Behaviour of Unbonded Post-Tensioned Flat Plates,” Proceeding of the Institution of Civil Engineers, Part 2, 73, pp. 609-631.

Gardner, N. J.; and Kallage, M. R., 1998, “Punching shear strength of continuous post-tensioned concrete flat plates,” Materials Journal, 95(3), 272-283.

Gerber, L. L.; and Burns, N. H., 1971, “Ultimate Strength Tests of Post-Tensioned Flat Plates,” PCI Journal, 16(6), pp. 40-58.

Hassanzadeh, G., 1998, “Betongplattor pa Pelare, Dimensionerings Metoder för Plattor Med Icke Vidhäftande Spännarmering,” TRITA-BKN Bulletin 43, Institutionen för Byggkonstruktion, Kungl-Tekniska Högskolan, Stockholm, Sweden, pp. 110-130.

Hawkins, N. M.; and Ospina, C. E., 2017, “Effect of slab flexural reinforcement and depth on punching strength,” SP-315, 117-140.

Kordina, K.; and Nölting, D., 1984, “Versuche zum Durchstanzen ohne Verbund Vorgespannter Flachdecken,” Lehrstuhl für Massivbau, Technische Universität, Braunschweig, Germany, 59 pp.

Kordina, K.; and Nölting, D., 1986, “Tragfähigkeit durchstanzgefährdeter stahlbetonplatten,” Deutscher Ausschuss für Stahlbeton, Berlin, Germany, 60 pp.

Kosut, G. M.; Burns, N. H.; and Winter, C. V., 1985, “Test of Four-Panel Post-Tensioned Flat Plate,” Journal of the Structural Division, ASCE, 111(9), pp. 1916-1929.

Melges, J. L. P., 2000, “Análise Experimental da Punção em Lajes de Concreto Armado e Protendido,” PhDEng thesis, Escola de Engenharia de São Carlos, Universidade de São Paulo, São Carlos, Brasil, 350 pp.

Naaman, A. E., 2012, “Prestressed concrete analysis and design: Fundamentals,” New York: McGraw-Hill, pp. 360-364.

Nylander, H.; Kinnunen, S.; and Ingvarsson, H., 1977 “Genomstansning av pelarunderstödd plattbro av betong med spänd och ospänd armering,” Test report KTH, No. 123, Stockholm.

Pralong, J.; Brändli, W.; and Thürlimann, B., 1979, “Durchstanzersuche an Stahlbeton und Spannbetonplatten, Birkhäuser Verlag,” Institute of Structural Engineering, Swiss federal Institute of Technology Zurich, No. 7305-3.

Ragab, M. S.; Riad, K. H.; and Zaher, A. H., 2014, “Punching behavior of post-tensioned high strength concrete slabs,” World Applied Sciences Journal, 32(4), 527-539.

Rahman, A. H., 1992, “Effect of Steel Corrosion on the Strength of Slab-Column Connections,” National Research Council Canada, 20 pp.

Ramos, A. P.; Lúcio, V.; and Regan, P. E., 2011 “Punching of flat slabs with in-plane force,” Engineering Structures, 33(3).

Regan, P. E., 1983 “Punching Shear in Prestressed Concrete Slab Bridges,” Engineering Structures Research group, Polytechnic of Central London, London.

Scordelis, A. C.; Lin, T. Y.; and Itaya, R., 1959, “Behaviour of a Continuous Slab Prestressed in Two Directions,” ACI Journal Proceedings, 56(12), pp. 441-459.

Scordelis, A. S.; Lin, T. Y.; and May, H. R., 1958, “Shearing Strength of Prestressed Lift Slabs,” ACI Journal, Proceedings 55(10), pp. 485-506.

Shehata, I. A., 1982, “Punching of Prestressed and Non-Prestressed Reinforced Concrete Flat Slabs,” MPhil thesis, Polytechnic of Central London, London, 336 pp.

Silva, R. J. C., 2004, “Punção em Lajes Cogumelo Protendida,” PhD thesis, Department of Civil and Environmental Engineering, University of Brasília, Brasília, Brasil, 223 pp.