ACI SPEC-440.5-22: Construction with Glass Fiber-Reinforced Polymer Reinforcing Bars—Specification (SI Units)

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ACI SPEC-440.5-22: Construction with Glass Fiber-Reinforced Polymer Reinforcing Bars—Specification (SI Units)

Author(s): ACI Committee 440

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 10

Keywords:

DOI:

Date: 3/1/2023

Abstract:
This Specification covers construction of concrete members internally reinforced with glass fiber-reinforced polymer reinforcing bars. Keywords: concrete construction; fiber-reinforced polymer reinforcement; placing; tolerance.