Behavior of NiTi Shape Memory Alloy- and Steel- Reinforced Shear Walls Repaired with Engineered Cementitious Composite

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of NiTi Shape Memory Alloy- and Steel- Reinforced Shear Walls Repaired with Engineered Cementitious Composite

Author(s): Michael A. Soto-Rojas, Anca C. Ferche, and Dan Palermo

Publication: Structural Journal

Volume: 120

Issue: 4

Appears on pages(s): 207-222

Keywords: energy dissipation; engineered cementitious composite (ECC); nickel-titanium (NiTi); recovery capacity; reinforced concrete; repair; shape memory alloys (SMAs); shear walls

DOI: 10.14359/51738745

Date: 7/1/2023

Abstract:
This paper presents the results of an experimental study investigating the response of two shear walls repaired with engineered cementitious composite (ECC). One of the walls was reinforced in the boundary regions within the plastic hinge with superelastic, nickel-titanium (NiTi) shape memory alloy (SMA) bars, while the companion wall was reinforced with deformed mild steel bars only. The repair method involved the removal of the heavily damaged concrete in the plastic hinge zone, replacement of ruptured and buckled steel reinforcement, placement of starter bars at the baseof the walls, and casting of ECC to replace the removed concrete. The SMA bars were reused as they sustained no damage from the initial testing. Summarized in this paper are an assessment of the performance of the repaired walls and a comparison with the responses of the walls previously tested in their original condition. The experimental program highlights the enhanced performance of the composite system that integrates the self-centering capabilities of SMA bars and the distinctive tension strain hardening and ductility of ECC. The lateral strength was markedly increased, while the energy dissipation and recovery capacities, in general, were improved for the repaired walls compared to the original walls. The repaired steel-reinforced wall developed a peak lateral strength of 23% larger compared to the original wall, whilethe repaired SMA-reinforced wall had a 16% increase in peaklateral strength compared to the original specimen. The strength enhancement of the repaired walls led to higher dissipated energy throughout testing. For both sets of walls, the SMA-reinforced walls exhibited larger rotations compared to the steel-reinforced walls primarily on account of the lower stiffness of the SMA bars.

Related References:

1. EN 1998-1:2004, “Eurocode 8: Design of Structures for Earthquake Resistance—Part 1: General Rules, Seismic Actions and Rules for Buildings,” European Committee for Standardization, Brussels, Belgium, 2004, 231 pp.

2. FEMA P-1050, “NEHRP Recommended Seismic Provisions for New Buildings and Other Structures,” Building Seismic Safety Council, Washington, DC, 2015.

3. Joint ACI-ASCE Committee 441, “High-Strength Concrete Columns: State of the Art (ACI 441R-96),” American Concrete Institute, Farmington Hills, MI, 1996, 13 pp.

4. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

5. Wallace, J. W.; Massone, L. M.; Bonelli, P.; Dragovich, J.; Lagos, R.; Lüders, C.; and Moehle, J., “Damage and Implications for Seismic Design of RC Structural Wall Buildings,” Earthquake Spectra, V. 28, No. 1_suppl1, June 2012, pp. 281-299. doi: 10.1193/1.4000047

6. Elwood, K. J., “Performance of Concrete Buildings in the 22 February 2011 Christchurch Earthquake and Implications for Canadian Codes,” Canadian Journal of Civil Engineering, V. 40, No. 8, Aug. 2013, pp. 759-776. doi: 10.1139/cjce-2011-0564

7. Pan, Z.; Wu, C.; Liu, J.; Wang, W.; and Liu, J., “Study on Mechanical Properties of Cost-Effective Polyvinyl Alcohol Engineered Cementitious Composites (PVA-ECC),” Construction and Building Materials, V. 78, Mar. 2015, pp. 397-404. doi: 10.1016/j.conbuildmat.2014.12.071

8. Mohammed, B. S.; Nuruddin, M. F.; Aswin, M.; Mahamood, N.; and Al-Mattarneh, H., “Structural Behavior of Reinforced Self-Compacted Engineered Cementitious Composite Beams,” Advances in Materials Science and Engineering, V. 2016, 2016, Article No. 5615124, 12 pp. doi: 10.1155/2016/5615124

9. Abdulridha, A., and Palermo, D., “Behaviour and Modelling of Hybrid SMA-Steel Reinforced Concrete Slender Shear Wall,” Engineering Structures, V. 147, Sept. 2017, pp. 77-89. doi: 10.1016/j.engstruct.2017.04.058

10. Morcos, M., and Palermo, D., “SMA-Reinforced Concrete Shear Walls Subjected to Reverse Cyclic Loading,” Proceedings of the Fifth International Conference on Smart Monitoring, Assessment and Rehabilitation of Civil Structures (SMAR 2019), Aug. 2019, Potsdam, Germany, 2019, 8 pp.

11. Morcos, M., and Palermo, D., “Numerical Modelling of Slender Superelastic-Shape Memory Alloy Reinforced Concrete Shear Walls,” Proceedings of 6th International Structural Specialty Conference (CSCE 2018), K. Arjomandi and A. El Damatty, eds., Fredericton, NB, Canada, June 2018, pp. 528-538.

12. Cortés-Puentes, L.; Zaidi, M.; Palermo, D.; and Dragomirescu, E., “Cyclic Loading Testing of Repaired SMA and Steel Reinforced Concrete Shear Walls,” Engineering Structures, V. 168, Aug. 2018, pp. 128-141. doi: 10.1016/j.engstruct.2018.04.044

13. Saiidi, M. S.; O’Brien, M.; and Sadrossadat-Zadeh, M., “Cyclic Response of Concrete Bridge Columns Using Superelastic Nitinol and Bendable Concrete,” ACI Structural Journal, V. 106, No. 1, Jan.-Feb. 2009, pp. 69-77.

14. Abdulridha, A.; Palermo, D.; Foo, S.; and Vecchio, F. J., “Behavior and Modeling of Superelastic Shape Memory Alloy Reinforced Concrete Beams,” Engineering Structures, V. 49, Apr. 2013, pp. 893-904. doi: 10.1016/j.engstruct.2012.12.041

15. Saiidi, M. S., and Wang, H., “Exploratory Study of Seismic Response of Concrete Columns with Shape Memory Alloys Reinforcement,” ACI Structural Journal, V. 103, No. 3, May-June 2006, pp. 436-443.

16. Youssef, M. A.; Alam, M. S.; and Nehdi, M., “Experimental Investigation on the Seismic Behavior of Beam-Column Joints Reinforced with Superelastic Shape Memory Alloys,” Journal of Earthquake Engineering, V. 12, No. 7, 2008, pp. 1205-1222. doi: 10.1080/13632460802003082

17. Nehdi, M.; Alam, M. S.; and Youssef, M. A., “Seismic Behaviour of Repaired Superelastic Shape Memory Alloy Reinforced Concrete Beam-Column Joint,” Smart Structures and Systems, V. 7, No. 5, 2011, pp. 329-348. doi: 10.12989/sss.2011.7.5.329

18. CAN/CSA A23.3-04 (R2010), “Design of Concrete Structures,” CSA Group, Toronto, ON, Canada, 2004, 352 pp.

19. Morcos, M., “Seismic Behaviour of SMA-Reinforced Slender Concrete Shear Walls,” master’s thesis, York University, Toronto, ON, Canada, 2021, 446 pp.

20. FEMA 461, “Interim Testing Protocols for Determining the Seismic Performance Characteristics of Structural and Nonstructural Components,” Applied Technology Council, Redwood City, CA, 2007, 138 pp.

21. ATC-24, “Guidelines for Cyclic Seismic Testing of Components of Steel Structures,” Applied Technology Council, Redwood City, CA, 1992, 58 pp.

22. Eshghi, N., “Behaviour and Analysis of Strain Hardening Fiber Reinforced Cementitious Composites Under Shear and Flexure,” MASc thesis, York University, Toronto, ON, Canada, 2018, 209 pp.

23. ASTM C1856/C1856M-17, “Standard Practice for Fabricating and Testing Specimens of Ultra-High Performance Concrete,” ASTM International, West Conshohocken, PA, 2017, 4 pp.

24. Soto Rojas, M. A., “Behavior of Engineered Cementitious Composite-Repaired Superelastic-Shape Memory Alloy Reinforced Shear Walls,” MASc thesis, York University, Toronto, ON, Canada, 2020, 289 pp.

25. Park, R., “State-of-the-Art Report: Ductility Evaluation from Laboratory and Analytical Testing,” Proceedings of the Ninth World Conference on Earthquake Engineering, Tokyo-Kyoto, Japan, Aug. 1988, 12 pp.

26. Oesterle, R. G.; Fiorato, A. E.; Johal, L. S.; Carpenter, J. E.; Russell, H. G.; and Corley, W. G., “Earthquake Resistant Structural Walls - Tests of Isolated Walls,” Portland Cement Association, Skokie, IL, 1976, 328 pp.