ACI Global Home Middle East Region Portal Western Europe Region Portal
Email Address is required Invalid Email Address
In today’s market, it is imperative to be knowledgeable and have an edge over the competition. ACI members have it…they are engaged, informed, and stay up to date by taking advantage of benefits that ACI membership provides them.
Read more about membership
Learn More
Become an ACI Member
Topics In Concrete
Home > Publications > International Concrete Abstracts Portal
The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.
Title: ACI CODE-437.2-22: Load Testing of Concrete Structures—Code and Commentary
Author(s): ACI Committee 437
Publication: Technical Documents
Volume:
Issue:
Appears on pages(s): 26
Keywords:
DOI:
Date: 3/1/2023
Abstract: This Code provides requirements for test load magnitudes, test protocols, and acceptance criteria for conducting a load test as a means of evaluating the safety and serviceability of concrete structural members and systems of structures. A load test may be conducted as part of a structural evaluation to determine whether a structure requires repair and rehabilitation, or to verify the adequacy of repair and rehabilitation measures. Keywords: acceptance criteria; cyclic loading; load test; monotonic loading; test load magnitude; test protocol.