Progressive Collapse Response of Reinforced Concrete Assembly with Realistic Boundary Conditions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Progressive Collapse Response of Reinforced Concrete Assembly with Realistic Boundary Conditions

Author(s): Kai Qian, Guang-Tao Li, Dong-Qiu Lan, and Liu Jin

Publication: Structural Journal

Volume: 120

Issue: 4

Appears on pages(s): 43-56

Keywords: boundary condition; progressive collapse; reinforced concrete (RC); special detailing

DOI: 10.14359/51738718

Date: 7/1/2023

Abstract:
Previous studies on reinforced concrete (RC) beam-column subassemblies under a column removal scenario are helpful to understand the load-resisting mechanisms of RC structures against progressive collapse, but most of these studies failed to simulate actual boundary conditions, which were simplified as fixed boundaries to allow sufficient development of the load-resisting mechanisms. These studies were unable to reflect the response of joints and side columns under progressive collapse. To fill this gap, an experimental program on six half-scale beam-column subassemblies with joints and side columns was designed and tested to fully understand the effects of boundary conditions on the structural behavior of RC planar frames against progressive collapse. Three subassemblies were specially designed, while the other three were ordinarily designed to quantify the benefits of special detailing. The test results show that the effects of boundary conditions on the development of load-resisting mechanisms are marginal, whereas the effects of special detailing are significant. Specifically, specimens under a middle-column removal scenario and a penultimatecolumn removal scenario develop similar compressive arch action (CAA) capacities and catenary action (CA) capacities. The CAA capacity dominates the load resistance of specimens with ordinary detailing. In contrast, the CA capacity governs the load resistance of specimens with special detailing mainly due to the larger areas of longitudinal reinforcing bars and the greater rotation capacities of beam ends. However, boundary conditions can greatly affect the failure mode of specimens with ordinary detailing. Finally, an analytical study was performed to demonstrate the contributions of axial force and shear force to load resistance. According to test results and analytical analyses, RC frames with special detailing have sufficient rotational capacity to develop adequate tie forces to resist progressive collapse.

Related References:

1. ASCE/SEI 7-05, “Minimum Design Loads for Buildings and Other Structures,” Structural Engineering Institute, American Society of Civil Engineers, Reston, VA, 2005, 424 pp.

2. UFC 4-023-03, “Design of Buildings to Resist Progressive Collapse,” Unified Facilities Criteria, U.S. Department of Defense, Washington, DC, 2013.

3. GSA, “Progressive Collapse Analysis and Design Guidelines for New Federal Office Buildings and Major Modernization Projects,” U.S. General Services Administration, Washington, DC, 2009.

4. Lew, H. S.; Bao, Y.; Pujol, S.; and Sozen, M. A., “Experimental Study of Reinforced Concrete Assemblies under Column Removal Scenario,” ACI Structural Journal, V. 111, No. 4, July-Aug. 2014, pp. 881-892. doi: 10.14359/51686739

5. Yu, J., and Tan, K.-H., “Experimental and Numerical Investigation on Progressive Collapse Resistance of Reinforced Concrete Beam Column Sub-Assemblages,” Engineering Structures, V. 55, Oct. 2013, pp. 90-106. doi: 10.1016/j.engstruct.2011.08.040

6. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-05) and Commentary (ACI 318R-05),” American Concrete Institute, Farmington Hills, MI, 2005, 430 pp.

7. Qian, K., and Li, B., “Performance of Three-Dimensional Reinforced Concrete Beam-Column Substructures under Loss of a Corner Column Scenario,” Journal of Structural Engineering, ASCE, V. 139, No. 4, Apr. 2013, pp. 584-594. doi: 10.1061/(ASCE)ST.1943-541X.0000630

8. Choi, H., and Kim, J., “Progressive Collapse-Resisting Capacity of RC Beam–Column Sub-Assemblage,” Magazine of Concrete Research, V. 63, No. 4, Apr. 2011, pp. 297-310.

9. Sadek, F.; Main, J. A.; Lew, H. S.; and Bao, Y., “Testing and Analysis of Steel and Concrete Beam-Column Assemblies under a Column Removal Scenario,” Journal of Structural Engineering, ASCE, V. 137, No. 9, Sept. 2011, pp. 881-892. doi: 10.1061/(ASCE)ST.1943-541X.0000422

10. Qian, K., and Li, B., “Dynamic Performance of RC Beam-Column Substructures under the Scenario of the Loss of a Corner Column—Experimental Results,” Engineering Structures, V. 42, Sept. 2012, pp. 154-167.

11. Li, Y.; Lu, X.; Guan, H.; and Ye, L., “Progressive Collapse Resistance Demand of Reinforced Concrete Frames under Catenary Mechanism,” ACI Structural Journal, V. 111, No. 5, Sept.-Oct. 2014, pp. 1225-1234. doi: 10.14359/51687029

12. Yu, J., and Tan, K. H., “Structural Behavior of RC Beam-Column Subassemblages under a Middle Column Removal Scenario,” Journal of Structural Engineering, ASCE, V. 139, No. 2, Feb. 2013, pp. 233-250. doi: 10.1061/(ASCE)ST.1943-541X.0000658

13. Deng, X.-F.; Liang, S.-L.; Fu, F.; and Qian, K., “Effects of High-Strength Concrete on Progressive Collapse Resistance of Reinforced Concrete Frame,” Journal of Structural Engineering, ASCE, V. 146, No. 6, June 2020, p. 04020078. doi: 10.1061/(ASCE)ST.1943-541X.0002628

14. Qian, K.; Liang, S.-L.; Fu, F.; and Li, Y., “Progressive Collapse Resistance of Emulative Precast Concrete Frames with Various Reinforcing Details,” Journal of Structural Engineering, ASCE, V. 147, No. 8, Aug. 2021, p. 04021107. doi: 10.1061/(ASCE)ST.1943-541X.0003065

15. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

16. Hwang, S.-J., and Lee, H.-J., “Strength Prediction for Discontinuity Regions by Softened Strut-and-Tie Model,” Journal of Structural Engineering, ASCE, V. 128, No. 12, Dec. 2002, pp. 1519-1526. doi: 10.1061/(ASCE)0733-9445(2002)128:12(1519)

17. Izzuddin, B. A.; Vlassis, A. G.; Elghazouli, A. Y.; and Nethercot, D. A., “Progressive Collapse of Multi-Storey Buildings due to Sudden Column Loss—Part I: Simplified Assessment Framework,” Engineering Structures, V. 30, No. 5, May 2008, pp. 1308-1318. doi: 10.1016/j.engstruct.2007.07.011

18. Yu, J., and Tan, K. H., “Analytical Model for the Capacity of Compressive Arch Action of Reinforced Concrete Sub-Assemblages,” Magazine of Concrete Research, V. 66, No. 3, Feb. 2014, pp. 109-126. doi: 10.1680/macr.13.00217

19. Lu, X.; Lin, K.; Li, C.; and Li, Y., “New Analytical Calculation Models for Compressive Arch Action in Reinforced Concrete Structures,” Engineering Structures, V. 168, Aug. 2018, pp. 721-735. doi: 10.1016/j.engstruct.2018.04.097


ALSO AVAILABLE IN:

Electronic Structural Journal