Prediction of Remaining Service Life of Prestressed Concrete Girders Containing Cracks

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Prediction of Remaining Service Life of Prestressed Concrete Girders Containing Cracks

Author(s): Savitha Sagari Srinivasan and Raissa Douglas Ferron

Publication: Materials Journal

Volume: 120

Issue: 3

Appears on pages(s): 93-102

Keywords: concrete girders; microcracks; precast concrete; prediction models; service life

DOI: 10.14359/51738686

Date: 5/1/2023

Abstract:
Most concrete service life models are designed for uncrackedconditions, and the effect of microcracks on such models has not been as well researched. A service life model for concrete structures that takes into account microcracking is presented. A unique feature of this model is that its input parameters can be determined using only nondestructive methods, thus allowing it to be used when samples for laboratory tests cannot be extracted— for example, in in-service or critical infrastructure. The model was developed for low water-cementitious materials ratio (w/cm) concrete mixtures and validated on full-scale prestressed concrete girders. The results showed that the presence of a large number of microcracks could cause a loss in the remaining service life of concrete structures, even if individual microcracks did not cause asignificant impact.

Related References:

1. Yang, L., Techniques for Corrosion Monitoring, Woodhead Publishing, Sawston, UK, 2008. doi: 10.1533/9781845694050

2. Ailaney, R., “Bridge Preservation Guide: Maintaining a Resilient Infrastructure to Preserve Mobility,” Publication No. FHWA-HIF-18-022, Federal Highway Administration, Washington, DC, 2018, 28 pp.

3. Alexander, M. G., and Nganga, G., “Importance of Marine Concrete Structures and Durability Design,” Marine Concrete Structures: Design, Durability and Performance, M. G. Alexander, ed., Woodhead Publishing, Sawston, UK, 2016, pp. 1-13.

4. Tiburzi, N. B.; Drimalas, T.; and Folliard, K. J., “Evaluation of Precast Bridge Girder Cracking: The Role of Volume Change,” Cement and Concrete Research, V. 101, Nov. 2017, pp. 55-67. doi: 10.1016/j.cemconres.2017.08.024

5. Srinivasan, S. S., “Effect of Microcracking on Strength and Durability of Low Water-to-Cement Ratio Concretes,” PhD dissertation, The University of Texas at Austin, Austin, TX, 2020, 175 pp.

6. Amin, M. S.; El-Gamal, S. M. A.; and Hashem, F. S., “Effect of Addition of Nano-Magnetite on the Hydration Characteristics of Hardened Portland Cement and High Slag Cement Pastes,” Journal of Thermal Analysis and Calorimetry, V. 112, No. 3, June 2013, pp. 1253-1259. doi: 10.1007/s10973-012-2663-1

7. Ray, I.; Gong, Z.; Davalos, J. F.; and Kar, A., “Shrinkage and Cracking Studies of High Performance Concrete for Bridge Decks,” Construction and Building Materials, V. 28, No. 1, Mar. 2012, pp. 244-254. doi: 10.1016/j.conbuildmat.2011.08.066

8. Srinivasan, S. S., and Ferron, R. D., “Effect of Crack Width, Density, and Depth on Strength and Durability of Concrete-Equivalent Mortar,” ACI Materials Journal, V. 118, No. 4, July 2021, pp. 65-78. doi: 10.14359/51732792

9. Mahmoodian M., “Methods for Structural Reliability Analysis,” Reliability and Maintainability of In-Service Pipelines, Gulf Professional Publishing, Houston, TX, 2018, pp. 79-101. doi: 10.1016/B978-0-12-813578-5.00003-2

10. Violetta, B., “Life-365 Service Life Prediction Model,” Concrete International, V. 24, No. 12, Dec. 2002, pp. 53-57.

11. DuraCrete, “Modelling of Degradation: DuraCrete, Probabilistic Performance Based Durability Design of Concrete Structures,” Brite EuRam III, DuraCrete Project Document BE95-1347/R4-5, CUR, Gouda, the Netherlands, 1998, 174 pp.

12. Kwon, S. J.; Na, U. J.; Park, S. S.; and Jung, S. H., “Service Life Prediction of Concrete Wharves with Early-Aged Crack: Probabilistic Approach for Chloride Diffusion,” Structural Safety, V. 31, No. 1, Jan. 2009, pp. 75-83. doi: 10.1016/j.strusafe.2008.03.004

13. Pacheco, J., “Incorporating Cracks in Chloride Ingress Modeling and Service Life Predictions,” ACI Materials Journal, V. 116, No. 5, Sept. 2019, pp. 113-118. doi: 10.14359/51716832

14. Erdoǧdu, Ş.; Kondratova, I. L.; and Bremner, T. W., “Determination of Chloride Diffusion Coefficient of Concrete Using Open-Circuit Potential Measurements,” Cement and Concrete Research, V. 34, No. 4, Apr. 2004, pp. 603-609. doi: 10.1016/j.cemconres.2003.09.024

15. Bolukbasi, M.; Mohammadi, J.; and Arditi, D., “Estimating the Future Condition of Highway Bridge Components Using National Bridge Inventory Data,” Practice Periodical on Structural Design and Construction, ASCE, V. 9, No. 1, Feb. 2004, pp. 16-25. doi: 10.1061/(ASCE)1084-0680(2004)9:1(16)

16. Stukhart, G.; James, R. W.; Garcia-Diaz, A.; Bligh, R. P.; Sobanjo, J.; and McFarland, W. F., “Study for a Comprehensive Bridge Management System for Texas,” Report No. FHWA/TX-90/1212-1F, Texas Transportation Institute, College Station, TX, 1991, 240 pp.

17. Koo, T. K., and Li, M. Y., “A Guideline of Selecting and Reporting Intraclass Correlation Coefficients for Reliability Research,” Journal of Chiropractic Medicine, V. 15, No. 2, June 2016, pp. 155-163. doi: 10.1016/j.jcm.2016.02.012

18. Bensoussan, A., “Reliability Index,” Optimal Control and Dynamic Games: Applications in Finance, Management Science and Economics, C. Deissenberg and R. F. Hartl, eds., Springer, New York, NY, 2005, pp. 311-317. doi: 10.1007/0-387-25805-1_18

19. Morgan, J. A., and Tatar, J. F., “Calculation of the Residual Sum of Squares for All Possible Regressions,” Technometrics, V. 14, No. 2, May 1972, pp. 317-325. doi: 10.1080/00401706.1972.10488918

20. Brown, J. D., Understanding Research in Second Language Learning: A Teacher’s Guide to Statistics and Research Design, Cambridge University Press, Cambridge, UK, 1988.

21. Thomas, M. D. A.; Folliard, K. J.; Fournier, B.; Rivard, P.; Drimalas, T.; and Garber, S. I., “Methods for Evaluating and Treating ASR-Affected Structures: Results of Field Application and Demonstration Projects – Volume II: Details of Field Applications and Analysis – Final Report,” Report No. FHWA-HIF-14-0003, Federal Highway Administration, Washington, DC, 2013, 342 pp.

22. Torkornoo, S.; Bradshaw, E.; Sharp, S. R.; and Sprinkel, M. M., “Design of Artificially Cracked Concrete Specimens for Virginia Department of Transportation Material Evaluation,” Report No. FHWA/VTRC 18-R2, Virginia Transportation Research Council, Charlottesville, VA, 2018, 35 pp.

23. Fournier, B.; Bérubé, M.-A.; Folliard, K. J.; and Thomas, M., “Report on the Diagnosis, Prognosis, and Mitigation of Alkali-Silica Reaction (ASR) in Transportation Structures,” Report No. FHWA-HIF-09-004, Federal Highway Administration, Washington, DC, 2010, 154 pp.

24. ASTM C597-16, “Standard Test Method for Pulse Velocity Through Concrete,” ASTM International, West Conshohocken, PA, 2016, 4 pp.

25. NT BUILD 492, “Concrete, Mortar and Cement-Based Repair Materials: Chloride Migration Coefficient from Non-Steady-State Migration Experiments,” NORDTEST, Espoo, Finland, 1999, 8 pp.

26. Srinivasan, S. S.; Rung, M.; and Ferron, R. D., “Factors Affecting Loss in Durability in Prestressed-Concrete Girders with Microcracking,” Journal of Bridge Engineering, ASCE, V. 25, No. 9, Sept. 2020, p. 04020068. doi: 10.1061/(ASCE)BE.1943-5592.0001590

27. Caré, S., “Influence of Aggregates on Chloride Diffusion Coefficient into Mortar,” Cement and Concrete Research, V. 33, No. 7, July 2003, pp. 1021-1028. doi: 10.1016/S0008-8846(03)00009-7

28. Weiss, W. J.; Yang, W.; and Shah, S. P., “Factors Influencing Durability and Early-Age Cracking in High-Strength Concrete Structures,” High-Performance Concrete: Research to Practice, SP-189, American Concrete Institute, Farmington Hills, MI, 2000, pp. 387-409.

29. Olive, D. J., Linear Regression, Springer International Publishing AG, Cham, Switzerland, 2017. doi: 10.1007/978-3-319-55252-1

30. Malumbela, G.; Alexander, M.; and Moyo, P., “Interaction between Corrosion Crack Width and Steel Loss in RC Beams Corroded under Load,” Cement and Concrete Research, V. 40, No. 9, Sept. 2010, pp. 1419-1428. doi: 10.1016/j.cemconres.2010.03.010

31. Kim, G.; Kim, J.-Y.; Kurtis, K. E.; and Jacobs, L. J., “Drying Shrinkage in Concrete Assessed by Nonlinear Ultrasound,” Cement and Concrete Research, V. 92, Feb. 2017, pp. 16-20. doi: 10.1016/j.cemconres.2016.11.010

32. Snee, R. D., “Validation of Regression Models: Methods and Examples,” Technometrics, V. 19, No. 4, 1977, pp. 415-428. doi: 10.1080/00401706.1977.10489581

33. Piñeiro, G.; Perelman, S.; Guerschman, J. P.; and Paruelo, J. M., “How to Evaluate Models: Observed vs. Predicted or Predicted vs. Observed?” Ecological Modelling, V. 216, No. 3-4, Sept. 2008, pp. 316-322. doi: 10.1016/j.ecolmodel.2008.05.006

34. Papé, T. M., and Melchers, R. E., “The Effects of Corrosion on 45-Year-Old Pre-stressed Concrete Bridge Beams,” Structure and Infrastructure Engineering, V. 7, No. 1-2, 2011, pp. 101-108. doi: 10.1080/15732471003588411

35. Possan, E., and de Oliveira Andrade, J. J., “Markov Chains and Reliability Analysis for Reinforced Concrete Structure Service Life,” Materials Research, V. 17, No. 3, 2014, pp. 593-602. doi: 10.1590/S1516-14392014005000074

36. Morcous, G., “Performance Prediction of Bridge Deck Systems Using Markov Chains,” Journal of Performance of Constructed Facilities, ASCE, V. 20, No. 2, May 2006, pp. 146-155. doi: 10.1061/(ASCE)0887-3828(2006)20:2(146)

37. Guimarães, A. T. da C., “Vida Útil de Estruturas de Concreto Armado em Ambientes Marítimos,” PhD thesis, University of São Paulo, São Paulo, SP, Brazil, 2000. (in Portuguese)

38. Kwon, S.-J.; Lee, B. J.; and Kim, Y. Y., “Concrete Mix Design for Service Life of RC Structures under Carbonation Using Genetic Algorithm,” Advances in Materials Science and Engineering, V. 2014, 2014, Article No. 653753. doi: 10.1155/2014/653753

39. Petcherdchoo, A., and Chindaprasirt, P., “Exponentially Aging Functions Coupled with Time-Dependent Chloride Transport Model for Predicting Service Life of Surface-Treated Concrete in Tidal Zone,” Cement and Concrete Research, V. 120, June 2019, pp. 1-12. doi: 10.1016/j.cemconres.2019.03.009


ALSO AVAILABLE IN:

Electronic Materials Journal