Title: Newly Synthesized Nanotube Hybrids for Sustainable and Multifunctional Coal Ash Based Concrete

Author(s): Maglogianni

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/23/2022

Abstract:
Carbon nanotube hybrids/coal ash-based concrete was prepared showing unmatched mechanical/fracture properties and sensing functionalities. The newly synthesized nanotube hybrid suspensions, prepared using ultrasonication, were found to exhibit excellent dispersibility and long-term stability for a period over 90 days. The chemical structure and functional groups of the dispersed nanotube hybrids were evaluated by FTIR and Raman Spectroscopy. A considerably increased (around 65%) electrical conductivity was observed, as compared to the plain coal ash concrete, which coupled with the enhanced modulus and toughness led to a superior electromechanical response, essential for strain sensing and progressive failure monitoring.