Title: Surface Damage Imaging for Input to Load Rating of Bridges

Author(s): Ziehl

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/23/2022

Abstract:
This talk will be focused on a tailored application for imaging based on the platform of aerial drones. The imaging in this case requires relatively precise information on the geometry of surface cracking to provide technical input to the load rating process for a family of bridges in South Carolina that frequently do not meet their load rating criteria (referred to a precast reinforced flat slab bridges).