Title: Detection and Characterization of Alkali-Silica Reaction Damage in Concrete Using Surface Wavefield Imaging

Author(s): Song

Publication: Web Session

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 10/23/2022

Abstract:
The objective of these sessions is to present and discuss different methods for detection and monitoring of surface damage in concrete elements. The focus is how to use SHM techniques to obtain useful information regarding formation and progression of surface damage. These sessions will be of interest to engineers, researchers, and infrastructure owners and operators.