The Mechanical and Thermal Properties of Cement CAST Mortar/Graphene Oxide Composites Materials

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: The Mechanical and Thermal Properties of Cement CAST Mortar/Graphene Oxide Composites Materials

Author(s): Thidatip Janjaroen, Sunisar Khammahong, Wattana Tuichai, Attaphol Karaphun, Chaiwat Phrompet, Chaval Sriwong & Chesta Ruttanapun

Publication: IJCSM

Volume: 16

Issue:

Appears on pages(s):

Keywords: graphene oxide (GO) nanosheets, GO/mortar (GMT) composite, mechanical and thermal properties

DOI: 10.1186/s40069-022-00521-z

Date: 9/30/2022

Abstract:
This paper presents the influence of the graphene oxide (GO) sheet contents at conditions of 0, 0.01, 0.03, 0.05, and 0.1 wt% on the mechanical and thermal properties of GO/CAST 11 LW mortar (GMT) composites for heat insulating brick. The GMT composites were prepared by a simple mixing method. The structure of GMT composites was investigated by X-ray diffraction (XRD) and Raman spectroscopy (Raman) techniques. The small grain sizes of GMT composites were confirmed by transmission electron microscopy (TEM). The mechanical properties of GMT composites are increased with increasing GO contents. A lot of functional groups in GO such as carboxylic acid reacted with a calcium silicate hydrate, CaH2O4Si (CSH), calcium hydroxide, Ca(OH)2 (CH) and Ettringite, and Ca6[Al(OH)6]2(SO4)3·26H2O (CA) phases in the mortar, which can be considered good mechanical properties in the GMT composites. The heat insulation values of GMT composites were improved by the interaction with the CSH, CH, and CA phases in the cement mortar on the surface of GO. The highest compressive and tensile strengths and low heat transfer rate of about 0.465 W/min were observed at 0.05 of GO (GMT_0.05) composites in the curing age of 7 days. Thus, a new pathway of GMT composites can be prepared by a simple mixing method to significantly improve the mechanical and thermal properties of mortar GMT composites.




  