Use of Welded Wire Reinforcement as Lateral Reinforcement in Concrete Beams: Part 1—Shear

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Use of Welded Wire Reinforcement as Lateral Reinforcement in Concrete Beams: Part 1—Shear

Author(s): Yazan Alhoubi, Sami W. Tabsh, and Abdelaziz Younes

Publication: Structural Journal

Volume: 120

Issue: 3

Appears on pages(s): 157-172

Keywords: beam; confinement; ductility; shear; welded wire reinforcement (WWR)

DOI: 10.14359/51738508

Date: 5/1/2023

Abstract:
Reinforced concrete beams are typically reinforced transversely with rectilinear stirrups made from steel reinforcing bars to resist shear. The process of making stirrups requires extended time and considerable labor, and results in relatively large tolerances. This study aims at studying the viability of using welded wire reinforcement (WWR), cold-formed into the shape of a closed steel cage to resist the shear load effect. To accomplish the objective of the study, 16 half-scale beams were tested by a universal testing machine under displacement-controlled loading conditions. The study considered different wire diameters (4, 6, and 8 mm [0.16, 0.24,and 0.32 in.]), grid openings (25, 50, and 100 mm [1, 2, and 4 in.]), shear span-to-thickness ratios (2.5 and 3.0), and transverse steel reinforcement ratios (251 and 505 N/mm [1433 and 2884 lb/in.]). A comparison was carried out between the test results of WWRreinforced beams and corresponding stirrup-reinforced beams in terms of the crack formation characteristics, stiffness, shear strength, residual strength, and ductility. Findings of the study showed that the WWR-reinforced beams possessed 2 to 17% higher shear strength than the corresponding stirrup-reinforced beams, without a compromise in the ductility. The predicted shear strengthbased on ACI 318 was within 10% of the strength obtained by the experiments.

Related References:

1. Bernold, L. E., and Chang, P., “Potential Gains through Welded-Wire Fabric Reinforcement,” Journal of Construction Engineering and Management, ASCE, V. 118, No. 2, 1992, pp. 244-257. doi: 10.1061/(ASCE)0733-9364(1992)118:2(244)

2. Xuan, X.; Rizkalla, S.; and Maruyama, K., “Effectiveness of Welded Wire Fabric as Shear Reinforcement in Pretensioned Prestressed Concrete T-Beams,” ACI Structural Journal, V. 85, No. 4, July-Aug. 1988, pp. 429-436. doi: 10.14359/2711

3. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

4. ASTM A1064/A1064M-18a, “Standard Specification for Carbon-Steel Wire and Welded Wire Reinforcement, Plain and Deformed, for Concrete,” ASTM International, West Conshohocken, PA, 2018.

5. ASTM A1022/A1022M-16b, “Standard Specification for Deformed and Plain Stainless Steel Wire and Welded Wire for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2016.

6. Durrani, A. J., and Robertson, I. N., “Shear Strength of Prestressed Concrete T-Beams with Welded Wire Fabric as Shear,” PCI Journal, V. 32, No. 2, 1987, pp. 46-61. doi: 10.15554/pcij.03011987.46.61

7. Xuan, X., and Rizkalla, S. H., “Welded Wire Shear Reinforcement under Cyclic Loading,” Batiment International, Building Research and Practice, V. 16, No. 3, 1988, pp. 161-166. doi: 10.1080/01823328808726884

8. Pincheira, J. A.; Rizkalla, S. H.; and Attiogbe, E. K., “Performance of Welded Wire Fabric as Shear Reinforcement under Cyclic Loading,” ACI Structural Journal, V. 86, No. 6, Nov.-Dec. 1989, pp. 728-735. doi: 10.14359/2770

9. Mansur, M. A.; Lee, C. K.; and Lee, S. L., “Deformed Wire Fabric as Shear Reinforcement in Concrete Beams,” ACI Structural Journal, V. 84, No. 5, Sept.-Oct. 1987, pp. 392-399. doi: 10.14359/1649

10. Griezic, A.; Cook, W. D.; and Mitchell, D., “Tests to Determine Performance of Deformed Welded Wire Fabric Stirrups,” ACI Structural Journal, V. 91, No. 2, Mar.-Apr. 1994, pp. 211-220. doi: 10.14359/4597

11. Lee, S. L.; Mansur, M. A.; Tan, K. H.; and Kasiraju, K., “Crack Control in Beams Using Deformed Wire Fabric,” Journal of Structural Engineering, ASCE, V. 115, No. 10, 1989, pp. 2645-2660. doi: 10.1061/(ASCE)0733-9445(1989)115:10(2645)

12. Akhnoukh, A. K., and Xie, H., “Welded Wire Reinforcement versus Random Steel Fibers in Precast/Prestressed Ultra-High-Performance Concrete I-Girders,” Construction and Building Materials, V. 24, No. 11, 2010, pp. 2200-2207. doi: 10.1016/j.conbuildmat.2010.04.037

13. Saatcioglu, M., and Razvi, S. R., “Strength and Ductility of Confined Concrete,” Journal of Structural Engineering, ASCE, V. 118, No. 6, 1992, pp. 1590-1607. doi: 10.1061/(ASCE)0733-9445(1992)118:6(1590)

14. Lambert-Aikhionbare, N., and Tabsh, S. W., “Ductility Enhancement of High Strength Concrete Columns with Welded Wire Mesh,” Structures 2004: Building on the Past, Securing the Future - Proceedings of the 2004 Structures Congress, G. E. Blandford, ed., Nashville, TN, 2004, pp. 1-20. doi: 10.1061/40700(2004)14

15. Lambert-Aikhionbare, N., and Tabsh, S. W., “Confinement of High-Strength Concrete with Welded Wire Reinforcement,” ACI Structural Journal, V. 98, No. 5, Sept.-Oct. 2001, pp. 677-685. doi: 10.14359/10621

16. Kusuma, B.; Tavio; and Suprobo, P., “Axial Load Behavior of Concrete Columns with Welded Wire Fabric as Transverse Reinforcement,” Procedia Engineering, V. 14, 2011, pp. 2039-2047. doi: 10.1016/j.proeng.2011.07.256

17. Riva, P., and Franchi, A., “Behavior of Reinforced Concrete Walls with Welded Wire Mesh Subjected to Cyclic Loading,” ACI Structural Journal, V. 98, No. 3, May-June 2001, pp. 324-334. doi: 10.14359/10221

18. Abu Maraq, M. A.; Tayeh, B. A.; Ziara, M. M.; and Alyousef, R., “Flexural Behavior of RC Beams Strengthened with Steel Wire Mesh and Self-Compacting Concrete Jacketing — Experimental Investigation and Test Results,” Journal of Materials Research and Technology, V. 10, 2021, pp. 1002-1019. doi: 10.1016/j.jmrt.2020.12.069

19. Tayeh, B. A.; Abu Maraq, M. A.; and Ziara, M. M., “Flexural Performance of Reinforced Concrete Beams Strengthened with Self-Compacting Concrete Jacketing and Steel Welded Wire Mesh,” Structures, V. 28, Dec. 2020, pp. 2146-2162. doi: 10.1016/j.istruc.2020.10.035

20. Manaha, Y. P.; Suprobo, P.; and Wahyuni, E., “Retrofitting of Square Reinforced Concrete Column by Welded Wire Mesh Jacketing with Consentric Axial Load,” IOP Conference Series: Materials Science and Engineering, V. 508, May 2019, Article No. 012042. doi: 10.1088/1757-899X/508/1/012042

21. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

22. ASTM C39/C39M-21, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2021.

23. ASTM A370-18, “Standard Test Methods and Definitions for Mechanical Testing of Steel Products,” ASTM International, West Conshohocken, PA, 2018.

24. ASTM E8/E8M-16a, “Standard Test Methods for Tension Testing of Metallic Materials,” ASTM International, West Conshohocken, PA, 2016.

25. Alhoubi, Y. L., “Shear Strength of Concrete Beams Reinforced with Steel Welded Wire Fabric,” master’s thesis, American University of Sharjah, Sharjah, UAE, 2019.

26. Maekawa, K.; Okamura, H.; and Pimanmas, A., Non-Linear Mechanics of Reinforced Concrete, first edition, CRC Press, London, UK, 2003. doi: 10.1201/978148228808


ALSO AVAILABLE IN:

Electronic Structural Journal