Near-Surface Mounting-Strengthened Reinforced Concrete Beams Incorporating Glass Fiber-Reinforced Polymer Channels

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Near-Surface Mounting-Strengthened Reinforced Concrete Beams Incorporating Glass Fiber-Reinforced Polymer Channels

Author(s): Hamza M. Y. Ali, M. Neaz Sheikh, and Muhammad N. S. Hadi

Publication: Structural Journal

Volume: 120

Issue: 3

Appears on pages(s): 75-85

Keywords: external bonding (EB); flexural strengthening; glass fiberreinforced polymer (GFRP) bars; GFRP channels; near-surface mounting (NSM); reinforced concrete (RC) beams

DOI: 10.14359/51738503

Date: 5/1/2023

Abstract:
Near-surface mounting (NSM) and external bonding (EB) arewildly used techniques for strengthening reinforced concrete(RC) beams using fiber-reinforced polymer (FRP) reinforcement. However, there are a few drawbacks to the use of these two techniques, including premature failure due to concrete cover separation (CCS), which can cause significant challenges for their wide practical applications. Hence, his experimental study investigates the efficiency of using a novel anchoring system for RC beams strengthened at the sides using NSM glass-FRP (NSM-GFRP) bars. The NSM-GFRP bars were anchored with either GFRP channels or GFRP channel strips. The experimental results showed that RC beams strengthened with side NSM-GFRP bars anchored with GFRP channels and GFRP channel strips increased the flexural load of the RC beams by 152% and 106%, respectively, compared to the unstrengthened reference beam. In addition, GFRP channelstrips prevented the CCS failure and improved the ductility of the RC beam, using the full strength of NSM-GFRP bars.

Related References:

1. Bakis, C. E.; Bank, L. C.; Brown, V. L.; Cosenza, E.; Davalos, J. F.; Lesko, J. J.; Machida, A.; Rizkalla, S. H.; and Triantafillou, T. C., “Fiber-Reinforced Polymer Composites for Construction - State-of-the-Art Review,” Journal of Composites for Construction, ASCE, V. 6, No. 2, 2002, pp. 73-87. doi: 10.1061/(ASCE)1090-0268(2002)6:2(73)

2. Hollaway, L. C., “A Review of the Present and Future Utilisation of FRP Composites in the Civil Infrastructure with Reference to Their Important In-Service Properties,” Construction and Building Materials, V. 24, No. 12, 2010, pp. 2419-2445.

3. Kang, T. H. K.; Howell, J.; Kim, S.; Lee, D. J., “A State-of-the-Art Review on Debonding Failures of FRP Laminates Externally Adhered to Concrete,” International Journal of Concrete Structures and Materials, V. 6, No. 2, 2012/06/01. 2012, pp. 123-34.

4. De Lorenzis, L., and Nanni, A., “Characterization of FRP Rods as Near-Surface Mounted Reinforcement,” Journal of Composites for Construction, ASCE, V. 5, No. 2, 2001, pp. 114-121. doi: 10.1061/(ASCE)1090-0268(2001)5:2(114)

5. El-Hacha, R., and Rizkalla, S. H., “Near-Surface-Mounted Fiber-Reinforced Polymer Reinforcements for Flexural Strengthening of Concrete Structures,” ACI Structural Journal, V. 101, No. 5, Sept.-Oct. 2004, pp. 717-726.

6. Yost, J. R.; Gross, S. P.; Dinehart, D. W.; and Mildenberg, J. J., “Flexural Behavior of Concrete Beams Strengthened with Near-Surface-Mounted CFRP Strips,” ACI Structural Journal, V. 104, No. 4, July-Aug. 2007, pp. 430-437.

7. Chennareddy, R., and Taha, M. M. R., “Effect of Combining Near-Surface-Mounted and U-Wrap Fiber-Reinforced Polymer Strengthening Techniques on Behavior of Reinforced Concrete Beams,” ACI Structural Journal, V. 114, No. 3, May-June 2017, pp. 719-728. doi: 10.14359/51689443

8. Nurbaiah, M. N.; Hanizah, A. H.; Nursafarina, A.; and Ashikin, M. N., “Flexural Behaviour of RC Beams Strengthened With Externally Bonded (EB) FRP Sheets or Near Surface Mounted (NSM) FRP Rods Method,” International Conference on Science and Social Research (CSSR 2010), 2010, pp. 1232-1237.

9. Sena-Cruz, J. M.; Barros, J. A. O.; Coelho, M. R. F.; Silva, L. F. F. T., “Efficiency of Different Techniques in Flexural Strengthening of RC Beams Under Monotonic and Fatigue Loading,” Construction and Building Materials, V. 29, 2012, pp. 175-82.

10. Sharaky, I. A.; Torres, L.; Baena, M.; and Vilanova, I., “Effect of Different Material and Construction Details on the Bond Behaviour of NSM FRP Bars in Concrete,” Construction and Building Materials, V. 38, 2013, pp. 890-902. doi: 10.1016/j.conbuildmat.2012.09.015

11. De Lorenzis, L., and Teng, J. G., “Near-Surface Mounted FRP Reinforcement: An Emerging Technique for Strengthening Structures,” Composites Part B: Engineering, V. 38, No. 2, 2007, pp. 119-143. doi: 10.1016/j.compositesb.2006.08.003

12. Reda, R. M.; Sharaky, I. A.; Ghanem, M.; Seleem, M. H.; and Sallam, H. E. M., “Flexural Behavior of RC Beams Strengthened by NSM GFRP Bars Having Different End Conditions,” Composite Structures, V. 147, 2016, pp. 131-142. doi: 10.1016/j.compstruct.2016.03.018

13. Sharaky, I. A.; Reda, R. M.; Ghanem, M.; Seleem, M. H.; and Sallam, H. E. M., “Experimental and Numerical Study of RC Beams Strengthened with Bottom and Side NSM GFRP Bars Having Different End Conditions,” Construction and Building Materials, V. 149, 2017, pp. 882-903. doi: 10.1016/j.conbuildmat.2017.05.192

14. Sharaky, I. A.; Torres, L.; and Sallam, H. E. M., “Experimental and Analytical Investigation into the Flexural Performance of RC Beams With Partially and Fully Bonded NSM FRP Bars/Strips,” Composite Structures, V. 122, 2015, pp. 113-126. doi: 10.1016/j.compstruct.2014.11.057

15. Hassan, T. K., and Rizkalla, S. H., “Bond Mechanism of NSM FRP Bars for Flexural Strengthening of Concrete Structures,” ACI Structural Journal, V. 101, No. 6, Nov.-Dec. 2004, pp. 830-839.

16. Hosen, M. A.; Jumaat, M. Z.; and Islam, A. B. M. S., “Side Near Surface Mounted (SNSM) Technique for Flexural Enhancement of RC Beams,” Materials & Design, V. 83, 2015, pp. 587-597. doi: 10.1016/j.matdes.2015.06.035

17. Hosen, A.; Alengaram, U. J.; Jumaat, M. Z.; Sulong, N. H. R.; and Darain, K. M., “Glass Fiber Reinforced Polymer (GFRP) Bars for Enhancing the Flexural Performance of RC Beams Using Side-NSM Technique,” Polymers, V. 9, No. 5, 2017, p. 180 doi: 10.3390/polym9050180

18. Sabau, C.; Popescu, C.; Sas, G.; Schmidt, J.; Blanksvärd, T.; Täljsten, B., “Strengthening of RC Beams Using Bottom and Side NSM Reinforcement,” Composites Part B: Engineering, V. 149, 2018.

19. Hosen, M. A.; Jumaat, M. Z.; Alengaram, U. J.; Ramli Sulong, N. H., “CFRP Strips for Enhancing Flexural Performance of RC Beams by SNSM Strengthening Technique,” Construction and Building Materials, V. 165, March 2018, pp. 28-44.

20. AS 3600-2018, “Concrete Structures,” Australian Standards, Sydney, Australia, 2018.

21. West System International, “Physical Properties of West System Epoxies,” https://atlcomposites.com.au/category/13/WEST-SYSTEM. (last accessed Apr. 2018)

22. Hanson. “Heidelberg Cement Group Pvt Ltd, Australia,” https://www.hanson.com.au. (last accessed May 2019)

23. AS 1012.3.1-2014, “Methods of Testing Concrete Determination of Properties Related to the Consistency of Concrete - Slump Test,” Standards Australia, Sydney, NSW, Australia, 2014.

24. AS 1012.9-2014, “Methods of Testing Concrete - Compressive Strength Tests - Concrete, Mortar and Grout Specimens,” Standards Australia, Sydney, NSW, Australia, 2014.

25. AS 1391-2020, “Metallic Materials - Tensile Testing - Method of Test at Room Temperature,” Standards Australia, Sydney, NSW, Australia, 2020.

26. Mateenbar, “Mateenbar Products Technical Data Sheet,” https://www.mateenbar.com/assets/Documents/Technical-Data-60.pdf. (last accessed Aug. 15, 2019)

27. ASTM D7205/D7205M-06-R2016, “Standard Test Method for Tensile Properties of Fiber Reinforced Polymer Matrix Composite Bars,” ASTM International, West Conshohocken, PA, 2016.

28. GRP Australia, “Design Guide Pultruded Sections,” https://www.grpaustralia.com.au/images/100-BR-04-GRP_Australia_DESIGN_GUIDE-Part1_D_compressed_1.pdf. (last accessed Apr. 2019)

29. ISO 527-4, “Determination of Tensile Properties of Plastics. Part 4: Test Conditions for Isotropic and Orthotropic Fibre-Reinforced Plastic Composites,” European Committee for Standardisation, Brussels, Belgium, 1997(R2014).

30. Foster, S. J., and Attard, M. M., “Experimental Tests on Eccentrically Loaded High Strength Concrete Columns,” ACI Structural Journal, V. 94, No. 3, May-June 1997, pp. 295-303.

31. Hadi, M. N. S.; Sarhan, M. M.; and Teh, L. H., “Behavior of Concrete Beams Reinforced with Steel Plates,” ACI Structural Journal, V. 115, No. 5, Sept. 2018, pp. 1307-1315. doi: 10.14359/51702445

32. Pessiki, S., and Pieroni, A., “Axial Load Behavior of Large Scale Spirally Reinforced High Strength Concrete Columns,” ACI Structural Journal, V. 94, No. 3, May-June 1997, pp. 304-31


ALSO AVAILABLE IN:

Electronic Structural Journal