Quantifying Conservativeness of Water-Soluble Chloride Testing

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Quantifying Conservativeness of Water-Soluble Chloride Testing

Author(s): Ahmed A. Ahmed and David Trejo

Publication: Materials Journal

Volume: 120

Issue: 2

Appears on pages(s): 13-24

Keywords: admixed chlorides; bound chlorides; carbonation; chloride release; chloride testing; specialty cements

DOI: 10.14359/51738499

Date: 3/1/2023

Abstract:
Proponents of water-soluble chloride testing argue that only chlorides in the pore solution contribute to corrosion and that this testing is more representative of free chlorides and therefore should be required. Proponents of acid-soluble chloride testing argue that although water-soluble testing may be more representative of free chlorides in the pore solution at early ages, bound chlorides can become unbound with time, making the water-soluble test unconservative for predicting later-age free chlorides. However, watersoluble testing likely unbinds some admixed chlorides during testing. If the number of chlorides released as part of the watersoluble test exceeds the number of chlorides released at later ages (that is, from carbonation), the water-soluble test should be sufficiently conservative. This research quantifies the release of admixed chlorides as a result of testing and carbonation. Results indicate that water-soluble testing is sufficiently conservative in most cases for assessing admixed chloride contents in various cementitious systems.

Related References:

Abrams, D. A., 1924, “Calcium Chloride as an Admixture in Concrete,” Structural Materials Research Laboratory, Chicago, IL, 57 pp.

ACI Committee 222, 2010, “Protection of Metals in Concrete Against Corrosion (ACI 222R-01) (Reapproved 2010),” American Concrete Institute, Farmington Hills, MI, 41 pp.

ACI Committee 222, 2019, “Guide to Protection of Reinforcing Steel in Concrete against Corrosion (ACI 222R-19),” American Concrete Institute, Farmington Hills, MI, 60 pp.

Ahmed, A. A., and Trejo, D., 2020, “Assessing Standard Tests for Admixed Chlorides in Calcium Aluminate and Calcium Sulfoaluminate Cement Systems,” ACI Materials Journal, V. 117, No. 1, Jan., pp. 71-84. doi: 10.14359/51720290

Ahmed, A. A., and Vaddey, N. P., 2021, “Reliability of Chloride Testing Results in Cementitious Systems Containing Admixed Chlorides,” Sustainable and Resilient Infrastructure, Apr., pp. 1-13. doi: 10.1080/23789689.2021.1917059

Ann, K. Y., and Cho, C.-G., 2014, “Corrosion Resistance of Calcium Aluminate Cement Concrete Exposed to a Chloride Environment,” Materials (Basel), V. 7, No. 2, pp. 887-898. doi: 10.3390/ma7020887

Ann, K. Y.; Hwang, J. P.; Kim, S. H.; and Jang, I. L., 2010a, “Effect of Calcium Aluminate Cement in Mitigating the Corrosion of Steel in Concrete,” 2nd International Symposium on Service Life Design for Infrastructure, Delft, the Netherlands, pp. 699-705.

Ann, K. Y.; Kim, T. S.; Kim, J. H.; and Kim, S. H., 2010b, “The Resistance of High Alumina Cement Against Corrosion of Steel in Concrete,” Construction and Building Materials, V. 24, No. 8, pp. 1502-1510. doi: 10.1016/j.conbuildmat.2010.01.022

Arya, C.; Buenfeld, N. R.; and Newman, J. B., 1987, “Assessment of Simple Methods of Determining the Free Chloride Ion Content of Cement Paste,” Cement and Concrete Research, V. 17, No. 6, pp. 907-918. doi: 10.1016/0008-8846(87)90079-2

Arya, C.; Buenfeld, N. R.; and Newman, J. B., 1990, “Factors Influencing Chloride-Binding in Concrete,” Cement and Concrete Research, V. 20, No. 2, pp. 291-300. doi: 10.1016/0008-8846(90)90083-A

ASTM C114-18, 2018, “Standard Test Methods for Chemical Analysis of Hydraulic Cement,” ASTM International, West Conshohocken, PA.

ASTM C305-14, 2014, “Standard Practice for Mechanical Mixing of Hydraulic Cement Pastes and Mortars of Plastic Consistency,” ASTM International, West Conshohocken, PA.

ASTM C1152/C1152M-04, 2004, “Standard Test Method for Acid-Soluble Chloride in Mortar and Concrete,” ASTM International, West Conshohocken, PA.

ASTM C1218/C1218M-17, 2017, “Standard Test Method for Water-Soluble Chloride in Mortar and Concrete,” ASTM International, West Conshohocken, PA.

ASTM D1193-06(2018), 2018, “Standard Specification for Reagent Water,” ASTM International, West Conshohocken, PA.

ASTM E104-02, 2022, “Standard Practice for Maintaining Constant Relative Humidity by Means of Aqueous Solutions,” ASTM International, West Conshohocken, PA.

Barneyback, R. S. Jr., and Diamond, S., 1981, “Expression and Analysis of Pore Fluids From Hardened Cement Pastes and Mortars,” Cement and Concrete Research, V. 11, No. 2, pp. 279-285. doi: 10.1016/0008-8846(81)90069-7

Blenkinsop, R. D.; Currell, B. R.; Midgley, H. G.; and Parsonage, J. R., 1985, “The Carbonation of High Alumina Cement, Part I,” Cement and Concrete Research, V. 15, No. 2, pp. 276-284. doi: 10.1016/0008-8846(85)90039-0

Canonico, F.; Buzzi, L.; and Schäffel, P., 2012, “Durability Properties of Concrete Based on Industrial Calcium Sulfoaluminate Cement,” International Congress on the Durability of Concrete, Trondheim, Norway.

CPC-18, 1988, “Measurement of Hardened Concrete Carbonation Depth,” RILEM Recommendations for the Testing and Use of Constructions Materials, RILEM, Champs-sur-Marne, France, pp. 56-58.

Dhir, R. K.; Jones, M. R.; and Ahmed, H. E. H., 1990, “Determination of Total and Soluble Chlorides in Concrete,” Cement and Concrete Research, V. 20, No. 4, pp. 579-590. doi: 10.1016/0008-8846(90)90100-C

Fernández-Carrasco, L.; Puertas, F.; Blanco-Varela, M.; and Vázquez, T., 2001, “Carbonation of Calcium Aluminate Cement Pastes,” Materiales de Construcción, V. 51, No. 263-264, pp. 127-136. doi: 10.3989/mc.2001.v51.i263-264.358

Florea, M. V. A., and Brouwers, H. J. H., 2012, “Chloride Binding Related to Hydration Products: Part I: Ordinary Portland Cement,” Cement and Concrete Research, V. 42, No. 2, pp. 282-290. doi: 10.1016/j.cemconres.2011.09.016

Geng, J.; Easterbrook, D.; Liu, Q. F.; and Li, L. Y., 2016, “Effect of Carbonation on Release of Bound Chlorides in Chloride-Contaminated Concrete,” Magazine of Concrete Research, V. 68, No. 7, pp. 353-363. doi: 10.1680/jmacr.15.00234

Goñi, S. A., and Guerrero, A., 2003, “Accelerated Carbonation of Friedel’s Salt in Calcium Aluminate Cement Paste,” Cement and Concrete Research, V. 33, No. 1, pp. 21-26. doi: 10.1016/S0008-8846(02)00910-9

Haque, M. N., and Kayyali, O. A., 1995, “Free and Water Soluble Chloride in Concrete,” Cement and Concrete Research, V. 25, No. 3, pp. 531-542. doi: 10.1016/0008-8846(95)00042-B

Hirao, H.; Yamada, K.; Takahashi, H.; and Zibara, H., 2005, “Chloride Binding of Cement Estimated by Binding Isotherms of Hydrates,” Journal of Advanced Concrete Technology, V. 3, No. 1, pp. 77-84. doi: 10.3151/jact.3.77

Ioannou, S.; Paine, K.; Reig, L.; and Quillin, K., 2015, “Performance Characteristics of Concrete Based on a Ternary Calcium Sulfoaluminate–Anhydrite–Fly Ash Cement,” Cement and Concrete Composites, V. 55, pp. 196-204. doi: 10.1016/j.cemconcomp.2014.08.009

Longuet, P.; Burglen, L.; and Zelwer, A., 1973, “La Phase Liquide du Ciment Hydrate, Rev des Materiaux de Constructions et des Travaux Publics,” Ciments et Betons, V. 676, pp. 35-41.

Mesbah, A.; Cau-dit-Coumes, C.; Renaudin, G.; Frizon, F.; and Leroux, F., 2012, “Uptake of Chloride and Carbonate Ions by Calcium Monosulfoaluminate Hydrate,” Cement and Concrete Research, V. 42, No. 8, pp. 1157-1165. doi: 10.1016/j.cemconres.2012.05.012

Nishikawa, T.; Suzuki, K.; Ito, S.; Sato, K.; and Takebe, T., 1992, “Decomposition of Synthesized Etrringite by Carbonation,” Cement and Concrete Research, V. 22, No. 1, pp. 6-14. doi: 10.1016/0008-8846(92)90130-N

Page, C. L., and Vennesland, Ø., 1983, “Pore Solution Composition and Chloride Binding Capacity of Silica-Fume Cement Pastes,” Materiales de Construcción, V. 16, No. 1, pp. 19-25.

Pavlík, V., 2000, “Water Extraction of Chloride, Hydroxide and Other Ions from Hardened Cement Pastes,” Cement and Concrete Research, V. 30, No. 6, pp. 895-906. doi: 10.1016/S0008-8846(00)00261-1

Pérez, M.; Vázquez, T.; and Trivino, F., 1983, “Study of Stabilized Phases in High Alumina Cement Mortars Part I Hydration at Elevated Temperatures Followed by Carbonation,” Cement and Concrete Research, V. 13, No. 6, pp. 759-770. doi: 10.1016/0008-8846(83)90077-7

Plusquellec, G.; Geiker, M. R.; Lindgård, J.; Duchesne, J.; Fournier, B.; and De Weerdt, K., 2017, “Determination of the pH and the Free Alkali Metal Content in the Pore Solution of Concrete: Review and Experimental Comparison,” Cement and Concrete Research, V. 96, pp. 13-26. doi: 10.1016/j.cemconres.2017.03.002

Robl, T. L.; Graham, U. M.; Taulbee, D. N.; and Giles, W., 1996, “The Effect of Carbonation Reactions on the Long-Term Stability of Products Made From Dry FGD Materials,” Report No. CONF-960376, 211th American Chemical Society (ACS) National Meeting, New Orleans, LA.

Sanjuán, M. A., 1997, “Formation of Chloroaluminates in Calcium Aluminate Cements Cured at High Temperatures and Exposed to Chloride Solutions,” Journal of Materials Science, V. 32, No. 23, pp. 6207-6213. doi: 10.1023/A:1018624824702

Shakouri, M.; Trejo, D.; Vaddey, N. P.; and Isgor, O. B., 2018, “Development of Empirical Models for Chloride Binding in Cementitious Systems Containing Admixed Chlorides,” Construction and Building Materials, V. 189, Nov., pp. 157-169.

Suryavanshi, A. K., and Swamy, R. N., 1996, “Stability of Friedel’s Salt in Carbonated Concrete Structural Elements,” Cement and Concrete Research, V. 26, No. 5, pp. 729-741. doi: 10.1016/S0008-8846(96)85010-1

Trejo, D., and Ahmed, A. A., 2019, “Adopting Auto-Titration to Assess Chlorides in Concrete,” ACI Materials Journal, V. 116, No. 3, May, pp. 43-52.

Trejo, D.; Vaddey, N. P.; and Shakouri, M., 2019, “Factors Influencing Chloride Test Results of Cementitious Systems,” ACI Materials Journal, V. 116, No. 1, Jan., pp. 135-145. doi: 10.14359/51712240

Vasudevan, G., and Trejo, D., 2022, “Suitability of CPC-18 and Carbonation of Specialty Cementitious Systems,” ACI Materials Journal, V. 119, No. 3, May, pp. 79-90.

Vesikari, E., 2009, “Carbonation and Chloride Penetration in Concrete With Special Objective of Service Life Modelling by the Factor Approach,” VTT Technical Research Centre of Finland, Espoo, Finland.

Winnefeld, F., and Lothenbach, B., 2010, “Hydration of Calcium Sulfoaluminate Cements—Experimental Findings and Thermodynamic Modelling,” Cement and Concrete Research, V. 40, No. 8, pp. 1239-1247. doi: 10.1016/j.cemconres.2009.08.014

Zajac, M.; Skocek, J.; Bullerjahn, F.; and Haha, M. B., 2016, “Effect of Retarders on the Early Hydration of Calcium-Sulpho-Aluminate (CSA) Type Cements,” Cement and Concrete Research, V. 84, pp. 62-75. doi: 10.1016/j.cemconres.2016.02.014

Zhang, L., and Glasser, F. P., 2002, “Hydration of Calcium Sulfoaluminate Cement at Less Than 24 h,” Advances in Cement Research, V. 14, No. 4, pp. 141-155. doi: 10.1680/adcr.2002.14.4.141