Design of Ambient-Cured Alkali-Activated Reactive Powder Concrete Using Taguchi Method

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Design of Ambient-Cured Alkali-Activated Reactive Powder Concrete Using Taguchi Method

Author(s): Nabeel A. Farhan, M. Neaz Sheikh, and Muhammad N. S. Hadi

Publication: Materials Journal

Volume: 120

Issue: 2

Appears on pages(s): 3-12

Keywords: alkaline activator; compressive strength; Taguchi method; ultra-high-strength concrete

DOI: 10.14359/51738489

Date: 3/1/2023

Abstract:
In this paper, the Taguchi method was used to identify the optimum mixture proportions of alkali-activated reactive powder concrete (AARPC) by considering the most influential parameters. Five main parameters, including binder content, alkaline activator-binder ratio (Al-binder), binder-fine aggregate ratio, sodium silicate to sodium hydroxide ratio (Na2SiO3-NaOH), and sodium hydroxide (NaOH) concentration, were considered in the mixture design. A total of 18 trial batches were designed according to the L18 array obtained from the Taguchi method. The results showed that the highest average compressive strength was 110.9 MPa (16.08 ksi) and the lowest average compressive strength was 50.6 MPa (7.34 ksi). The test results of the 18 trial batches were then evaluated by the analysis of variance (ANOVA) method to determine the optimum level of each parameter. It was found that specimens with a binder content of 700 kg/m3 (0.025 lb/in.3), Al-binder ratio of 0.3, binder-fine aggregate ratio of 0.8, Na2SiO3-NaOH ratio of 2, and NaOH concentration of 14 M produced the highest 28-day compressive strength (116.77 MPa [16.94 ksi]) at the ambient curing conditions.

Related References:

1. Farhan, N. A.; Sheikh, M. N.; and Hadi, M. N. S., “Behaviour of Ambient Cured Steel Fibre Reinforced Geopolymer Concrete Columns under Axial and Flexural Loads,” Structures, V. 15, Aug. 2018, pp. 184-195. doi: 10.1016/j.istruc.2018.07.001

2. McLellan, B. C.; Williams, R. P.; Lay, J.; van Riessen, A.; and Corder, G. D., “Costs and Carbon Emissions for Geopolymer Pastes in Comparison to Ordinary Portland Cement,” Journal of Cleaner Production, V. 19, No. 9-10, June-July 2011, pp. 1080-1090. doi: 10.1016/j.jclepro.2011.02.010

3. Canadell, P., and Raupach, M., “Global Carbon Report: Emissions Will Hit New Heights in 2014,” The Conversation, Sept. 21, 2014, http://theconversation.com/global-carbon-report-emissions-will-hit-new-heights-in-2014-31834. (last accessed March 1, 2023)

4. Farhan, N. A.; Sheikh, M. N.; and Hadi, M. N. S., “Experimental Investigation on the Effect of Corrosion on the Bond between Reinforcing Steel Bars and Fibre Reinforced Geopolymer Concrete,” Structures, V. 14, June 2018, pp. 251-261. doi: 10.1016/j.istruc.2018.03.013

5. Farhan, N. A.; Sheikh, M. N.; and Hadi, M. N. S., “Behavior of Ambient-Cured Geopolymer Concrete Columns under Different Loads,” ACI Structural Journal, V. 115, No. 5, Sept. 2018, pp. 1419-1429. doi: 10.14359/51702250

6. Al‐Hedad, A. S. A.; Farhan, N. A.; Zhang, M.; Sheikh, M. N.; and Hadi, M. N. S., “Effect of Geogrid Reinforcement on the Drying Shrinkage and Thermal Expansion of Geopolymer Concrete,” Structural Concrete, V. 21, No. 3, June 2020, pp. 1029-1039. doi: 10.1002/suco.201900299

7. Farhan, N. A.; Sheikh, M. N.; and Hadi, M. N. S., “Engineering Properties of Ambient Cured Alkali-Activated Fly Ash–Slag Concrete Reinforced with Different Types of Steel Fiber,” Journal of Materials in Civil Engineering, ASCE, V. 30, No. 7, July 2018, p. 04018142. doi: 10.1061/(ASCE)MT.1943-5533.0002333

8. Ken, P. W.; Ramli, M.; and Ban, C. C., “An Overview on the Influence of Various Factors on the Properties of Geopolymer Concrete Derived from Industrial By-Products,” Construction and Building Materials, V. 77, Feb. 2015, pp. 370-395. doi: 10.1016/j.conbuildmat.2014.12.065

9. Waldmann, D., and Thapa, V. B., “A Short Review on Alkali-Activated Binders and Geopolymer Binders,” Vielfalt im Massivbau: Festschrift zum 65. Geburtstag von Prof. Dr.-Ing. Jürgen Schnell, M. Pahn, C. Thiele, and C. Glock, eds., Ernst & Sohn, Berlin, Germany, 2018, pp. 576-591.

10. Barcelo, L.; Kline, J.; Walenta, G.; and Gartner, E., “Cement and Carbon Emissions,” Materials and Structures, V. 47, No. 6, June 2014, pp. 1055-1065. doi: 10.1617/s11527-013-0114-5

11. Reed, M.; Lokuge, W.; and Karunasena, W., “Fibre-Reinforced Geopolymer Concrete with Ambient Curing for In Situ Applications,” Journal of Materials Science, V. 49, No. 12, June 2014, pp. 4297-4304. doi: 10.1007/s10853-014-8125-3

12. Farhan, N. A.; Sheikh, M. N.; and Hadi, M. N. S., “Investigation of Engineering Properties of Normal and High Strength Fly Ash Based Geopolymer and Alkali-Activated Slag Concrete Compared to Ordinary Portland Cement Concrete,” Construction and Building Materials, V. 196, Jan. 2019, pp. 26-42. doi: 10.1016/j.conbuildmat.2018.11.083

13. Farhan, N. A.; Sheikh, M. N.; and Hadi, M. N. S., “Effect of Steel Fiber on Engineering Properties of Geopolymer Concrete,” ACI Materials Journal, V. 117, No. 3, May 2020, pp. 29-40.

14. Hadi, M. N. S.; Farhan, N. A.; and Sheikh, M. N., “Design of Geopolymer Concrete with GGBFS at Ambient Curing Condition Using Taguchi Method,” Construction and Building Materials, V. 140, June 2017, pp. 424-431. doi: 10.1016/j.conbuildmat.2017.02.131

15. Deb, P. S.; Nath, P.; and Sarker, P. K., “The Effects of Ground Granulated Blast-Furnace Slag Blending with Fly Ash and Activator Content on the Workability and Strength Properties of Geopolymer Concrete Cured at Ambient Temperature,” Materials & Design, V. 62, Oct. 2014, pp. 32-39.

16. Olivia, M., and Nikraz, H., “Properties of Fly Ash Geopolymer Concrete Designed by Taguchi Method,” Materials & Design, V. 36, Apr. 2012, pp. 191-198.

17. Nazari, A.; Khanmohammadi, H.; Amini, M.; Hajiallahyari, H.; and Rahimi, A., “Production Geopolymers by Portland Cement: Designing the Main Parameters’ Effects on Compressive Strength by Taguchi Method,” Materials & Design, V. 41, Oct. 2012, pp. 43-49. doi: 10.1016/j.matdes.2012.04.045

18. Khalaj, G.; Hassani, S. E. S.; Khezrloo, A.; and Haratifar, E., “Split Tensile Strength of OPC-Based Geopolymers: Application of DOE Method in Evaluating the Effect of Production Parameters and Their Optimum Condition,” Ceramics International, V. 40, No. 7, Part B, Aug. 2014, pp. 10945-10952. doi: 10.1016/j.ceramint.2014.03.094

19. Mijarsh, M. J. A.; Megat Johari, M. A.; and Ahmad, Z. A., “Synthesis of Geopolymer from Large Amounts of Treated Palm Oil Fuel Ash: Application of the Taguchi Method in Investigating the Main Parameters Affecting Compressive Strength,” Construction and Building Materials, V. 52, Feb. 2014, pp. 473-481. doi: 10.1016/j.conbuildmat.2013.11.039

20. Türkmen, İ.; Gül, R.; and Çelik, C., “A Taguchi Approach for Investigation of Some Physical Properties of Concrete Produced from Mineral Admixtures,” Building and Environment, V. 43, No. 6, June 2008, pp. 1127-1137. doi: 10.1016/j.buildenv.2007.02.005

21. Lee, M.-G.; Wang, Y.-C.; and Chiu, C.-T., “A Preliminary Study of Reactive Powder Concrete as a New Repair Material,” Construction and Building Materials, V. 21, No. 1, Jan. 2007, pp. 182-189. doi: 10.1016/j.conbuildmat.2005.06.024

22. Al-Tikrite, A., and Hadi, M. N. S., “Mechanical Properties of Reactive Powder Concrete Containing Industrial and Waste Steel Fibres at Different Ratios under Compression,” Construction and Building Materials, V. 154, Nov. 2017, pp. 1024-1034. doi: 10.1016/j.conbuildmat.2017.08.024

23. Elchalakani, M.; Karrech, A.; Dong, M.; Mohamed Ali, M. S.; and Yang, B., “Experiments and Finite Element Analysis of GFRP Reinforced Geopolymer Concrete Rectangular Columns Subjected to Concentric and Eccentric Axial Loading,” Structures, V. 14, June 2018, pp. 273-289. doi: 10.1016/j.istruc.2018.04.001

24. ASA, “Ground Granulated Blast Furnace Slag (GGBFS),” Australasian (Iron & Steel) Slag Association, Wollongong, NSW, Australia, https://www.asa-inc.org.au/products/ground-granulated-blast-furnace-slag. (last accessed March 1, 2023)

25. PQ Australia, “Sodium Silicate,” PQ Australia Pty Ltd., Chipping Norton, NSW, Australia, http://www.pqcorp.com/products/. (last accessed March 10, 2023)

26. Nutek, Inc., “Qualitek-4: IBM/Compatible Software for Automatic Design and Analysis of Taguchi Experiments,” Nutek, Inc., Bloomfield Hills, MI, http://nutek-us.com/wp-q4w.html. (last accessed March 10, 2023)

27. Ross, P. J., Taguchi Techniques for Quality Engineering: Loss Function, Orthogonal Experiments, Parameter and Tolerance Design, McGraw Hill Professional, New York, 1996.

28. AS 1012.9-1999, “Methods of Testing Concrete. Method 9: Determination of the Compressive Strength of Concrete Specimens,” Standards Australia, Sydney, NSW, Australia, 1999, 10 pp.

29. Bernal, S. A., Mejíade Gutiérrez, R. M.; Pedraza, A. L.; Provis, J. L.; Rodriguez, E. D.; and Delvasto, S., “Effect of Binder Content on the Performance of Alkali-Activated Slag Concretes,” Cement and Concrete Research, V. 41, No. 1, Jan. 2011, pp. 1-8. doi: 10.1016/j.cemconres.2010.08.017

30. Humad, A. M.; Kothari, A.; Provis, J. L.; and Cwirzen, A., “The Effect of Blast Furnace Slag/Fly Ash Ratio on Setting, Strength, and Shrinkage of Alkali-Activated Pastes and Concretes,” Frontiers in Materials, V. 6, Feb. 2019, Article No. 9. doi: 10.3389/fmats.2019.00009

31. Farhan, N.; Sheikh, M. N.; and Hadi, M. N. S., “Design of Alkali Activated Concrete Using the Taguchi Method,” Mechanics of Structures and Materials XXIV: Proceedings of the 24th Australian Conference on the Mechanics of Structures and Materials, H. Hao and C. Zhang, eds., Perth, WA, Australia, 2016, pp. 465-469.

32. Liu, Y.; Zhu, W.; and Yang, E.-H., “Alkali-Activated Ground Granulated Blast-Furnace Slag Incorporating Incinerator Fly Ash as a Potential Binder,” Construction and Building Materials, V. 112, June 2016, pp. 1005-1012. doi: 10.1016/j.conbuildmat.2016.02.153

33. Puligilla, S., and Mondal, P., “Role of Slag in Microstructural Development and Hardening of Fly Ash-Slag Geopolymer,” Cement and Concrete Research, V. 43, Jan. 2013, pp. 70-80. doi: 10.1016/j.cemconres.2012.10.004

34. Saha, S., and Rajasekaran, C., “Enhancement of the Properties of Fly Ash Based Geopolymer Paste by Incorporating Ground Granulated Blast Furnace Slag,” Construction and Building Materials, V. 146, Aug. 2017, pp. 615-620. doi: 10.1016/j.conbuildmat.2017.04.139

35. Diaz-Loya, E. I.; Allouche, E. N.; and Vaidya, S., “Mechanical Properties of Fly-Ash-Based Geopolymer Concrete,” ACI Materials Journal, V. 108, No. 3, May-June 2011, pp. 300-306.

36. Marjanović, N.; Komljenović, M.; Baščarević, Z.; and Nikolić, V., “Improving Reactivity of Fly Ash and Properties of Ensuing Geopolymers through Mechanical Activation,” Construction and Building Materials, V. 57, Apr. 2014, pp. 151-162. doi: 10.1016/j.conbuildmat.2014.01.095


ALSO AVAILABLE IN:

Electronic Materials Journal