Title: ASTM F1554-20, "Standard Specification for Anchor Bolts, Steel, 36, 55, and 105-ksi Yield Strength."

Author(s): ASTM Subcommittee F16.02 on Steel Bolts, Nuts, Rivets and Washers

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI: 10.1520/F1554-20

Date: 1/1/2021

Abstract:
This specification covers the chemical, mechanical, and dimensional requirements, and associated test methods for straight and bent, headed and headless anchor bolts (also known as anchor rods) made of carbon, carbon boron, alloy, or high-strength low-alloy steel and having specified yield strengths. The anchor bolts are furnished in three strength grades, two thread classes, and various sizes, and are intended for anchoring structural supports to concrete foundations such as building columns, column supports for highway signs, street lighting and traffic signals, steel bearing plates, and similar applications. This specification, however, does not cover the requirements for mechanical expansion anchors, powder-activated nails or studs, and anchor bolts fabricated from deformed bars. The bolts shall adhere to specified elemental chemical compositions as examined by heat and product analysis. They shall also be tested for their conformance with mechanical properties such as tensile strength, yield strength, elongation, reduction of area, and stress area. The anchor bolts shall also meet specified values for nominal size, body diameter, bend section, length, bend angle, and coated length.