ASTM E8/E8M‑21, "Standard Test Methods for Tension Testing of Metallic Materials."

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ASTM E8/E8M‑21, "Standard Test Methods for Tension Testing of Metallic Materials."

Author(s): ASTM Subcommittee E28.04 on Uniaxial Testing

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI: 10.1520/E0008_E0008M-21

Date: 2/1/2021

Abstract:
These test methods cover the tension testing of metallic materials in any form at room temperature, specifically, the methods of determination of yield strength, yield point elongation, tensile strength, elongation, and reduction of area.