ASTM D3665-12(2017), "Standard Practice for Random Sampling of Construction Materials."

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ASTM D3665-12(2017), "Standard Practice for Random Sampling of Construction Materials."

Author(s): ASTM Subcommittee D04.30 on Methods of Sampling

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI: 10.1520/D3665-12R17

Date: 10/1/2017

Abstract:
This practice covers the determination of random locations (or timing) at which samples of construction materials can be taken. For the exact physical procedures for securing the sample, such as a description of the sampling tool, the number of increments needed for a sample, or the size of the sample, reference should be made to the appropriate standard method. The selection procedures in Section 6 utilize the table of four-digit numbers given in Table 1.