ASTM C900-19, "Standard Test Method for Pullout Strength of Hardened Concrete."

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ASTM C900-19, "Standard Test Method for Pullout Strength of Hardened Concrete."

Author(s): ASTM Subcommittee C09.64 on Nondestructive and In-Place Testing

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI: 10.1520/C0900-19

Date: 2/1/2020

Abstract:
This test method covers determination of the pullout strength of hardened concrete by measuring the force required to pull an embedded metal insert and the attached concrete fragment from a concrete test specimen or structure. The insert is either cast into fresh concrete or installed in hardened concrete. This test method does not provide statistical procedures to estimate other strength properties.