International Concrete Abstracts Portal

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ASTM C567/C567M-19, "Standard Test Method for Determining Density of Structural Lightweight Concrete."

Author(s): ASTM Subcommittee C09.21 on Lightweight Aggregates and Concrete

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI: 10.1520/C0567_C0567M-19

Date: 2/1/2020

Abstract: