ASTM C31/C31M-21a, "Standard Practice for Making and Curing Concrete Test Specimens in the Field."

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ASTM C31/C31M-21a, "Standard Practice for Making and Curing Concrete Test Specimens in the Field."

Author(s): ASTM Subcommittee C09.61 on Testing for Strength

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI: 10.1520/C0031_C0031M-21A

Date: 5/1/2021

Abstract:
This practice covers procedures for making and curing cylinder and beam specimens from representative samples of fresh concrete for a construction project.