ASTM C29/C29M-17a, "Standard Test Method for Bulk Density (“Unit Weight”) and Voids in Aggregate."

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ASTM C29/C29M-17a, "Standard Test Method for Bulk Density (“Unit Weight”) and Voids in Aggregate."

Author(s): ASTM Subcommittee C09.20 on Aggregates

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI: 10.1520/C0029_C0029M-17A

Date: 6/1/2017

Abstract:
This test method covers the determination of bulk density (“unit weight”) of aggregate in a compacted or loose condition, and calculated voids between particles in fine, coarse, or mixed aggregates based on the same determination. This test method is applicable to aggregates not exceeding 125 mm [5 in.] in nominal maximum size.