ASTM C192-19, "Standard Practice for Making and Curing Concrete Test Specimens in the Laboratory."

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ASTM C192-19, "Standard Practice for Making and Curing Concrete Test Specimens in the Laboratory."

Author(s): ASTM Subcommittee C09.61 on Testing for Strength

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI: 10.1520/C0192_C0192M-19

Date: 2/1/2020

Abstract:
This practice covers procedures for making and curing test specimens of concrete in the laboratory under accurate control of materials and test conditions using concrete that can be consolidated by rodding or vibration as described herein.