ASTM C1797-17, "Standard Specification for Ground Calcium Carbonate and Aggregate Mineral Fillers for use in Hydraulic Cement Concrete."

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ASTM C1797-17, "Standard Specification for Ground Calcium Carbonate and Aggregate Mineral Fillers for use in Hydraulic Cement Concrete."

Author(s): ASTM Subcommittee C09.20 on Aggregates

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI: 10.1520/C1797-17

Date: 1/1/2018

Abstract:
This specification covers ground calcium carbonate (GCC, a type of ground limestone) and other finely divided aggregate mineral filler (AMF) materials for use in concrete mixtures. It defines the types of GCC and AMF materials for use in concrete. If concrete in service is subject to sulfate exposure, fillers derived from ground limestone should not be used unless mitigation methods are used. This specification includes requirements with respect to chemical composition and physical properties, sampling, test methods, storage and inspection, packaging and package marking, certification, and manufacturer’s statement (mineral origin, nature, amount, and type of any processing or other additions made to the product).