ASTM C173/C173M-16, "Standard Test Method for Air Content of Freshly Mixed Concrete by the Volumetric Method."

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ASTM C173/C173M-16, "Standard Test Method for Air Content of Freshly Mixed Concrete by the Volumetric Method."

Author(s): ASTM Subcommittee C09.60 on Testing Fresh Concrete

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI: 10.1520/C0173_C0173M-16

Date: 3/1/2016

Abstract:
This test method covers determination of the air content of freshly mixed concrete containing any type of aggregate, whether it be dense, cellular, or lightweight.