Title: ASTM C1157/C1157M-20a, "Standard Performance Specification for Hydraulic Cement."

Author(s): ASTM Subcommittee C01.10 on Hydraulic Cements for General Concrete Construction

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI: 10.1520/C1157_C1157M-20A

Date: 1/1/2021

Abstract:
This performance specification covers hydraulic cements for both general and special applications. There are no restrictions on the composition of the cement or its constituents (see Note 1).