Title: ASTM C1074-19e1, "Standard Practice for Estimating Concrete Strength by the Maturity Method."

Author(s): ASTM Subcommittee C09.64 on Nondestructive and In-Place Testing

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI: 10.1520/C1074-19E01

Date: 7/1/2019

Abstract:
This practice provides a procedure for estimating concrete strength by means of the maturity method. The maturity index is expressed either in terms of the temperature-time factor or in terms of the equivalent age at a specified temperature.