ASTM C1012/C1012M-18b, "Standard Test Method for Length Change of Hydraulic-Cement Mortars Exposed to a Sulfate Solution."

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ASTM C1012/C1012M-18b, "Standard Test Method for Length Change of Hydraulic-Cement Mortars Exposed to a Sulfate Solution."

Author(s): ASTM Subcommittee C01.29 on Sulfate Resistance

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI: 10.1520/C1012_C1012M-18B

Date: 1/1/2019

Abstract:
This test method covers the determination of length change of mortar bars immersed in a sulfate solution. Mortar bars made using mortar described in Test Method C109/C109M are cured until they attain a compressive strength of 20.0 ± 1.0 MPa [3000 ± 150 psi], as measured using cubes made of the same mortar, before the bars are immersed.