ASTM A934/A934M-19, "Standard Specification for Epoxy-Coated Prefabricated Steel Reinforcing Bars."

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ASTM A934/A934M-19, "Standard Specification for Epoxy-Coated Prefabricated Steel Reinforcing Bars."

Author(s): ASTM Subcommittee A01.05 on Steel Reinforcement

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI: 10.1520/A0934_A0934M-19

Date: 6/1/2019

Abstract:
This specification covers deformed and plain steel reinforcing bars. Steel samples shall be blast cleaned and shall be coated with a protective fusion-bonded epoxy coating by electrostatic spray or other suitable method. The steel specimens shall undergo deformation test, holiday checks, bending tests, and cathodic disbondment test. The steels materials shall conform to the required values of coating thickness, continuity, flexibility, adhesion.