ASTM A820/A820M-16, "Standard Specification for Steel Fibers for Fiber-Reinforced Concrete."

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: ASTM A820/A820M-16, "Standard Specification for Steel Fibers for Fiber-Reinforced Concrete."

Author(s): ASTM Subcommittee A01.05 on Steel Reinforcement

Publication: Commentary Reference

Volume:

Issue:

Appears on pages(s):

Keywords:

DOI: 10.1520/A0820_A0820M-16

Date: 6/1/2016

Abstract:
This specification covers steel fibers intended for use in fiber-reinforced concrete. The fibers shall be straight or deformed and of Types I (cold-drawn wire), II (cut sheet), III (melt-extracted), IV (mill cut), and V ( modified cold-drawn wire). Tensile and bend tests of randomly-selected finished fibers shall be performed. Measurement of dimensions shall be performed and values should conform to permissible variations of length, nominal length, diameter, equivalent diameter, aspect ratio, and nominal aspect ratio. Guidelines for inspection, rejection, rehearing, certification, and packaging are also given.