Title: NEx insights

Author(s):

Publication: Concrete International

Volume: 44

Issue: 12

Appears on pages(s): 24-25

Keywords:

DOI: 10.14359/51738364

Date: 12/1/2022

Abstract:
Nonmetallic polymer-based materials are being increasingly deployed across multiple industries and offer new possibilities for construction. NEx was established to accelerate the use of nonmetallic materials and products in the building and construction sector.