One Year Closer to a Carbon-Neutral Cement Future

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: One Year Closer to a Carbon-Neutral Cement Future

Author(s): Michael Ireland

Publication: Concrete International

Volume: 44

Issue: 12

Appears on pages(s): 40-41

Keywords: roadmap, emission, construction, sustainability

DOI: 10.14359/51738359

Date: 12/1/2022

Abstract:
This past October marked the 1-year anniversary of the Portland Cement Association (PCA) Roadmap to Carbon Neutrality. The Roadmap has specific levers and actions outlined for the private sector at every step and while new opportunities to reduce emissions will certainly emerge, this document provides tangible actions to realize a more sustainable built environment.