Shear Strength of GFRP-Reinforced Concrete Squat Walls: A Strut-and-Tie Model

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Strength of GFRP-Reinforced Concrete Squat Walls: A Strut-and-Tie Model

Author(s): Islam Shabana, Ahmed Sabry Farghaly, and Brahim Benmokrane

Publication: Structural Journal

Volume: 120

Issue: 2

Appears on pages(s): 61-75

Keywords: design codes; experimental and analytical modeling; glass fiber-reinforced polymer (GFRP) reinforcing bars; load paths; reinforced concrete (RC); seismic; shear strength; squat walls; strut-and-tie

DOI: 10.14359/51738347

Date: 3/1/2023

Abstract:
Increasing interest in the use of fiber-reinforced polymer (FRP) reinforcement for reinforced concrete (RC) structures has made it clear that insufficient information about the seismic performance of such structures is currently available for practicing engineers. This paper summarizes the results of seven full-scale pseudo-static cyclic tests of squat concrete walls reinforced with glass FRP (GFRP) bars and spirals. Test variables were the wall aspect ratio, the axial load level, and the web reinforcement amount. The test results were analyzed and used to develop a strut-and-tie model (STM) that accurately estimates the peak shear strength and reflects the effects of various influential parameters. The model was achieved by idealizing the shear-transfer mechanism of the web reinforcement using a statically indeterminate truss, and that of the concrete using a direct strut-and-tie system representing the tiedarch action developed through the web. Streamlined expressions were formulated to calculate the shear-transfer capacity of the two mechanisms, and due to lack of a sufficient experimental database, a series of 90 finite element models were conducted to assist in formulating the truss expression. The validity of the developed STM and expressions was examined against the results of the tested walls, showing great accuracy and uniformity. Comparisons were also made with predictions from STMs in ACI 318-19, CSA S806-12, and Eurocode 2 to indicate the accuracy of the developed model.

Related References:

ACI Committee 318, 2019, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 624 pp.

Arafa, A.; Farghaly, A. S.; and Benmokrane, B., 2018a, “Effect of Web Reinforcement on the Seismic Response of Concrete Squat Walls Reinforced with Glass-FRP Bars,” Engineering Structures, V. 174, pp. 712-723. doi: 10.1016/j.engstruct.2018.07.092

Arafa, A.; Farghaly, A. S.; and Benmokrane, B., 2018b, “Experimental Behavior of GFRP-Reinforced Concrete Squat Walls Subjected to Simulated Earthquake Load,” Journal of Composites for Construction, ASCE, V. 22, No. 2, p. 04018003. doi: 10.1061/(ASCE)CC.1943-5614.0000836

Baek, J. W.; Park, H. G.; Lee, J. H.; and Bang, C. J., 2017, “Cyclic Loading Test for Walls of Aspect Ratio 1.0 and 0.5 with Grade 550 MPa (80 ksi) Shear Reinforcing Bars,” ACI Structural Journal, V. 114, No. 4, July-Aug., pp. 969-982. doi: 10.14359/51689680

Collins, M. P., and Mitchell, D., 1997, Prestressed Concrete Structures, Response Publications, Quebec, QC, Canada, 766 pp.

CSA A23.3-14, 2014, “Design of Concrete Structures,” CSA Group, Toronto, ON, Canada, 290 pp.

CSA S806-12, 2012, “Design and Construction of Building Components with Fibre-Reinforced Polymers,” CSA Group, Toronto, ON, Canada, 208 pp.

Deng, X.; Koutromanos, I.; Murcia-Delso, J.; and Panagiotou, M., 2021, “Nonlinear Truss Models for Strain-Based Seismic Evaluation of Planar RC Walls,” Earthquake Engineering & Structural Dynamics, V. 50, No. 11, pp. 2939-2960. doi: 10.1002/eqe.3480

Devine, R. D.; Barbachyn, S. M.; Thrall, A. P.; and Kurama, T. C., 2020, “Effect of Aspect Ratio, Flanges, and Material Strength on Squat Reinforced Concrete Shear Walls,” ACI Structural Journal, V. 117, No. 5, Sept., pp. 283-300.

El-Gendy, M. G., and El-Salakawy, E. F., 2020, “GFRP Shear Reinforcement for Slab-Column Edge Connections Subjected to Reversed Cyclic Lateral Load,” Journal of Composites for Construction, ASCE, V. 24, No. 2, p. 04020003. doi: 10.1061/(ASCE)CC.1943-5614.0001000

EN 1992-1-1:2004, “Eurocode 2—Design of Concrete Structures - Part 1-1 General Rules and Rules for Buildings,” European Committee for Standardization, Brussels, Belgium, 225 pp.

Gupta, A., and Rangan, B. V., 1998, “High-Strength Concrete (HSC) Structural Walls,” ACI Structural Journal, V. 95, No. 2, Mar.-Apr., pp. 194-204.

Hsu, T. T. C., and Mo, Y. L., 1985, “Softening of Concrete in Low-Rise Shearwalls,” ACI Structural Journal, V. 82, No. 6, Nov.-Dec., pp. 883-889.

Hwang, S. J.; Fang, W. H.; Lee, H. J.; and Yu, H. W., 2001, “Analytical Model for Predicting Shear Strength of Squat Walls,” Journal of Structural Engineering, ASCE, V. 127, No. 1, pp. 43-50. doi: 10.1061/(ASCE)0733-9445(2001)127:1(43)

Kassem, W., 2015, “Shear Strength of Squat Walls: A Strut-and-Tie Model and Closed-Form Design Formula,” Engineering Structures, V. 84, pp. 430-438. doi: 10.1016/j.engstruct.2014.11.027

Kharal, Z.; Carrette, J. K.; and Sheikh, S. A., 2021, “Large Concrete Columns Internally Reinforced with GFRP Spirals Subjected to Seismic Loads,” Journal of Composites for Construction, ASCE, V. 25, No. 3, p. 04021014. doi: 10.1061/(ASCE)CC.1943-5614.0001121

Koutromanos, I., and Farhadi, M., 2018, “FE-MultiPhys: A Finite Element Program for Nonlinear Analysis of Continua and Structures,” Report No. CE/VPI-ST-18/02, Virginia Polytechnic Institute and State University, Blacksburg, VA, 80 pp.

Lefas, I. D.; Kotsovos, M. D.; and Ambraseys, N. N., 1990, “Behavior of Reinforced Concrete Structural Walls: Strength, Deformation Characteristics, and Failure Mechanism,” ACI Structural Journal, V. 87, No. 1, Jan.-Feb., pp. 23-31.

LSTC, 2007, LS-DYNA Manual, Livermore Software Technology Corporation, Livermore, CA.

Lu, Y., and Panagiotou, M., 2014, “Three-Dimensional Cyclic Beam-Truss Model for Nonplanar Reinforced Concrete Walls,” Journal of Structural Engineering, ASCE, V. 140, No. 3, p. 04013071. doi: 10.1061/(ASCE)ST.1943-541X.0000852

Luna, B. N., and Whittaker, A. S., 2019, “Peak Strength of Shear-Critical Reinforced Concrete Walls,” ACI Structural Journal, V. 116, No. 2, Mar., pp. 257-266. doi: 10.14359/51712280

Mohamed, N.; Farghaly, A. S.; Benmokrane, B.; and Neale, K. W., 2014a, “Experimental Investigation of Concrete Shear Walls Reinforced with Glass Fiber–Reinforced Bars under Lateral Cyclic Loading,” Journal of Composites for Construction, ASCE, V. 18, No. 3, p. A4014001. doi: 10.1061/(ASCE)CC.1943-5614.0000393

Mohamed, N.; Farghaly, A. S.; Benmokrane, B.; and Neale, K. W., 2014b, “Drift Capacity Design of Shear Walls Reinforced with Glass Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 111, No. 6, Nov.-Dec., pp. 1397-1406. doi: 10.14359/51687099

Mun, J. H., and Yang, K. H., 2016, “Load Capacity of Squat RC Shear Walls by Strut-and-Tie Model,” Magazine of Concrete Research, V. 68, No. 24, pp. 1265-1277. doi: 10.1680/jmacr.15.00523

Paulay, T., and Priestley, M. J. N., 1995, Seismic Design of Reinforced Concrete and Masonry Buildings, John Wiley & Sons, Inc., New York, 744 pp.

Pultrall Inc., 2018, “Data Sheet—V-ROD GFRP Rebars,” Thetford Mines, Quebec, QC, Canada.

Shabana, I. S.; Farghaly, A. S.; and Benmokrane, B., 2021, “Effect of the Axial Load and Web Reinforcement Ratio on the Seismic Behavior and Strength of GFRP-RC Squat Walls,” ACI Structural Journal, V. 118, No. 4, July, pp. 109-121.

Tobbi, H.; Farghaly, A. S.; and Benmokrane, B., 2014, “Strength Model for Concrete Columns Reinforced with Fiber-Reinforced Polymer Bars and Ties,” ACI Structural Journal, V. 111, No. 4, July-Aug., pp. 789-798. doi: 10.14359/51686630

Vecchio, F. J., and Collins, M. P., 1986, “The Modified Compression-Field Theory for Reinforced Concrete Elements Subjected to Shear,” ACI Journal Proceedings, V. 83, No. 2, Mar.-Apr., pp. 219-231.

Whyte, C. A., and Stojadinovic, B., 2014, “Effect of Ground Motion Sequence on Response of Squat Reinforced Concrete Shear Walls,” Journal of Structural Engineering, ASCE, V. 140, No. 8, p. A4014004. doi: 10.1061/(ASCE)ST.1943-541X.0000912

Wight, J. K., and MacGregor, J. G., 2009, Reinforced Concrete: Mechanics and Design, sixth edition, Pearson Prentice Hall, Upper Saddle River, NJ, 1157 pp.


ALSO AVAILABLE IN:

Electronic Structural Journal