Precast Concrete Wall Panels Incorporating Mixed Recycled Aggregates

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Precast Concrete Wall Panels Incorporating Mixed Recycled Aggregates

Author(s): Xiaoguang Chen, Zeger Sierens, Elke Gruyaert, and Jiabin Li

Publication: Materials Journal

Volume: 120

Issue: 1

Appears on pages(s): 75-88

Keywords: aesthetic characteristics; architectural precast concrete; mechanical property; mixed recycled aggregate (MRA); natural carbonation; resilience; self-consolidating concrete (SCC); surface electrical resistivity; sustainability

DOI: 10.14359/51737333

Date: 1/1/2023

Abstract:
Mixed recycled aggregate (MRA) is considered a sustainable construction material, and its use in precast concrete is currently banned due to its poor engineering performance. This paper aims to evaluate the feasibility of partial replacement of natural coarse aggregate with MRA in self-consolidating concrete (SCC) for manufacturing architectural precast concrete sandwich wall panels. To this end, five MRAs from recycling plants were characterized, out of which two were selected to develop SCC. SCC mixtures with three replacement levels and three water compensation degrees were produced, and their physical, mechanical, durability, and aesthetic properties were examined. The results showed that the incorporation of MRA dominated the mechanical properties of SCC, while the water compensation degree primarily affected the flowability and carbonation resistance. The presence of MRA had no considerable effect on the aesthetic characteristics. Up to 10% MRA in weight of total aggregates could be used in precast SCC.

Related References:

1. Ospitia, N.; Tsangouri, E.; Pourkazemi, A.; Stiens, J. H.; and Aggelis, D. G., “NDT Inspection on TRC and Precast Concrete Sandwich Panels: A Review,” Construction and Building Materials, V. 296, Aug. 2021, Article No. 123622. doi: 10.1016/j.conbuildmat.2021.123622

2. Lee, B.-J., and Pessiki, S., “Thermal Performance Evaluation of Precast Concrete Three-Wythe Sandwich Wall Panels,” Energy and Buildings, V. 38, No. 8, Aug. 2006, pp. 1006-1014. doi: 10.1016/j.enbuild.2005.11.014

3. NBN EN 12620:2013, “Aggregates for Concrete,” Bureau of Normalization, Brussels, Belgium, 2013.

4. Silva, R. V.; de Brito, J.; and Dhir, R. K., “Properties and Composition of Recycled Aggregates from Construction and Demolition Waste Suitable for Concrete Production,” Construction and Building Materials, V. 65, Aug. 2014, pp. 201-217. doi: 10.1016/j.conbuildmat.2014.04.117

5. Dhir, R. K.; de Brito, J.; Silva, R. V.; and Lye, C. Q., Sustainable Construction Materials: Recycled Aggregates, Woodhead Publishing, Sawston, UK, 2019, 652 pp.

6. Santos, S.; da Silva, P. R.; and de Brito, J., “Self-Compacting Concrete with Recycled Aggregates – A Literature Review,” Journal of Building Engineering, V. 22, Mar. 2019, pp. 349-371. doi: 10.1016/j.jobe.2019.01.001

7. Rodríguez-Robles, D.; García-González, J.; Juan-Valdés, A.; Morán-del Pozo, J. M.; and Guerra-Romero, M. I., “Quality Assessment of Mixed and Ceramic Recycled Aggregates from Construction and Demolition Wastes in the Concrete Manufacture According to the Spanish Standard,” Materials (Basel), V. 7, No. 8, Aug. 2014, pp. 5843-5857. doi: 10.3390/ma7085843

8. Khoury, E.; Ambrós, W.; Cazacliu, B.; Sampaio, C. H.; and Remond, S., “Heterogeneity of Recycled Concrete Aggregates, An Intrinsic Variability,” Construction and Building Materials, V. 175, June 2018, pp. 705-713. doi: 10.1016/j.conbuildmat.2018.04.163

9. Gonzalez-Corominas, A., and Etxeberria, M., “Properties of High Performance Concrete Made with Recycled Fine Ceramic and Coarse Mixed Aggregates,” Construction and Building Materials, V. 68, Oct. 2014, pp. 618-626. doi: 10.1016/j.conbuildmat.2014.07.016

10. López Gayarre, F.; López-Colina, C.; Serrano, M. A.; and López-Martínez, A., “Manufacture of Concrete Kerbs and Floor Blocks with Recycled Aggregate from C&DW,” Construction and Building Materials, V. 40, Mar. 2013, pp. 1193-1199. doi: 10.1016/j.conbuildmat.2011.11.040

11. Limbachiya, M. C.; Leelawat, T.; and Dhir, R. K., “Use of Recycled Concrete Aggregate in High-Strength Concrete,” Materials and Structures, V. 33, No. 9, Nov. 2000, pp. 574-580. doi: 10.1007/BF02480538

12. Revilla-Cuesta, V.; Skaf, M.; Faleschini, F.; Manso, J. M.; and Ortega-López, V., “Self-Compacting Concrete Manufactured with Recycled Concrete Aggregate: An Overview,” Journal of Cleaner Production, V. 262, July 2020, Article No. 121362. doi: 10.1016/j.jclepro.2020.121362

13. Manzi, S., and Bignozzi, M. C., “Self-Compacting Concrete with Recycled Aggregates,” Advances in Construction and Demolition Waste Recycling: Management, Processing and Environmental Assessment, F. Pacheco-Torgal, Y. Ding, F. Colangelo, R. Tuladhar, and A. Koutamanis, eds., Woodhead Publishing, Sawston, UK, 2020, pp. 229-252.

14. NBN EN 13369:2018, “Common Rules for Precast Concrete Products,” Bureau of Normalization, Brussels, Belgium, 2018.

15. COPRO vzw, “Activiteitenrapport 2020 (Activity Report),” COPRO vzw, Asse, Belgium, 2021, http://www.copro.eu/nl/activiteitenrapport. (in Dutch) (last accessed Dec. 28, 2022)

16. Eurostat, “Generation of Waste by Waste Category, Hazardousness and NACE Rev. 2 Activity,” Eurostat, European Commission, Luxembourg City, Luxembourg, 2022, https://ec.europa.eu/eurostat/web/products-datasets/-/env_wasgen. (last accessed Dec. 28, 2022)

17. COPRO vzw, “PTV 406 (9.0) - Technische Voorschriften voor Gerecycleerde Granulaten (Technical Requirements for Recycled Aggregates),” COPRO vzw, Asse, Belgium, 2020, http://www.copro.eu/en/document/ptv-406-90-prescriptions-techniques-pour-granulats-recycles. (in Dutch) (last accessed Dec. 28, 2022)

18. NBN EN 933-11:2009, “Tests for Geometrical Properties of Aggregates - Part 11: Classification Test for the Constituents of Coarse Recycled Aggregate,” Bureau of Normalization, Brussels, Belgium, 2009.

19. NBN EN 206:2013+A2:2021, “Concrete - Specification, Performance, Production and Conformity,” Bureau of Normalization, Brussels, Belgium, 2021.

20. Flemish Government, “VLAREMA (Decree of the Flemish Government establishing the Flemish regulations regarding the sustainable management of material cycles and waste materials),” Government of Flanders, Brussels, Belgium, 2012, https://navigator.emis.vito.be/mijn-navigator?woId=43991. (in Dutch) (last accessed Dec. 28, 2022)

21. Flemish Government, “M.B. Eenheidsreglement Gerecycleerde Granulaten (Unitary Regulations for Recycled Aggregates),” Government of Flanders, Brussels, Belgium, 2018, https://navigator.emis.vito.be/mijn-navigator?woId=40409. (in Dutch) (last accessed Dec. 28, 2022)

22. Tracimat vzw, “Waarom Tracimat - LMRP/HMRP (Why Tracimat - LMRP/HMRP),” Tracimat vzw, Brussels, Belgium, 2018, http://www.tracimat.be/over-ons/traceerbaarheid-sloopafval/. (in Dutch) (last accessed Dec. 28, 2022)

23. NBN EN 933-1:2012, “Tests for Geometrical Properties of Aggregates - Part 1: Determination of Particle Size Distribution - Sieving Method,” Bureau of Normalization, Brussels, Belgium, 2012.

24. NBN EN 933-11:2009, “Tests for Geometrical Properties of Aggregates - Part 11: Classification Test for the Constituents of Coarse Recycled Aggregate,” Bureau of Normalization, Brussels, Belgium, 2009.

25. NBN EN 1097-1:2011, “Tests for Mechanical and Physical Properties of Aggregates - Part 1: Determination of the Resistance to Wear (Micro-Deval),” Bureau of Normalization, Brussels, Belgium, 2011.

26. NBN EN 1097-2:2020, “Tests for Mechanical and Physical Properties of Aggregates - Part 2: Methods for the Determination of Resistance to Fragmentation,” Bureau of Normalization, Brussels, Belgium, 2020.

27. NBN EN 1097-6:2013, “Tests for Mechanical and Physical Properties of Aggregates - Part 6: Determination of Particle Density and Water Absorption,” Bureau of Normalization, Brussels, Belgium, 2013.

28. NBN EN 1097-5:2008, “Tests for Mechanical and Physical Properties of Aggregates - Part 5: Determination of the Water Content by Drying in a Ventilated Oven,” Bureau of Normalization, Brussels, Belgium, 2008.

29. Leite, M. B., “Evaluation of Mechanical Properties of Concrete Produced with Recycled Aggregates from Construction and Demolition Waste,” PhD dissertation, Federal University of Rio Grande do Sul, Porto Alegre, Rio Grande do Sul, Brazil, 2001. (in Portuguese)

30. Evangelista, L., and de Brito, J., “Mechanical Behaviour of Concrete Made with Fine Recycled Concrete Aggregates,” Cement and Concrete Composites, V. 29, No. 5, May 2007, pp. 397-401. doi: 10.1016/j.cemconcomp.2006.12.004

31. Etxeberria, M.; Vázquez, E.; Marí, A.; and Barra, M., “Influence of Amount of Recycled Coarse Aggregates and Production Process on Properties of Recycled Aggregate Concrete,” Cement and Concrete Research, V. 37, No. 5, May 2007, pp. 735-742. doi: 10.1016/j.cemconres.2007.02.002

32. Gomes, M., and de Brito, J., “Structural Concrete with Incorporation of Coarse Recycled Concrete and Ceramic Aggregates: Durability Performance,” Materials and Structures, V. 42, No. 5, June 2009, pp. 663-675. doi: 10.1617/s11527-008-9411-9

33. Mas, B.; Cladera, A.; Bestard, J.; Muntaner, D.; López, C. L.; Piña, S.; and Prades, J., “Concrete with Mixed Recycled Aggregates: Influence of the Type of Cement,” Construction and Building Materials, V. 34, Sept. 2012, pp. 430-441. doi: 10.1016/j.conbuildmat.2012.02.092

34. González-Taboada, I.; González-Fonteboa, B.; Martínez-Abella, F.; and Seara-Paz, S., “Analysis of Rheological Behaviour of Self-Compacting Concrete Made with Recycled Aggregates,” Construction and Building Materials, V. 157, Dec. 2017, pp. 18-25. doi: 10.1016/j.conbuildmat.2017.09.076

35. Poon, C. S.; Shui, Z. H.; Lam, L.; Fok, H.; and Kou, S. C., “Influence of Moisture States of Natural and Recycled Aggregates on the Slump and Compressive Strength of Concrete,” Cement and Concrete Research, V. 34, No. 1, Jan. 2004, pp. 31-36. doi: 10.1016/S0008-8846(03)00186-8

36. González-Taboada, I.; González-Fonteboa, B.; Martínez-Abella, F.; and Pérez-Ordóñez, J. L., “Prediction of the Mechanical Properties of Structural Recycled Concrete Using Multivariable Regression and Genetic Programming,” Construction and Building Materials, V. 106, Mar. 2016, pp. 480-499. doi: 10.1016/j.conbuildmat.2015.12.136

37. Tam, V. W. Y.; Gao, X. F.; and Tam, C. M., “Microstructural Analysis of Recycled Aggregate Concrete Produced from Two-Stage Mixing Approach,” Cement and Concrete Research, V. 35, No. 6, June 2005, pp. 1195-1203. doi: 10.1016/j.cemconres.2004.10.025

38. NBN EN 12350-8:2019, “Testing Fresh Concrete - Part 8: Self-Compacting Concrete - Slump-Flow Test,” Bureau of Normalization, Brussels, Belgium, 2019.

39. NBN EN 12390-7:2019, “Testing Hardened Concrete - Part 7: Density of Hardened Concrete,” Bureau of Normalization, Brussels, Belgium, 2019.

40. NBN EN 12504-4:2004, “Testing Concrete - Part 4: Determination of Ultrasonic Pulse Velocity,” Bureau of Normalization, Brussels, Belgium, 2004.

41. Chen, X.; Capiau, L.; Reynaert, I.; Zheng, K.; Gruyaert, E.; and Li, J., “Comparative Study on Modelling Concrete Properties Using Physical and Mechanical Properties of Recycled Coarse Aggregate,” Construction and Building Materials, V. 345, Aug. 2022, Article No. 128249. doi: 10.1016/j.conbuildmat.2022.128249

42. NBN B 15-215:2018, “Testing Hardened Concrete - Absorption of Water by Immersion,” Bureau of Normalization, Brussels, Belgium, 2018.

43. NBN EN 12390-3:2019, “Testing Hardened Concrete - Part 3: Compressive Strength of Test Specimens,” Bureau of Normalization, Brussels, Belgium, 2019.

44. NBN EN 12390-6:2010, “Testing Hardened Concrete - Part 6: Tensile Splitting Strength of Test Specimens,” Bureau of Normalization, Brussels, Belgium, 2010.

45. NBN EN 12390-13:2014, “Testing Hardened Concrete - Part 13: Determination of Secant Modulus of Elasticity in Compression,” Bureau of Normalization, Brussels, Belgium, 2014.

46. NBN EN 12390-10:2019, “Testing Hardened Concrete - Part 10: Determination of the Carbonation Resistance of Concrete at Atmospheric Levels of Carbon Dioxide,” Bureau of Normalization, Brussels, Belgium, 2019.

47. AASHTO T 358-19, “Standard Method of Test for Surface Resistivity Indication of Concrete’s Ability to Resist Chloride Ion Penetration,” American Association of State Highway and Transportation Officials, Washington, DC, 2019.

48. PTV 21-601:2001, “Technische voorschriften (Technical regulations),” PROBETON vzw, Brussels, Belgium, 2001. (in Dutch)

49. Kurda, R.; de Brito, J.; and Silvestre, J. D., “Influence of Recycled Aggregates and High Contents of Fly Ash on Concrete Fresh Properties,” Cement and Concrete Composites, V. 84, Nov. 2017, pp. 198-213. doi: 10.1016/j.cemconcomp.2017.09.009

50. Thomas, C.; Setién, J.; and Polanco, J. A., “Structural Recycled Aggregate Concrete Made with Precast Wastes,” Construction and Building Materials, V. 114, July 2016, pp. 536-546. doi: 10.1016/j.conbuildmat.2016.03.203

51. Limbachiya, M.; Meddah, M. S.; and Ouchagour, Y., “Use of Recycled Concrete Aggregate Fly-Ash Concrete,” Construction and Building Materials, V. 27, No. 1, Feb. 2012, pp. 439-449. doi: 10.1016/j.conbuildmat.2011.07.023

52. Amario, M.; Rangel, C. S.; Pepe, M.; and Toledo Filho, R. D., “Optimization of Normal and High Strength Recycled Aggregate Concrete Mixtures by Using Packing Model,” Cement and Concrete Composites, V. 84, Nov. 2017, pp. 83-92. doi: 10.1016/j.cemconcomp.2017.08.016

53. Chen, X.; Vanoutrive, H.; Gruyaert, E.; and Li, J., “Properties of High-Performance Concrete with Coarse Recycled Concrete Aggregate for Precast Industry,” Proceedings of the 75th RILEM Annual Week and International Conference on Advances in Sustainable Construction Materials and Structures, Mérida, Yucatán, Mexico, Aug. 29-Sept. 3, 2021.

54. Hansen, T. C., “Recycled Aggregates and Recycled Aggregate Concrete Second State-of-the-Art Report Developments 1945–1985,” Materials and Structures, V. 19, No. 3, May 1986, pp. 201-246. doi: 10.1007/BF02472036

55. Safiuddin, M. D., Salam, M. A., Jumaat, M. Z., “Effects of Recycled Concrete Aggregate on the Fresh Properties of Self-Consolidating Concrete,” Archives of Civil and Mechanical Engineering, V. 11, No. 4, 2011, pp. 1023-1041. (in Polish) doi: 10.1016/S1644-9665(12)60093-4

56. Tuyan, M.; Mardani-Aghabaglou, A.; and Ramyar, K., “Freeze–Thaw Resistance, Mechanical and Transport Properties of Self-Consolidating Concrete Incorporating Coarse Recycled Concrete Aggregate,” Materials & Design, V. 53, Jan. 2014, pp. 983-991. doi: 10.1016/j.matdes.2013.07.100

57. Whitehurst, E. A., “Evaluation of Concrete Properties from Sonic Tests,” ACI Monograph, No. 2, American Concrete Institute, Farmington Hills, MI, 1966, 94 pp.

58. NBN EN 1992-1-1:2005, “Eurocode 2: Design of Concrete Structures - Part 1-1: General Rules and Rules for Buildings (+AC:2010),” Bureau of Normalization, Brussels, Belgium, 2005.

59. Chen, X.; Gruyaert, E.; and Li, J., “Modelling the Effect of Coarse Recycled Concrete Aggregate on Compressive Strength of Portland Cement Concrete Using Volume Fraction-Based Approach,” Construction and Building Materials, V. 309, Nov. 2021, Article No. 125159. doi: 10.1016/j.conbuildmat.2021.125159

60. Gonzalez, A., and Etxeberria, M., “Experimental Analysis of Properties of High Performance Recycled Aggregate Concrete,” Construction and Building Materials, V. 52, Feb. 2014, pp. 227-235. doi: 10.1016/j.conbuildmat.2013.11.054

61. DN-27-13, “Designer’s Notebooks: Design Factors Affecting Aesthetics of Architectural Precast Concrete,” Precast/Prestressed Concrete Institute, Chicago, IL, 2013.

62. CIB Working Commission W 29, “Tolerances on Blemishes of Concrete,” CIB Report No. 24, International Council for Building Research, Studies and Documentation, Rotterdam, the Netherlands, 1973, 17 pp.

63. ISO 14040:2006, “Environmental Management – Life Cycle Assessment – Principles and Framework,” International Organization for Standardization, Geneva, Switzerland, 2006, 20 pp.

64. Damineli, B. L.; Kemeid, F. M.; Aguiar, P. S.; and John, V. M., “Measuring the Eco-Efficiency of Cement Use,” Cement and Concrete Composites, V. 32, No. 8, Sept. 2010, pp. 555-562. doi: 10.1016/j.cemconcomp.2010.07.009

65. Kurad, R.; Silvestre, J. D.; de Brito, J.; and Ahmed, H., “Effect of Incorporation of High Volume of Recycled Concrete Aggregates and Fly Ash on the Strength and Global Warming Potential of Concrete,” Journal of Cleaner Production, V. 166, Nov. 2017, pp. 485-502. doi: 10.1016/j.jclepro.2017.07.236

66. Chen, C.; Habert, G.; Bouzidi, Y.; Jullien, A.; and Ventura, A., “LCA Allocation Procedure Used as an Incitative Method for Waste Recycling: An Application to Mineral Additions in Concrete,” Resources, Conservation and Recycling, V. 54, No. 12, Oct. 2010, pp. 1231-1240. doi: 10.1016/j.resconrec.2010.04.001

67. Miller, S. A.; John, V. M.; Pacca, S. A.; and Horvath, A., “Carbon Dioxide Reduction Potential in the Global Cement Industry by 2050,” Cement and Concrete Research, V. 114, Dec. 2018, pp. 115-124. doi: 10.1016/j.cemconres.2017.08.026

68. Braga, A. M.; Silvestre, J. D.; and de Brito, J., “Compared Environmental and Economic Impact from Cradle to Gate of Concrete with Natural and Recycled Coarse Aggregates,” Journal of Cleaner Production, V. 162, Sept. 2017, pp. 529-543. doi: 10.1016/j.jclepro.2017.06.057

69. Martínez-Lage, I.; Vázquez-Burgo, P.; and Velay-Lizancos, M., “Sustainability Evaluation of Concretes with Mixed Recycled Aggregate Based on Holistic Approach: Technical, Economic and Environmental Analysis,” Waste Management, V. 104, Mar. 2020, pp. 9-19. doi: 10.1016/j.wasman.2019.12.044

70. Tošić, N.; Marinković, S.; Dašić, T.; and Stanić, M., “Multicriteria Optimization of Natural and Recycled Aggregate Concrete for Structural Use,” Journal of Cleaner Production, V. 87, Jan. 2015, pp. 766-776. doi: 10.1016/j.jclepro.2014.10.070

71. Noterman, B.; Geerts, F.; Verstraeten, G.; Geerts, G.; Vrijders, J.; Wouters, J.; van der Have, J.-A.; Van Cauwenberghe, L.; Boehme, L.; Joseph, M.; Schaerlaekens, S.; and Moerman, W., “Recybet Roadmap: Ontwikkeling van een Nieuwe Waardeketen voor de Valorisatie van Betonpuin in Betonproducten (Recybet Roadmap: Developing a New Value Chain for the Valorisation of Concrete Rubble in Concrete Products),” Agentschap Innoveren & Ondernemen (VLAIO), Belgium, 2016, 85 pp. (in Dutch)

72. Coelho, A., and de Brito, J., “Environmental Analysis of a Construction and Demolition Waste Recycling Plant in Portugal – Part I: Energy Consumption and CO2 Emissions,” Waste Management, V. 33, No. 5, May 2013, pp. 1258-1267. doi: 10.1016/j.wasman.2013.01.025

73. Plaza, P.; Sáez del Bosque, I. F.; Frías, M.; Sánchez de Rojas, M. I.; and Medina, C., “Use of Recycled Coarse and Fine Aggregates in Structural Eco-Concretes. Physical and Mechanical Properties and CO2 Emissions,” Construction and Building Materials, V. 285, May 2021, Article No. 122926. doi: 10.1016/j.conbuildmat.2021.122926

74. Wijayasundara, M.; Mendis, P.; and Crawford, R. H., “Integrated Assessment of the Use of Recycled Concrete Aggregate Replacing Natural Aggregate in Structural Concrete,” Journal of Cleaner Production, V. 174, Feb. 2018, pp. 591-604. doi: 10.1016/j.jclepro.2017.10.301

75. Lizarralde, G.; Chmutina, K.; Bosher, L.; and Dainty, A., “Sustainability and Resilience in the Built Environment: The Challenges of Establishing a Turquoise Agenda in the UK,” Sustainable Cities and Society, V. 15, July 2015, pp. 96-104. doi: 10.1016/j.scs.2014.12.004

76. Bocchini, P.; Frangopol, D. M.; Ummenhofer, T.; and Zinke, T., “Resilience and Sustainability of Civil Infrastructure: Toward a Unified Approach,” Journal of Infrastructure Systems, ASCE, V. 20, No. 2, June 2014, p. 04014004. doi: 10.1061/(ASCE)IS.1943-555X.0000177

77. O’Grady, T.; Minunno, R.; Chong, H.-Y.; and Morrison, G. M., “Design for Disassembly, Deconstruction and Resilience: A Circular Economy Index for the Built Environment,” Resources, Conservation and Recycling, V. 175, Dec. 2021, Article No. 105847. doi: 10.1016/j.resconrec.2021.105847

78. Vyncke, J., and Vrijders, J., “Recycling of C&D Waste in Belgium: State-of-the-Art and Opportunities for Technology Transfer,” Proceedings of the 2nd International Conference on Sustainable Construction Materials and Technologies, Ancona, Italy, June 28-30, 2010, 11 pp.


ALSO AVAILABLE IN:

Electronic Materials Journal