Volume-Based Concrete Mix Design

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Volume-Based Concrete Mix Design

Author(s): Anderson S. H. Chu

Publication: Materials Journal

Volume: 120

Issue: 1

Appears on pages(s): 243-256

Keywords: slurry film thickness; strength; volume-based design; wet packing density

DOI: 10.14359/51737295

Date: 1/1/2023

Abstract:
Concrete mixture design is the foundation of cement and concrete research. Innovations in concrete materials could, should, and would inevitably be incorporated into new mixture designs. Thus, a rigorous method for concrete mixture design can better bridge the research community and the construction industry with high reliability and high fidelity. However, current methods for concrete mixture design vary a lot in the literature, thus compromising the accuracy and consistency in interpreting the properties of concrete subject to changes in its raw ingredients. Moreover, the extraneous variables in controlled experiments are not always controlled well. To solve this old but critical problem, this paper summarizes the prevalent concrete mixture design methods in the literature and in practice. By contrast, the volume-based mixture design method is superior to the mass ratio-based mixture design method in terms of simplicity, accuracy, and consistency. Further discussion on packing density measurement and water or slurry film thickness (SFT) as a basis of volume-based mixture design is elaborated. Mathematically, the hardened properties were linked to the particle packing behavior and fresh properties of concrete. This research contributes to a unified volume-based design method to bridge the research community and the construction industry. In the end, it is conducive to upgrading from concrete technology to science.

Related References:

1. Neville, A. M., Properties of Concrete, Longman, London, UK, 1995.

2. Wadud, Z., and Ahmad, S., “ACI Method of Concrete Mix Design: A Parametric Study,” The Eighth East Asia-Pacific Conference on Structural Engineering and Construction, Nanyang Technological University, Singapore, 2001.

3. Christ, R.; Tutikian, B. F.; and do Lago Helene, P. R., “Proposition of Mixture Design Method for Ultra-High-Performance Concrete,” ACI Materials Journal, V. 119, No. 1, Jan. 2022, pp. 79-89.

4. Elemam, W. E.; Abdelraheem, A. H.; Mahdy, M. G.; and Tahwia, A. M., “Prediction and Optimization of Self-Consolidating Concrete Properties,” ACI Materials Journal, V. 119, No. 1, Jan. 2020, pp. 91-104.

5. Leite, M. B., and Santana, V. M., “Evaluation of an Experimental Mix Proportion Study and Production of Concrete Using Fine Recycled Aggregate,” Journal of Building Engineering, V. 21, 2019, pp. 243-253. doi: 10.1016/j.jobe.2018.10.016

6. Yurdakul, E.; Taylor, P. C.; Ceylan, H.; and Bektas, F., “Effect of Paste-to-Voids Volume Ratio on the Performance of Concrete Mixtures,” Journal of Materials in Civil Engineering, ASCE, V. 25, No. 12, 2013, pp. 1840-1851. doi: 10.1061/(ASCE)MT.1943-5533.0000728

7. Kim, J., “Properties of Recycled Aggregate Concrete Designed with Equivalent Mortar Volume Mix Design,” Construction and Building Materials, V. 301, 2021, p. 124091. doi: 10.1016/j.conbuildmat.2021.124091

8. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-08) and Commentary (ACI 318R-08),” American Concrete Institute, Farmington Hills, MI, 2008, 473 pp.

9. Chen, J. J., and Kwan, A. K. H., “Triple Blending with Fly Ash Microsphere and Condensed Silica Fume to Improve Performance of Cement Paste,” Journal of Materials in Civil Engineering, ASCE, V. 25, No. 5, 2013, pp. 618-626. doi: 10.1061/(ASCE)MT.1943-5533.0000620

10. Chu, S. H.; Chen, J. J.; Li, L. G.; Ng, P. L.; and Kwan, A. K. H., “Roles of Packing Density and Slurry Film Thickness in Synergistic Effects of Metakaolin and Silica Fume,” Powder Technology, V. 387, 2021, pp. 575-583. doi: 10.1016/j.powtec.2021.04.029

11. Poon, C. S.; Lam, L.; and Wong, Y. L., “Effects of Fly Ash and Silica Fume on Interfacial Porosity of Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 11, No. 3, 1999, pp. 197-205. doi: 10.1061/(ASCE)0899-1561(1999)11:3(197)

12. Bourchy, A.; Barnes, L.; Bessette, L.; Chalencon, F.; Joron, A.; and Torrenti, J. M., “Optimization of Concrete Mix Design to Account for Strength and Hydration Heat in Massive Concrete Structures,” Cement and Concrete Composites, V. 103, 2019, pp. 233-241. doi: 10.1016/j.cemconcomp.2019.05.005

13. Ghorbani, S.; Taji, I.; de Brito, J.; Negahban, M.; Ghorbani, S.; Tavakkolizadeh, M.; and Davoodi, A., “Mechanical and Durability Behaviour of Concrete with Granite Waste Dust as Partial Cement Replacement under Adverse Exposure Conditions,” Construction and Building Materials, V. 194, 2019, pp. 143-152. doi: 10.1016/j.conbuildmat.2018.11.023

14. Lu, B.; Shi, C.; Zhang, J.; and Wang, J., “Effects of Carbonated Hardened Cement Paste Powder on Hydration and Microstructure of Portland Cement,” Construction and Building Materials, V. 186, 2018, pp. 699-708. doi: 10.1016/j.conbuildmat.2018.07.159

15. Wellmann, C., and Wriggers, P., “A Two-Scale Model of Granular Materials,” Computer Methods in Applied Mechanics and Engineering, V. 205-208, 2012, pp. 46-58. doi: 10.1016/j.cma.2010.12.023

16. Chu, S. H.; Jiang, Y.; and Kwan, A. K. H., “Effect of Rigid Fibres on Aggregate Packing,” Construction and Building Materials, V. 224, 2019, pp. 326-335. doi: 10.1016/j.conbuildmat.2019.07.072

17. Liu, Y.; Jing, R.; Cao, F.; and Yan, P., “Effects of Aggregate Content on Rheological Properties of Lubrication Layer and Pumping Concrete,” ACI Materials Journal, V. 118, No. 6, Nov. 2021, pp. 7-18.

18. Chu, S. H., “Effect of Paste Volume on Fresh and Hardened Properties of Concrete,” Construction and Building Materials, V. 218, 2019, pp. 284-294. doi: 10.1016/j.conbuildmat.2019.05.131

19. Lai, M.; Binhowimal, S.; Hanzic, L.; Wang, Q.; and Ho, J. C. M., “Dilatancy Mitigation of Cement Powder Paste by Pozzolanic and Inert Fillers,” Structural Concrete, V. 21, No. 3, 2020, pp. 1164-1180. doi: 10.1002/suco.201900320

20. Hansen, B. S.; Howard, I. L.; Shannon, J.; Cost, T.; and Wilson, W. M., “Portland-Limestone Cement Fineness Effects on Concrete Properties,” ACI Materials Journal, V. 117, No. 2, Mar. 2020, pp. 157-168.

21. Li, L. G., and Kwan, A. K. H., “Concrete Mix Design Based on Water Film Thickness and Paste Film Thickness,” Cement and Concrete Composites, V. 39, 2013, pp. 33-42. doi: 10.1016/j.cemconcomp.2013.03.021

22. Chu, S. H., and Yao, J. J., “A Strength Model for Concrete Made with Marine Dredged Sediment,” Journal of Cleaner Production, V. 274, 2020, p. 122673. doi: 10.1016/j.jclepro.2020.122673

23. Nataraja, M., and Das, L., “Concrete Mix Proportioning as per IS 10262: 2009–Comparison with IS 10262: 1982 and ACI 211.1-91,” Indian Concrete Journal, V. 84, 2010, pp. 64-70.

24. Malecot, Y.; Zingg, L.; Briffaut, M.; and Baroth, J., “Influence of Free Water on Concrete Triaxial Behavior: The Effect of Porosity,” Cement and Concrete Research, V. 120, 2019, pp. 207-216. doi: 10.1016/j.cemconres.2019.03.010

25. Shah, H. A.; Yuan, Q.; and Zuo, S., “Air Entrainment in Fresh Concrete and its Effects on Hardened Concrete-A Review,” Construction and Building Materials, V. 274, 2020, p. 121835. doi: 10.1016/j.conbuildmat.2020.121835

26. Radlinski, M., and Olek, J., “Investigation into the Synergistic Effects in Ternary Cementitious Systems Containing Portland Cement, Fly Ash and Silica Fume,” Cement and Concrete Composites, V. 34, No. 4, 2012, pp. 451-459. doi: 10.1016/j.cemconcomp.2011.11.014

27. Chu, S. H., and Kwan, A. K. H., “Mixture Design of Self-Levelling Ultra-High Performance FRC,” Construction and Building Materials, V. 228, 2019, p. 116761. doi: 10.1016/j.conbuildmat.2019.116761

28. Chu, S. H.; Li, L. G.; and Kwan, A. K. H., “Fibre Factors Governing the Fresh and Hardened Properties of Steel FRC,” Construction and Building Materials, V. 186, 2018, pp. 1228-1238. doi: 10.1016/j.conbuildmat.2018.08.047

29. Tang, Z.; Hu, Y.; Tam, V. W.; and Li, W., “Uniaxial Compressive Behaviors of Fly Ash/Slag-Based Geopolymeric Concrete with Recycled Aggregates,” Cement and Concrete Composites, V. 104, 2019, p. 103375. doi: 10.1016/j.cemconcomp.2019.103375

30. Wu, Z.; Khayat, K. H.; and Shi, C., “Changes in Rheology and Mechanical Properties of Ultra-High Performance Concrete with Silica Fume Content,” Cement and Concrete Research, V. 123, 2019, p. 105786. doi: 10.1016/j.cemconres.2019.105786

31. Hu, C., and Li, Z., “Property Investigation of Individual Phases in Cementitious Composites Containing Silica Fume and Fly Ash,” Cement and Concrete Composites, V. 57, 2015, pp. 17-26. doi: 10.1016/j.cemconcomp.2014.11.011

32. Lam, L.; Wong, Y.; and Poon, C. S., “Effect of Fly Ash and Silica Fume on Compressive and Fracture Behaviors of Concrete,” Cement and Concrete Research, V. 28, No. 2, 1998, pp. 271-283. doi: 10.1016/S0008-8846(97)00269-X

33. Chen, T.; Gao, X.; and Ren, M., “Effects of Autoclave Curing and Fly Ash on Mechanical Properties of Ultra-High Performance Concrete,” Construction and Building Materials, V. 158, 2018, pp. 864-872. doi: 10.1016/j.conbuildmat.2017.10.074

34. Wong, H. H. C., and Kwan, A. K. H., “Packing Density of Cementitious Materials: Part 1 - Measurement Using a Wet Packing Method,” Materials and Structures, V. 41, No. 4, 2008, pp. 689-701. doi: 10.1617/s11527-007-9274-5

35. Kwan, A. K. H., and Li, L. G., “Combined Effects of Water Film, Paste Film and Mortar Film Thicknesses on Fresh Properties of Concrete,” Construction and Building Materials, V. 50, 2014, pp. 598-608. doi: 10.1016/j.conbuildmat.2013.10.014

36. Chu, S. H., “Development of Infilled Cementitious Composites (ICC),” Composite Structures, V. 267, 2021, p. 113885. doi: 10.1016/j.compstruct.2021.113885


ALSO AVAILABLE IN: