Role of High-Volume Mineral Admixtures on Characteristics of Engineered Cementitious Composites

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Role of High-Volume Mineral Admixtures on Characteristics of Engineered Cementitious Composites

Author(s): Adeyemi Adesina and Sreekanta Das

Publication: Materials Journal

Volume: 120

Issue: 1

Appears on pages(s): 193-204

Keywords: drying shrinkage; engineered cementitious composites (ECCs); fly ash (FA); ground calcium carbonate (GCC); permeability; slag.

DOI: 10.14359/51737292

Date: 1/1/2023

Abstract:
In this study, mineral admixtures were used to substitute a high volume of portland cement (PC) in engineered cementitious composites (ECCs), and the corresponding permeability properties and drying shrinkage were evaluated. Six ECC mixtures were made with high-volume mineral admixtures (MAs) (that is, MA/PC ratio of 5) alongside a control ECC mixture (that is, MA/PC of 2.2). The findings from this study revealed that the application of a higher content of MAs ensued in a rise in the permeability of the ECCs at early ages. However, the permeability properties of the ECCs were significantly reduced in the long term, resulting in similar or lower permeability compared to that of the ECCs made with a lower amount of MA (that is, 2.2). The 28-day water absorption of ECC made with blast-furnace slag (BFS) as the MA at an MA/PC of 5 is 5.4%, while that of the control ECC with an MA/PC of 2.2 is 5.1%. The outcome of this research also revealed that the application of ground calcium carbonate (GCC) is beneficial in reducing the drying shrinkage of the ECCs. The drying shrinkage at 32 days of ECC made with GCC at an MA/PC of 5 is 14.3% and 60% lower than when fly ash (FA) and BFS were used at the same MA/PC (that is, 5). However, GCC should be used in ECCs as a filler rather than an MA as there was a significant increase in the permeability of ECCs made with only GCC as the MA. Nonetheless, FA or BFS can be used alongside GCC to reduce the detrimental impact of GCC on the permeability characteristics of the ECCs.

Related References:

1. Li, V. C.; Wu, C.; Wang, S.; Ogawa, A.; and Saito, T., “Interface Tailoring for Strain-Hardening Polyvinyl Alcohol-Engineered Cementitious Composite (PVA-ECC),” ACI Materials Journal, V. 99, No. 5, Sept.-Oct. 2002, pp. 463-472. doi: 10.14359/12325

2. Li, V. C.; Wang, S.; and Wu, C., “Tensile Strain-Hardening Behavior of Polyvinyl Alcohol Engineered Cementitious Composite (PVA-ECC),” ACI Materials Journal, V. 98, No. 6, Nov.-Dec. 2001, pp. 483-492. doi: 10.14359/10851

3. Şahmaran, M., and Li, V. C., “Durability of Mechanically Loaded Engineered Cementitious Composites under Highly Alkaline Environments,” Cement and Concrete Composites, V. 30, No. 2, 2008, pp. 72-81. doi: 10.1016/j.cemconcomp.2007.09.004

4. Zhang, Z.; Qian, S.; and Ma, H., “Investigating Mechanical Properties and Self-Healing Behavior of Micro-Cracked ECC with Different Volume of Fly Ash,” Construction and Building Materials, V. 52, 2014, pp. 17-23. doi: 10.1016/j.conbuildmat.2013.11.001

5. Liu, H.; Zhang, Q.; Gu, C.; Su, H.; and Li, V., “Influence of Microcrack Self-Healing Behavior on the Permeability of Engineered Cementitious Composites,” Cement and Concrete Composites, V. 82, 2017, pp. 14-22. doi: 10.1016/j.cemconcomp.2017.04.004

6. Meyer, C., “The Greening of the Concrete Industry,” Cement and Concrete Composites, V. 31, No. 8, 2009, pp. 601-605. doi: 10.1016/j.cemconcomp.2008.12.010

7. Adesina, A., “Recent Advances in the Concrete Industry to Reduce Its Carbon Dioxide Emissions,” Environmental Challenges, V. 1, 2020, Article No. 100004. doi: 10.1016/j.envc.2020.100004

8. Purnell, P., “The Carbon Footprint of Reinforced Concrete,” Advances in Cement Research, V. 25, No. 6, 2013, pp. 362-368. doi: 10.1680/adcr.13.00013

9. Özbay, E.; Karahan, O.; Lachemi, M.; Hossain, K. M. A.; and Duran Atiş, C., “Investigation of Properties of Engineered Cementitious Composites Incorporating High Volumes of Fly Ash and Metakaolin,” ACI Materials Journal, V. 109, No. 5, Sept.-Oct. 2012, pp. 565-571. doi: 10.14359/51684088

10. Adesina, A., and Das, S., “Evaluation of the Durability Properties of Engineered Cementitious Composites Incorporating Recycled Concrete as Aggregate,” Journal of Materials in Civil Engineering, ASCE, V. 33, No. 2, 2021, p. 04020439. doi: 10.1061/(ASCE)MT.1943-5533.0003563

11. Huang, X.; Ranade, R.; Ni, W.; and Li, V. C., “Development of Green Engineered Cementitious Composites Using Iron Ore Tailings as Aggregates,” Construction and Building Materials, V. 44, 2013, pp. 757-764. doi: 10.1016/j.conbuildmat.2013.03.088

12. Şahmaran, M.; Lachemi, M.; Hossain, K. M. A.; and Li, V. C., “Internal Curing of Engineered Cementitious Composites for Prevention of Early Age Autogenous Shrinkage Cracking,” Cement and Concrete Research, V. 39, No. 10, 2009, pp. 893-901. doi: 10.1016/j.cemconres.2009.07.006

13. Yang, E.-H.; Yang, Y.; and Li, V. C., “Use of High Volumes of Fly Ash to Improve ECC Mechanical Properties and Material Greenness,” ACI Materials Journal, V. 104, No. 6, Nov.-Dec. 2007, pp. 620-628. doi: 10.14359/18966

14. Booya, E.; Gorospe, K.; Das, S.; and Loh, P., “The Influence of Utilizing Slag in Lieu of Fly Ash on the Performance of Engineered Cementitious Composites,” Construction and Building Materials, V. 256, 2020, Article No. 119412. doi: 10.1016/j.conbuildmat.2020.119412

15. Adesina, A., and Das, S., “Influence of Glass Powder on the Durability Properties of Engineered Cementitious Composites,” Construction and Building Materials, V. 242, 2020, Article No. 118199. doi: 10.1016/j.conbuildmat.2020.118199

16. Adesina, A., and Das, S., “Performance of Engineered Cementitious Composites Incorporating Crumb Rubber as Aggregate,” Construction and Building Materials, V. 274, 2021, Article No. 122033. doi: 10.1016/j.conbuildmat.2020.122033

17. Hisseine, O. A., and Tagnit-Hamou, A., “Development of Ecological Strain-Hardening Cementitious Composites Incorporating High-Volume Ground-Glass Pozzolans,” Construction and Building Materials, V. 238, 2020, Article No. 117740. doi: 10.1016/j.conbuildmat.2019.117740

18. Zhu, Y.; Yang, Y.; and Yao, Y., “Use of Slag to Improve Mechanical Properties of Engineered Cementitious Composites (ECCs) with High Volumes of Fly Ash,” Construction and Building Materials, V. 36, 2012, pp. 1076-1081. doi: 10.1016/j.conbuildmat.2012.04.031

19. Zhang, Z.; Yang, F.; Liu, J.-C.; and Wang, S., “Eco-Friendly High Strength, High Ductility Engineered Cementitious Composites (ECC) with Substitution of Fly Ash by Rice Husk Ash,” Cement and Concrete Research, V. 137, 2020, Article No. 106200. doi: 10.1016/j.cemconres.2020.106200

20. Al-Najjar, Y.; Yeşilmen, S.; Majeed Al-Dahawi, A.; Şahmaran, M.; Yıldırım, G.; Lachemi, M.; and Amleh, L., “Physical and Chemical Actions of Nano-Mineral Additives on Properties of High-Volume Fly Ash Engineered Cementitious Composites,” ACI Materials Journal, V. 113, No. 6, Nov.-Dec. 2016, pp. 791-801. doi: 10.14359/51689114

21. ASTM C642-13, “Standard Test Method for Density, Absorption, and Voids in Hardened Concrete,” ASTM International, West Conshohocken, PA, 2013, 3 pp. doi: 10.1520/C0642-13

22. ASTM C1757-13, “Standard Test Method for Determination of One-Point, Bulk Water Sorption of Dried Concrete (Withdrawn 2022),” ASTM International, West Conshohocken, PA, 2013. doi: 10.1520/C1757-13

23. ASTM C1585-13, “Standard Test Method for Measurement of Rate of Absorption of Water by Hydraulic-Cement Concretes,” ASTM International, West Conshohocken, PA, 2013, 6 pp. doi: 10.1520/C1585-13

24. ASTM C1202-10, “Standard Test Method for Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration,” ASTM International, West Conshohocken, PA, 2010, 7 pp. doi: 10.1520/C1202-10

25. ASTM C596-01, “Standard Test Method for Drying Shrinkage of Mortar Containing Hydraulic Cement,” ASTM International, West Conshohocken, PA, 2001, 3 pp. doi: 10.1520/C0596-01

26. Özbay, E.; Karahan, O.; Lachemi, M.; Hossain, K. M. A.; and Atis, C. D., “Dual Effectiveness of Freezing–Thawing and Sulfate Attack on High-Volume Slag-Incorporated ECC,” Composites Part B: Engineering, V. 45, No. 1, 2013, pp. 1384-1390. doi: 10.1016/j.compositesb.2012.07.038

27. Şahmaran, M., and Li, V. C., “Durability Properties of Micro-Cracked ECC Containing High Volumes Fly Ash,” Cement and Concrete Research, V. 39, No. 11, 2009, pp. 1033-1043. doi: 10.1016/j.cemconres.2009.07.009

28. Li, M., and Li, V. C., “Behavior of ECC/Concrete Layer Repair System Under Drying Shrinkage Conditions,” Restoration of Buildings and Monuments, V. 12, No. 2, 2006, pp. 143-160. doi: 10.1515/rbm-2006-6040

29. Calis, G.; Yildizel, S. A.; Erzin, S.; and Tayeh, B. A., “Evaluation and Optimisation of Foam Concrete Containing Ground Calcium Carbonate and Glass Fibre (Experimental and Modelling Study),” Case Studies in Construction Materials, V. 15, 2021, Article No. e00625. doi: 10.1016/j.cscm.2021.e00625


ALSO AVAILABLE IN:

Electronic Materials Journal