Studies on Portland Slag Cement Made Using Blast Furnace and Linz-Donawitz Slag

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Studies on Portland Slag Cement Made Using Blast Furnace and Linz-Donawitz Slag

Author(s): P. N. Ojha, Abhishek Singh, Brijesh Singh, Subhadra Sen, Ritesh Kumar, and Biswajit M. Patra

Publication: Materials Journal

Volume: 120

Issue: 1

Appears on pages(s): 143-154

Keywords: composite slag; durability; granulated blast-furnace slag (GBFS); Linz-Donawitz (LD) slag; portland slag cement (PSC)

DOI: 10.14359/51737289

Date: 1/1/2023

Abstract:
This study aims to investigate the possibility of using Linz-Donawitz (LD) slag as one of the cementitious materials for preparation of composite slag (having 8 and 15% LD slag), which will subsequently be used for manufacturing portland slag cement (PSC). PSC samples (having overall 4 to 9% LD slag) were prepared using LD slag from two sources in a laboratory ball mill. PSC samples were analyzed for various chemical characteristics and physical properties. Studies were conducted on concrete mixtures prepared at water-cement ratios (w/c) of 0.65 and 0.40. Fresh, hardened, and durability properties of concrete mixtures prepared using PSCs made with composite slag having up to 15% LD slag were found to be comparable to their corresponding control mixtures. Based on results, it was observed that composite slag having LD slag up to 15% of total slag can be used up to 60% for manufacturing PSC along with clinker and gypsum. The 3-, 7-, and 28-day compressive strength of PSC samples containing LD slags in different proportions were found to be comparable to control PSC samples and meeting the requirements of IS 455:2015. Even though the free lime content in LD slags was significantly higher (free lime content of 3.03 and 3.48%) in comparison to granulated blast-furnace slag (GBFS), it had almost a negligible effect on the PSC prepared using LD slag and soundness of experimental and control PSC was comparable because the maximum amount of LD slag added in overall PSC was restricted to 9%. The addition of LD slag in different proportions up to 9% in overall PSC does not seem to have any detrimental effect on performance of concrete in terms of sorptivity, carbonation depth, chloride penetration, and diffusion, which indicates its suitability for application in reinforced concrete structures.

Related References:

1. Cement Compendium, “The India Cement Industry – 2019,” National Council for Cement and Building Materials, Ballabgarh, India, 2019.

2. Low Carbon Technology Roadmap for the Indian Cement Sector, “Status Review 2018, WBCSD,” Nov. 2018.

3. Ghisellini, P.; Ripa, M.; and Ulgiati, S., “Exploring Environmental and Economic Costs and Benefits of a Circular Economy Approach to the Construction and Demolition Sector: A Literature Review,” Journal of Cleaner Production, V. 178, 2018, pp. 618-643. doi: 10.1016/j.jclepro.2017.11.207

4. Mahinroosta, M.; Karimi, Z.; and Allahverdi, A., “Recycling of Red Mud for Value-Added Applications: A Comprehensive Review,” Encyclopedia of Renewable and Sustainable Materials, 2019.

5. Singh, S. K.; Jyoti; and Vashistha, P., “Development of Newer Composite Cement through Mechano-Chemical Activation of Steel Slag,” Construction and Building Materials, V. 268, 2021, p. 121147. doi: 10.1016/j.conbuildmat.2020.121147

6. Palod, R.; Deo, S. V.; and Ramtekkar, G. D., “Sustainable Approach for Linz-Donawitz Slag Waste as a Replacement of Cement in Concrete: Mechanical, Microstructural, and Durability Properties,” Advances in Civil Engineering, 2020, pp. 1-9. doi: 10.1155/2020/5691261

7. Allahverdi, A.; Shahrbabaki, M. N.; Ghezelasheghi, M.; and Mahinroosta, M., “Sulfate Resistance of RFCC Spent Catalyst-Blended Portland Cement,” Boletín de la Sociedad Española de Cerámica y Vidrio, 2018.

8. Allahverdi, A.; Maleki, A.; and Mahinroosta, M., “Enhancement of Hydraulic Activity of Slag-Blended Portland Cement,” Asian Journal of Civil Engineering, V. 19, 2018, pp. 1009-1020.

9. World Crude Steel Production, Summary, World Steel Association, Jan. 24, 2018, https://worldsteel.org/media-centre/press-releases/2018/world-crude-steel-output-increases-by-5-3-in-2017/. (last accessed Jan. 27, 2023)

10. Tossavainen, M.; Engstrom, F.; Yang, Q.; Menad, N.; Lidstrom Larsson, M.; and Bjorkman, B., “Characteristics of Steel Slag under Different Cooling Conditions,” Waste Management (New York, N.Y.), V. 27, No. 10, 2007, pp. 1335-1344. doi: 10.1016/j.wasman.2006.08.002

11. Proctor, D. M.; Fehling, K. A.; Shay, E. C.; Wittenborn, J. L.; Green, J. J.; Avent, C.; Bigham, R. D.; Connolly, M.; Lee, B.; Shepker, T. O.; and Zak, M. A., “Physical and Chemical Characteristics of Blast Furnace, Basic Oxygen Furnace, and Electric Arc Furnace Steel Industry Slags,” Environmental Science & Technology, V. 34, No. 8, 2000, pp. 1576-1582. doi: 10.1021/es9906002

12. Das, B.; Prakash, S.; Reddy, P. S. R.; and Misra, V. N., “An Overview of Utilization of Slag and Sludge from Steel Industries,” Resources, Conservation and Recycling, V. 50, No. 1, 2007, pp. 40-57. doi: 10.1016/j.resconrec.2006.05.008

13. Yadav, U. S.; Das, B. K.; Kumar, A.; and Sandhu, H. S., “Solid Waste Recycling through Sinter Status at Tata Steel,” Proceedings on International Environment and Waste Management, NML, Jamshedpur, India, 2002, pp. 81-94.

14. Umadevi, T.; Rao, S. P.; and Roy, P., “Influence of LD Slag on Iron Ore Sinter Properties and Productivity,” 6th International Seminar on Mineral Processing Technology, NML Jamshedpur, Jamshedpur, India, 2010, pp. 747-757.

15. Ministry of Steel, Government of India, Annual Report 2017-2018, Feb. 9, 2018, https://steel.gov.in/annual-reports. (last accessed Jan. 27, 2023)

16. Pal, J.; Chaudhary, P. N.; and Goswami, M. C., “Utilization of LD Slag – An Overview,” Journal of Metallurgy and Materials Science, V. 45, No. 2, 2003, pp. 61-72.

17. Motz, H., and Geiseler, J., “Products of Steel Slags; An Opportunity to Save Natural Resources,” Waste Management (New York, N.Y.), V. 21, No. 3, 2001, pp. 285-293. doi: 10.1016/S0956-053X(00)00102-1

18. Wimmer, G.; Wulfert, H.; and Ludwig, H. M., “A New Process for Production of Cement Clinker from Steel Making Slags,” Proceedings of the 14th NCB International Seminar on Cement and Building Materials, New Delhi, India, 2015.

19. Shen, W.; Zhou, M.; Ma, W.; Hu, J.; and Cai, Z., “Investigation on the Application of Steel Slag-Fly Ash-Phosphogypsum Solidified Material as Road Base Material,” Journal of Hazardous Materials, V. 164, No. 1, 2009, pp. 99-104. doi: 10.1016/j.jhazmat.2008.07.125

20. Erlin, B., and Jana, D., “Forces of Hydration that Can Cause Havoc in Concrete,” Concrete International, V. 25, No. 11, Nov. 2003, pp. 51-57.

21. Chand, S.; Paul, B.; and Kumar, M., “A Comparative Study of Physicochemical and Mineralogical Properties of LD Slags from Some Selected Steel Plants in India,” International Journal of Environmental Science and Technology, V. 9, No. 1, 2015, pp. 75-87. doi: 10.3923/jest.2016.75.87

22. IS 455:2015, “Portland Slag Cement – Specification,” Bureau of Indian Standards, New Delhi, India, 2015.

23. IS 4032:1985 (Reaffirmed 2010), “Methods of Chemical Analysis of Hydraulic Cement,” Bureau of Indian Standards, New Delhi, India, 2010.

24. IS 12089:1987 (Reaffirmed 2008), “Specification for Granulated Slag for Manufacture of Portland Slag Cement,” Bureau of Indian Standards, New Delhi, India, 2008.

25. IS 16714:2018, “Ground Granulated Blast Furnace Slag for Use in Cement, Mortar and Concrete – Specification,” Bureau of Indian Standards, New Delhi, India, 2018.

26. IS 10218:1982 (Reaffirmed 2006), “Method of Determination of Grindability Index,” Bureau of Indian Standards, New Delhi, India, 2006.

27. IS 4031(2):1999 (Reaffirmed 2017), “Methods of Physical Tests for Hydraulic Cement - Part 2: Determination of Fineness by Specific Surface by Blaine Air Permeability Method,” Bureau of Indian Standards, New Delhi, India, 2017.

28. IS 4031(4):1988 (Reaffirmed 2005), “Methods of Physical Tests for Hydraulic Cement - Part 4: Determination of Consistency of Standard Cement Paste,” Bureau of Indian Standards, New Delhi, India, 2005.

29. IS 4031(5):1988 (Reaffirmed 2005), “Methods of Physical Tests for Hydraulic Cement - Part 5: Determination of Initial and Final Setting Times,” Bureau of Indian Standards, New Delhi, India, 2005.

30. IS 4031(6):1988 (Reaffirmed 2005), “Methods of Physical Tests for Hydraulic Cement - Part 6: Determination of Compressive Strength of Hydraulic Cement Other Than Masonry Cement,” Bureau of Indian Standards, New Delhi, India, 2005.

31. IS 4031(3):1988 (Reaffirmed 2005), “Methods of Physical Tests for Hydraulic Cement - Part 3: Determination of Soundness,” Bureau of Indian Standards, New Delhi, India, 2005.

32. IS 1199:1959 (Reaffirmed 2004), “Methods of Sampling and Analysis of Concrete,” Bureau of Indian Standards, New Delhi, India, 2004.

33. IS 516:1959 (Reaffirmed 2004), “Method of Tests for Strength of Concrete,” Bureau of Indian Standards, New Delhi, India, 2004.

34. Arora, V. V.; Singh, B.; and Jain, S., “Experimental Studies on Short Term Mechanical Properties of High Strength Concrete,” Indian Concrete Journal, V. 90, No. 10, 2016, pp. 65-75.

35. Arora, V. V.; Singh, B.; and Jain, S., “Effect of Indigenous Aggregate Type on Mechanical Properties of High Strength Concrete,” Indian Concrete Journal, V. 91, No. 1, 2017, pp. 34-44.

36. Arora, V. V.; Singh, B.; Patel, V.; and Trivedi, A., “Evaluation of Modulus of Elasticity for Normal and High Strength Concrete with Granite and Calc‐Granulite Aggregate,” Structural Concrete, V. 22, 2021, doi: 10.1002/suco.202000023

37. Ojha, P. N.; Singh, B.; Singh, A.; Patel, V.; and Arora, V. v., “Experimental Study on Creep and Shrinkage Behaviour of High Strength Concrete,” Indian Concrete Journal, V. 95, No. 2, 2021, pp. 30-42.

38. Ojha, P. N.; Singh, A.; Singh, B.; and Patel, V., “Mechanical and Durability Properties of Cement Mortar and Concrete Reinforced with Glass Micro Fibre,” Research on Engineering Structures and Materials, 2021.

39. ASTM C1202-19, “Standard Test Method for Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration,” ASTM International, West Conshohocken, PA, 2019, 8 pp.

40. Ojha, P. N.; Singh, B.; Kaura, P.; and Singh, A., “Lightweight Geopolymer Fly Ash Sand: An Alternative to Fine Aggregate for Concrete Production,” Research on Engineering Structures and Materials, 2021.

41. ISO 1920-11:2013 (Reaffirmed 2018), “Testing of Concrete - Part 11: Determination of the Chloride Resistance of Concrete, Unidirectional Diffusion,” International Organization for Standardization, Geneva, Switzerland, 2018.

42. ISO 1920-12:2015, “Testing Of Concrete - Part 12: Determination of the Carbonation Resistance of Concrete - Accelerated Carbonation Method,” International Organization for Standardization, Geneva, Switzerland, 2015.

43. ASTM C1585-20, “Standard Test Method for Measurement of Rate of Absorption of Water by Hydraulic-Cement Concretes,” ASTM International, West Conshohocken, PA, 2020, 6 pp.

44. IS 383:2016, “Coarse and Fine Aggregate for Concrete—Specification,” Bureau of Indian Standards, New Delhi, India, 2016.

45. Arora, V. V., and Kaura, P., “Suitability of Accelerated Test Methods as a Tool for Service Life Prediction of RC Structures Made of Ordinary Portland and Blended Cement,” RILEM Annual Week & ICACMS, Chennai, India, 2017


ALSO AVAILABLE IN:

Electronic Materials Journal