Numerical Evaluation of a New Concrete Sandwich Panel Containing UHPC Wythes, and GFRP Reinforcement and Connectors

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Numerical Evaluation of a New Concrete Sandwich Panel Containing UHPC Wythes, and GFRP Reinforcement and Connectors

Author(s): Akram Jawdhari and Amir Fam

Publication: Symposium Paper

Volume: 356

Issue:

Appears on pages(s): 273-290

Keywords: concrete, composite degree, FRP, finite element, numerical analysis, sandwich panels, shear connectors, ultra-high-performance concrete (UHPC), thin panels

DOI: 10.14359/51737276

Date: 10/1/2022

Abstract:
Recently, a new generation of concrete sandwich panels (CSPs) comprising ultra-high performance concrete (UHPC) wythes and glass fiber reinforced polymer (GFRP) as reinforcement and shear connectors was developed and evaluated experimentally. In this study, a non-linear finite element model is presented to study the detailed behavior of these panels under bending. The model included detailed features such as a constitutive material law that considers the post-crack stiffening of UHPC, failure of GFRP material, wythe-to-insulation contact and slipping, and stability failure. Compared with eight previously tested panels, the model predictions of ultimate load, general load-deflection behavior, and failure modes matched those from experiments. The composite degree of each panel, a key design parameter frequently used in characterizing the structural and thermal efficiencies of CSPs, was determined from the ultimate load of the tested panel and that of two additional numerically-based non and fully composite ones and ranged between 3 to 34%. The structural performance of the GFRP connector was deemed satisfactory for the range of composite degrees proposed for the panels. The validated model will be deployed in a large parametric analysis studying different material and geometric variables and assisting in developing a design tool to estimate the strength and composite degree of UHPC CSPs with GFRP reinforcement.