Title: Parking Structure Failure and Incidents

Author(s): by William L. Gamble

Publication: Concrete International

Volume: 44

Issue: 10

Appears on pages(s): 39-44

Keywords: collapse, barrier, concrete, design

DOI:

Date: 10/1/2022

Abstract:
The article reviews structural problems with concrete parking structures, including incidents of vehicles going through edge barriers. Recommendations are provided for implementing current requirements on parking barriers to avoid or minimize future incidents.




  