Evaluation of FRP Bars & Meshes Used as Secondary Reinforcement for Nonstructural Concrete Members for Building Code Compliance
Author(s):
Mahmut Ekenel, Hossein Roghani, Francisco De Caso y Basalo, and Antonio Nanni
Publication:
Symposium Paper
Volume:
356
Issue:
Appears on pages(s):
109-119
Keywords:
building codes; composites; FRP Bars; FRP meshes; noncorrosive; non-structural; reinforcement
DOI:
10.14359/51737250
Date:
10/1/2022
Abstract:
Advances in technology have opened doors for building construction with new materials that are lightweight, efficient, noncorrosive, and reliable in terms of durability without a sacrifice in strength and performance. One of these technologies is the use of FRP bars and meshes in concrete members as internal reinforcement. Although FRP bars as structural reinforcement in concrete members have been successfully utilized in building and bridge projects (i.e., slabs, beams, etc.) for the past three decades; recently, there has been an interest in using FRP bars and meshes as secondary reinforcement for non-structural concrete members such as plain concrete footings, concrete slabs-on-ground, and plain concrete walls in lieu of code-compliant conventional temperature and shrinkage steel reinforcement. Because the use of FRP bars and meshes as secondary reinforcement is not within the provisions of the International Building Code (IBC), the predominant building code in the United States, an acceptance criterion (AC521) has been developed under IBC Section 104.11. This paper explains the requirements of AC521, and how FRP bars and meshes as secondary reinforcement of nonstructural concrete members are evaluated to show compliance with the provisions of the IBC.
Related References:
ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI318-11) and Commentary,” ACI 318-11, American Concrete Institute, Farmington Hills, MI, 2011.
ACI Committee 332-14, “Residential Code Requirements for Structural Concrete and Commentary”, American Concrete Institute, Farmington Hills, MI.
ACI Committee 360-10, “Guide to Design of Slabs-on-Ground”, American Concrete Institute, Farmington Hills, MI.
ACI Committee 440.5-08, “Specification for Construction with Fiber-Reinforced Polymer Reinforcing Bars”, American Concrete Institute, Farmington Hills, MI.
AC521, “ICC-ES Acceptance Criteria for Fiber-Reinforced Polymer (FRP) Bars and Meshes for Internal Reinforcement of Non-Structural Concrete Members,” AC521, ICC Evaluation Services, Inc., October 2020.
ASTM A1064 – 18A, Standard Specification for Carbon-Steel Wire and Welded Wire Reinforcement, Plain and Deformed, for Concrete, ASTM International.
ASTM C1579, Standard Test Method for Evaluating Plastic Shrinkage Cracking of Restrained Fiber Reinforced Concrete (Using a Steel Form Insert), ASTM International.
ASTM D570-98 (2010) e1, Standard Test Method for Water Absorption of Plastics, ASTM International.
ASTM D792-13, Standard Test Methods for Density and Specific Gravity (Relative Density) of Plastics by Displacement, ASTM International.
ASTM D2584-11, Test Method for Ignition Loss of Cured Reinforced Resins, ASTM International.
ASTM D4475-02(2008), Standard Test Method for Apparent Horizontal Shear Strength of Pultruded Reinforced Plastic Rods by the Short-Beam Method, ASTM International.
ASTM D5229/D5229M-14 Standard Test Method for Moisture Absorption Properties and Equilibrium Conditioning of Polymer Matrix Composite Materials, ASTM International.
ASTM D7205/D7205M-06 (2011), Standard Test Method for Tensile Properties of Fiber–Reinforced Polymer Matrix Composite Bars, ASTM International.
ASTM D7617/D7617M-11, Standard Test Method for Transverse Shear Strength of Fiber–Reinforced Polymer Matrix Composite Bars, ASTM International.
ASTM D7913/D7913M-14(2020), Test Method for Bond Strength of Fiber-Reinforced Polymer Matrix Composite Bars to Concrete by Pullout Testing, ASTM International.
ASTM D7957/D7957M-17, Standard Specification for Solid Round Glass Fiber Reinforced Polymer Bars for Concrete Reinforcement, ASTM International.
ASTM E1356-08 (2014), Standard Test Method for Assignment of the Glass Transition Temperatures by Differential Scanning Calorimetry, ASTM International.
ASTM E1640-13, Standard Test Method for Assignment of the Glass Transition Temperature by Dynamic Mechanical Analysis, ASTM International.
ASTM E2160–04 (Reapproved 2012), Standard Test Method for Heat of Reaction of Thermally Reactive Materials by Differential Scanning Calorimetry, ASTM International.
IBC and IRC, 2018, International Code Council, “International Building Code (IBC); International Residential Code (IRC),” International Code Council, Country Club Hills, IL, 2018 edition.
ISO/IEC 17025, 2017, “General requirements for the competence of testing and calibration laboratories” International Organization for Standardization, Geneva, Switzerland.
ISO/IEC 17065, 2012, “Conformity assessment -- Requirements for bodies certifying products, processes and services” International Organization for Standardization, Geneva, Switzerland.