Effect of Cast-in-Place Beams on Seismic Performance of Precast Shear Walls

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Cast-in-Place Beams on Seismic Performance of Precast Shear Walls

Author(s): Wei Zhang, Deuckhang Lee, Won-Jun Lee, Min-Su Kim, and Je-Young Park

Publication: Structural Journal

Volume: 120

Issue: 1

Appears on pages(s): 89-102

Keywords: cast-in-place (CIP) beam; precast; seismic performance; shear wall; underground

DOI: 10.14359/51737231

Date: 1/1/2023

Abstract:
There is a drastic change in design and construction trends of underground structures, where a precast concrete (PC) shear wall system is quickly replacing a cast-in-place (CIP) diaphragm wall (that is, the so-called slurry wall) system in urban areas for better constructability and reliable performances. However, it is challenging to achieve the proper coupling action or composite performance through vertical connections between adjacent PC walls and that in horizontal connection between PC walls and foundations to satisfy the seismic design criteria specified in codes. To this end, this study introduces cast-in-place (CIP) cap beam and waling beam at the top and midheight of PC walls to connect individual precast wall panels by means of a coupling action. Precast specimens were carefully designed to be code-compliant as intermediate precast shear wall systems, and were then fabricated and tested under the reversed cyclic loads to evaluate seismic performances. Detailed numerical models were also developed to identify how CIP beams can effectively improve the seismic performance of a precast shear wall system by restraining the free rotation and axial deformation of individual precast wall panels.

Related References:

1. Jaillon, L., and Poon, C. S., “Sustainable Construction Aspects of Using Prefabrication in Dense Urban Environment: A Hong Kong Case Study,” Construction Management and Economics, V. 26, No. 9, 2008, pp. 953-966. doi: 10.1080/01446190802259043

2. Lee, D. H.; Park, M. K.; Ju, H. E.; Han, S. J.; and Kim, K. S., “Strengths of Thick Prestressed Precast Hollow-Core Slab Members Strengthened in Shear,” ACI Structural Journal, V. 117, No. 2, Mar. 2020, pp. 129-140. doi: 10.14359/51720203

3. Jaillon, L., and Poon, C. S., “The Evolution of Prefabricated Residential Building Systems in Hong Kong: A Review of the Public and the Private Sector,” Automation in Construction, V. 18, No. 3, 2009, pp. 239-248. doi: 10.1016/j.autcon.2008.09.002

4. Richard, R. B., “Industrialised Building Systems: Reproduction before Automation and Robotics,” Automation in Construction, V. 14, No. 4, 2005, pp. 442-451. doi: 10.1016/j.autcon.2004.09.009

5. Dong, Y. H.; Jaillon, L.; Chu, P.; and Poon, C. S., “Comparing Carbon Emissions of Precast and Cast-in-Situ Construction Methods—A Case Study of High-Rise Private Building,” Construction and Building Materials, V. 99, 2015, pp. 39-53. doi:10.1016/j.conbuildmat.2015.08.14510.1016/j.conbuildmat.2015.08.145

6. Zhang, D. C.; Fleischman, R.; and Lee, D. H., “Verification of Diaphragm Seismic Design Factors for Precast Concrete Office Buildings,” Earthquakes and Structures, V. 20, No. 1, 2021, pp. 13-27. doi: 10.12989/sem.2019.71.6.643

7. Han, S. J.; Lee, D. H.; and Kim, K. S., “Web-Shear Capacity of Prestressed Composite Inverted Multi-Tee Slabs,” ACI Structural Journal, V. 118, No. 3, May 2021, pp. 295-304. doi: 10.14359/51730538

8. Heo, I. W.; Kang, H.; Lee, D. H.; Oh, J. Y.; Lee, J. M.; and Kim, K. S., “Performance-Based Fire Behavior Analysis for Underground Parking Structures,” International Journal of Urban Sciences, V. 20, Supplement 1, 2016, pp. 90-100. doi: 10.1080/12265934.2016.117816510.1080/12265934.2016.1178165

9. Comodromos, E. M.; Papadopoulou, M. C.; and Konstantinidis, G. K., “Effects from Diaphragm Wall Installation to Surrounding Soil and Adjacent Buildings,” Computers and Geotechnics, V. 53, 2013, pp. 106-121. doi: 10.1016/j.compgeo.2013.05.003

10. Gudjon, O. J., “Functional Requirements for Permanent Diaphragm Walls,” master’s thesis, Department of Civil and Environmental Engineering, Chalmers University of Technology, Gothenburg, Sweden, 2014, 62 pp.

11. Shu, J.; Sun, J.; Zhang, D.; and Wei, H., “Sequential Measurement and Analysis of Large Underground Retaining Structures by Diaphragm Wall Anchor for the Spring Area,” Advances in Civil Engineering, V. 2019, 2019, pp. 1-21. doi: 10.1155/2019/5291420

12. Yao, C.; Yan, Q.; Sun, M.; Dong, W.; and Guo, D., “Rigid Diaphragm Wall with a Relief Shelf to Mitigate the Deformations of Soil and Shallow Foundations Subjected to Normal Faulting,” Soil Dynamics and Earthquake Engineering, V. 137, 2020, p. 106264. doi:10.1016/j. soildyn.2020.10626410.1016/j

13. Sun, C. F.; Liang, S. T.; Zhu, X. J.; Li, H.; Guo, J. M.; Li, G.; Song, Y. M.; and Wu, D. Y., “Experimental Study and Numerical Simulation of Precast Shear Wall with Rabbet-Unbonded Horizontal Connection,” International Journal of Concrete Structures and Materials, V. 14, No. 1, 2020, 16 pp. doi: 10.1186/s40069-019-0379-3

14. KDS 41 17 00, “Building Seismic Design: Standard,” Architectural Institute of Korea, Seoul, Korea, 2019, 123 pp.

15. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 623 pp.

16. ASCE 7-16, “Minimum Design Loads and Associated Criteria for Buildings and Other Structures,” American Society of Civil Engineers, Reston, VA, 2016.

17. Lee, D.; Kang, T. H. K.; Ju, H.; Moon, S.-W.; and Yang, I.-S., “Seismic Performance of Reinforced Concrete Column-Foundation Connections Using Combo-Type Mechanical Splices,” ACI Structural Journal, V. 116, No. 5, Sept. 2019, pp. 173-186. doi: 10.14359/51716766

18. El-Tawil, S.; Kuenzli, C. M.; and Hassan, M., “Pushover of Hybrid Coupled Walls. I: Design and Modeling,” Journal of Structural Engineering, ASCE, V. 128, No. 10, 2002, pp. 1272-1281. doi: 10.1061/(ASCE)0733-9445(2002)128:10(1272)

19. ACI Committee 374, “Guide for Testing Reinforced Concrete Structural Elements under Slowly Applied Simulated Seismic Loads (ACI 374.2-13),” American Concrete Institute, Farmington Hills, MI, 2013, 18 pp.

20. ASCE/SEI 41-17, “Seismic Rehabilitation of Existing Buildings,” American Society of Civil Engineers, Reston, VA, 2017.

21. Ameen, S.; Lequesne, R. D.; and Lepage, A., “Diagonally Reinforced Concrete Coupling Beams with Grade 120 (830) High-Strength Steel Bars,” ACI Structural Journal, V. 117, No. 6, Nov. 2020, pp. 199-210. doi: 10.14359/51728067

22. Zhang, W.; Lee, D. H.; Ikechukwu, O.; and Okonkwo, M., “Nonlinear Shear Analysis of Corroded RC Beams Considering Bond Mechanism,” ACI Structural Journal, V. 118, No. 6, Nov. 2021, pp. 47-61. doi:10.14359/5173299610.14359/51732996

23. Zhang, W.; Lee, D. H.; Lee, C. J.; Zhang, X. H.; and Ikechukwu, O., “Bond Performance of SFRC Considering Random Distributions of Aggregates and Steel Fibers,” Construction and Building Materials, V. 291, 2021, p. 123304. doi: 10.1016/j.conbuildmat.2021.123304


ALSO AVAILABLE IN:

Electronic Structural Journal