Evaluation of Electromagnetic Pulse Shielding Performance of Carbon Fiber-Mixed Cement Paste

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Evaluation of Electromagnetic Pulse Shielding Performance of Carbon Fiber-Mixed Cement Paste

Author(s): Tae-Beom Min & Hyeong-Kyu Cho

Publication: IJCSM

Volume: 16

Issue:

Appears on pages(s):

Keywords: cement, EMP shielding, milled carbon fiber, concrete

DOI: 10.1186/s40069-022-00500-4

Date: 7/31/2022

Abstract:
This study investigated the physical properties and electromagnetic pulse (EMP) shielding performance of cement paste containing small-diameter carbon fibers to develop an EMP-shielding cement. Small-diameter carbon fibers were used as a cement admixture because the powders were approximately 100 μm in length and were visually powder-shaped. As a result of the experiment, it was indicated that ordinary Portland cement do not have shielding performance. However, cement paste with 5% carbon fibers showed effectiveness in compressive strength and EMP shielding. However, the shielding performance did not increase when the cement contained more than 5% carbon fibers. Furthermore, a review of the EMP shielding performance relative to the thickness of the specimen showed that the plain cement without small-diameter carbon fibers did not increase the shielding performance with an increase in thickness, but the shielding performance of the specimens with small-diameter carbon fibers increased with an increase in thickness. Therefore, it was more effective to increase the thickness of the cement containing 5% carbon fibers rather than increasing the carbon fiber content.