Seismic Safety Evaluation of Concrete Dams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seismic Safety Evaluation of Concrete Dams

Author(s): Kenneth D. Hansen

Publication: Concrete International

Volume: 44

Issue: 9

Appears on pages(s): 33-41

Keywords: crack, stress, earthquake, shaking

DOI: 10.14359/51737203

Date: 9/1/2022

Abstract:
The article discusses the seismic safety of existing concrete dams and demonstrates why the probability of a concrete dam failing due to seismic shaking is extremely remote. It focuses on historical evolution of seismic design and analysis, lessons learned from previous earthquakes, causes of seismic induced damage, seismic safety assessment in the United States, and seismic failure modes for different dam types.

Related References:

1. ICOLD Bulletin 148, “Selecting Seismic Parameters for Large Dams, Guidelines,” International Commission on Large Dams, Paris,France, 2010, 37 pp.

2. Westergaard, H.M., “Water Pressures on Dams During Earthquakes,” ASCE, Transaction 98, 1933.

3. Hansen, K.D., and Nuss, L.K., “Seismic Upgrades for Concrete Dams – Then and Now,” The Journal of Dam Safety, V. 11, No. 4, July 2013, pp. 21-35.

4. Chopra, A.K., Earthquake Engineering for Concrete Dams: Analysis, Design, and Evaluation, first edition, Wiley-Blackwell, Hoboken, NJ, 2020, 320 pp.

5. Curtis, D.D.; Sooch, G.; Brewer T.; and Schildmeyer, A., “Explicit Seismic Analysis of Mossyrock Dam,” Proceedings of USSD 33rd Annual Conference, Phoenix, AZ, Feb. 11-15, 2013, p. 23.

6. Nuss, L.K.; Matsumoto, N.; and Hansen, K.D., “Shaken, but not Stirred – Earthquake Performance of Concrete Dams,” Proceedings of the 32nd USSD Annual Conference, New Orleans, LA, Apr. 23-27, 2012, p. 189.

7. Charlwood, R., and Little, T., “Dam Earthquake Damage in Taiwan Assessed,” USCOLD Newsletter, No. 19, Nov. 1999, p. 1, 4, and 5.

8. Parme, A.L., Consultant to the Los Angeles Flood Control District, personal correspondence, 1971, to include portions of the Cal Tech report on Pacoima Dam, 1978.

9. Shen, C.; Chen, H.; Huang, L.; Li, T.; Yang, C.; and Lo, A., “Earthquake Induced by Reservoir Impounding and their Effects on Hsinfengkiang Dam,” Scientia Sinica, V. 17, No. 2, 1974, pp. 239-272.

10. Ahmadi, M.T.; Khoshrang, G.; Mokhtarzadeh, A.; and Jalalzadeh, A., “Behavior of a Large Concrete Dam due to an Actual Maximum Credible Earthquake,” Proceedings of Tenth World Conference on Earthquake Engineering, Rotterdam, Holland, 1992, pp. 3995-4000.

11. Wieland, M., “Damage of Sefid Rud Buttress Dam Project in Iran Caused by the Magnitude 7.4 Manjil Earthquake of June 21, 1990,” INCOLD Journal, V. 10, No. 2, 2021 pp. 4-14.

12. Raphael, J.M., “Tensile Strength of Concrete,” ACI Journal Proceedings, V. 81, No. 2, Mar. 1984, pp. 158-165.

13. Wong, W.C.; Bischoff, J.A.; and Callahan J.F., “The Seismic Reinforcement of Gibraltar Arch Dam,” Proceedings of Ninth World Conference of Earthquake Engineering, Tokyo-Kyoto, Japan, V. VII, Aug. 2-9, 1988, pp. 493-498.

14. Tarbox, G.; Iso-Ahola, V.; and Schultz, M., “The Seismic and Hydraulic Rehabilitation of Big Tujunga Dam,” The Journal of Dam Safety, V. 10, No. 2, 2012, pp. 8-17.

15. Hall, J.F., “Dams and Earthquake Safety,” Engineering and Science, V. 47, No. 5, May 1984, pp. 17-20.

16. “Engineering Guidelines for the Evaluation of Hydropower Projects, Chapter 11 – Arch Dams,” Federal Energy Regulatory Commission (FERC), Washington, DC, 2018, 104 pp.

17. Wieland, M., “Dam Safety and Earthquakes,” personal communication, 2020.

18. “San Francisco’s Historic Dam Undergoes Core Sampling Work,” Western Construction, July 1976.

19. Payne, T., “Shaking Table Study to Investigate Failure Modes of Arch Dams,” Report No. DSO-02-01, Bureau of Reclamation, Denver, CO, Mar. 2002, 243 pp.

20. Hansen, K.D., and Forbes, B.A., “Some of These Dams Are Not What They Are Cracked Up to Be – Thermal Performance of RCC Dams,”2012 Dam Safety Conference Proceedings, Denver, CO, Sept. 16-20, 2012.

21. Matsumoto, N.; Sasaki, T.; and Sato N., “The Behavior of Dams During the M9 Tohoku Earthquake, Japan,” The International Journal on Hydropower and Dams, V. 19, No. 3, 2012.

22. Noguera, G., “Dam Performance During the Cauquenes (Chile) Earthquake of February 2010,” presented to ICOLD Committee on Seismic Aspects of Dam Design, Hanoi, Vietnam, May 2010.

23. Walters, R.C., “Damage by Earthquake to Blackbrook Dam,” Eighth International Congress of Large Dams, Question 20, Lovyborough, England, 1964.

24. Zhang, C., “The Performance of Dams During the Wenchuan 5-12 Earthquake and Lessons Learned from the Event,” International Journal of Earthquake and Tsunami, V. 5, No. 4, 2011, pp. 309-327.