Title: Turning Buildings into Carbon Storage Structures

Author(s):

Publication: Concrete International

Volume: 44

Issue: 9

Appears on pages(s): 28-29

Keywords:

DOI: 10.14359/51737201

Date: 9/1/2022

Abstract:
The University of Pennsylvania (Penn) has been selected to receive $2.4M in funding from the U.S. Department of Energy Advanced Research Projects Agency-Energy (ARPA-E).