Effect of Bacterial Spore in Surface-Treated Fiber-Reinforced Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Bacterial Spore in Surface-Treated Fiber-Reinforced Concrete

Author(s): Davood Mostofinejad, Nasrin Karimi, and Bahareh Tayebani

Publication: Materials Journal

Volume: 119

Issue: 6

Appears on pages(s): 263-272

Keywords: bacteria; compressive strength; electrical resistance; fiber; spore; water absorption

DOI: 10.14359/51737198

Date: 11/1/2022

Abstract:
One way to reinforce concrete is to use steel bars. It is essential to find substitute artificial materials because such bars are prone to corrosion, and reinforcing steel suffers from the penetration of hazardous substances into porous concrete. Several solutions have been proposed in recent years for reducing the pores and microcracks thus created. From these solutions, biological methods have attracted more attention due to their cost-effective and eco-friendly nature. On the other hand, fiber reinforcement may significantly improve concrete tensile strength, crack-related properties, and ductility. In the present study, Bacillus subtilis is used in specimens in which one of the three polypropylene, hooked-end steel, or barchip fibers (at volume percentages of 0.3%, 1%, and 0.75%, respectively) is considered as reinforcement. Moreover, bacterial strains in the culture medium are used in place of concrete mixing water, and bacterial spores in the culture medium are applied as a surface treatment gel. Cylindrical specimens were cast to be used for the compressive strength, water absorption, and electrical resistance tests. With a reduction of 36% in water absorption, the bacterial specimens outperformed their corresponding controls. The compressive strength test revealed an increase of 25.5% in compressive strength in surface-treated specimens relative to the corresponding control ones. The best performance of bacteria was observed in reducing electrical resistance in the concrete specimens reinforced with polypropylene fibers. Overall, the three applications of bacteria were found capable of forming calcite sediments, with greater deposits formed due to bacterial activity than by the spores used in the surface treatment.

Related References:

1. Islam, M. M. U., “Investigation of Long-Term Tension Stiffening Mechanism for Ultra-High-Performance Fiber Reinforced Concrete (UHPFRC),” Construction and Building Materials, V. 321, 2022, p. 126310. doi: 10.1016/j.conbuildmat.2022.126310

2. Islam, M. M. U.; Li, J.; Wu, Y. F.; Roychand, R.; and Saberian, M., “Design and Strength Optimization Method for the Production of Structural Lightweight Concrete: An Experimental Investigation for the Complete Replacement of Conventional Coarse Aggregates by Waste Rubber Particles,” Resources, Conservation and Recycling, V. 184, 2022, p. 106390. doi: 10.1016/j.resconrec.2022.106390

3. Islam, M. M. U.; Mo, K. H.; Alengaram, U. J.; and Jumaat, M. Z., “Mechanical and Fresh Properties of Sustainable Oil Palm Shell Lightweight Concrete Incorporating Palm Oil Fuel Ash,” Journal of Cleaner Production, V. 115, 2016, pp. 307-314. doi: 10.1016/j.jclepro.2015.12.051

4. Knoben, W., “Bacteria Care for Concrete,” Materials Today, V. 14, No. 9, 2011, p. 444 doi: 10.1016/S1369-7021(11)70193-6

5. Siddique, R., and Chahal, N. K., “Effect of Ureolytic Bacteria on Concrete Properties,” Construction and Building Materials, V. 25, No. 10, 2011, pp. 3791-3801. doi: 10.1016/j.conbuildmat.2011.04.010

6. Seifan, M.; Samani, A. K.; and Berenjian, A., “Bioconcrete: Next Generation of Self-Healing Concrete,” Applied Microbiology and Biotechnology, V. 100, No. 6, 2016, pp. 2591-2602. doi: 10.1007/s00253-016-7316-z

7. Mondal, S., and Ghosh, A. D., “Review on Microbial Induced Calcite Precipitation Mechanisms Leading to Bacterial Selection for Microbial Concrete,” Construction and Building Materials, V. 225, 2019, pp. 67-75. doi: 10.1016/j.conbuildmat.2019.07.122

8. Ramakrishnan, V.; Panachalan, R. K.; and Bang, S. S., “Improvement of Concrete Durability by Bacterial Mineral Precipitation,” Proceedings of 11th International Conference on Fracture, Turin, Italy, 2001.

9. Ramachandran, S. K.; Ramakrishnan, V.; and Bang, S. S., “Remediation of Concrete Using Micro-Organisms,” ACI Materials Journal, V. 98, No. 1, Jan.-Feb. 2001, pp. 3-9.

10. Ghosh, P.; Mandal, S.; Chattopadhyay, B. D.; and Pal, S., “Use of Microorganism to Improve the Strength of Cement Mortar,” Cement and Concrete Research, V. 35, No. 10, 2005, pp. 1980-1983. doi: 10.1016/j.cemconres.2005.03.005

11. Tayebani, B., and Mostofinejad, D., “Self-Healing Bacterial Mortar with Improved Chloride Permeability and Electrical Resistance,” Construction and Building Materials, V. 208, 2019, pp. 75-86. doi: 10.1016/j.conbuildmat.2019.02.172

12. Parastegari, N.; Mostofinejad, D.; and Poursina, D., “Use of Bacteria to Improve Electrical Resistivity and Chloride Penetration of Air-Entrained Concrete,” Construction and Building Materials, V. 210, 2019, pp. 588-595. doi: 10.1016/j.conbuildmat.2019.03.150

13. Mostofinejad, D.; Nosouhian, F.; and Tayebani, B., “Evaluation of Mechanical Properties of Bacteria-Containing Mortar in Seawater Environment,” ACI Materials Journal, V. 118, No. 5, Sept. 2021, pp. 35-43.

14. Karimi, N., and Mostofinejad, D., “Bacillus Subtilis Bacteria Used in Fiber Reinforced Concrete and their Effects on Concrete Penetrability,” Construction and Building Materials, V. 230, 2020, p. 117051. doi: 10.1016/j.conbuildmat.2019.117051

15. Stocks-Fischer, S.; Galinat, J. K.; and Bang, S. S., “Microbiological Precipitation of CaCO3,” Soil Biology & Biochemistry, V. 31, No. 11, 1999, pp. 1563-1571. doi: 10.1016/S0038-0717(99)00082-6

16. Hammes, F., and Verstraete, W., “Key Roles of pH and Calcium Metabolism in Microbial Carbonate Precipitation,” Reviews in Environmental Science and Biotechnology, V. 1, No. 1, 2002, pp. 3-7. doi: 10.1023/A:1015135629155

17. Kim, H. K.; Park, S. J.; Han, J. I.; and Lee, H. K., “Microbially Mediated Calcium Carbonate Precipitation on Normal and Lightweight Concrete,” Construction and Building Materials, V. 38, 2013, pp. 1073-1082. doi: 10.1016/j.conbuildmat.2012.07.040

18. Kalhori, H., and Bagherpour, R., “Application of Carbonate Precipitating Bacteria for Improving Properties and Repairing Cracks of Shotcrete,” Construction and Building Materials, V. 148, 2017, pp. 249-260. doi: 10.1016/j.conbuildmat.2017.05.074

19. Erşan, Y. Ç.; Van Tittelboom, K.; Boon, N.; and De Belie, N., “Nitrite Producing Bacteria Inhibit Reinforcement Bar Corrosion in Cementitious Materials,” Scientific Reports, V. 8, No. 1, 2018, pp. 1-10. doi: 10.1038/s41598-018-32463-6

20. Erşan, Y. Ç.; Hernandez-Sanabria, E.; Boon, N.; and De Belie, N., “Enhanced Crack Closure Performance of Microbial Mortar through Nitrate Reduction,” Cement and Concrete Composites, V. 70, 2016, pp. 159-170. doi: 10.1016/j.cemconcomp.2016.04.001

21. Siddique, R.; Jameel, A.; Singh, M.; Barnat-Hunek, D.; Kunal; Aït-Mokhtar, A.; Belarbi, R.; and Rajor, A., “Effect of Bacteria on Strength, Permeation Characteristics and Micro-Structure of Silica Fume Concrete,” Construction and Building Materials, V. 142, 2017, pp. 92-100. doi: 10.1016/j.conbuildmat.2017.03.057

22. Chahal, N.; Siddique, R.; and Rajor, A., “Influence of Bacteria on the Compressive Strength, Water Absorption and Rapid Chloride Permeability of Fly Ash Concrete,” Construction and Building Materials, V. 28, No. 1, 2012, pp. 351-356. doi: 10.1016/j.conbuildmat.2011.07.042

23. Chahal, N.; Siddique, R.; and Rajor, A., “Influence of Bacteria on the Compressive Strength, Water Absorption and Rapid Chloride Permeability of Concrete Incorporating Silica Fume,” Construction and Building Materials, V. 37, 2012, pp. 645-651. doi: 10.1016/j.conbuildmat.2012.07.029

24. Chahal, N., and Siddique, R., “Permeation Properties of Concrete Made with Fly Ash and Silica Fume: Influence of Ureolytic Bacteria,” Construction and Building Materials, V. 49, 2013, pp. 161-174. doi: 10.1016/j.conbuildmat.2013.08.023

25. Siddique, R.; Singh, K.; Kunal; Singh, M.; Corinaldesi, V.; and Rajor, A., “Properties of Bacterial Rice Husk Ash Concrete,” Construction and Building Materials, V. 121, 2016, pp. 112-119. doi: 10.1016/j.conbuildmat.2016.05.146

26. Siddique, R.; Nanda, V.; Kunal; Kadri, E. H.; Khan, M. I.; Singh, M.; and Rajor, A., “Influence of Bacteria on Compressive Strength and Permeation Properties of Concrete Made with Cement Baghouse Filter Dust,” Construction and Building Materials, V. 106, 2016, pp. 461-469. doi: 10.1016/j.conbuildmat.2015.12.112

27. Mostofinejad, D.; Khademolmomenin, M.; and Tayebani, B., “Evaluating Durability Parameters of Concrete Containing Limestone Powder and Slag under Bacterial Remediation,” Journal of Building Engineering, V. 40, 2021, p. 102312. doi: 10.1016/j.jobe.2021.102312

28. Grabiec, A. M.; Klama, J.; Zawal, D.; and Krupa, D., “Modification of Recycled Concrete Aggregate by Calcium Carbonate Biodeposition,” Construction and Building Materials, V. 34, 2012, pp. 145-150. doi: 10.1016/j.conbuildmat.2012.02.027

29. Hosseini Balam, N.; Mostofinejad, D.; and Eftekhar, M., “Effects of Bacterial Remediation on Compressive Strength, Water Absorption, and Chloride Permeability of Lightweight Aggregate Concrete,” Construction and Building Materials, V. 145, 2017, pp. 107-116. doi: 10.1016/j.conbuildmat.2017.04.003

30. Hosseini Balam, N.; Tayebani, B.; and Mostofinejad, D., “Seawater Used as a Natural Medium for Curing Bacterially-Treated Concrete with Either Lightweight or Normal Weight Aggregates,” Journal of Materials in Civil Engineering, ASCE, V. 33, No. 9, 2021, p. 04021216 doi: 10.1061/(ASCE)MT.1943-5533.0003857

31. Salmasi, F., and Mostofinejad, D., “Investigating the Effects of Bacterial Activity on Compressive Strength and Durability of Natural Lightweight Aggregate Concrete Reinforced with Steel Fibers,” Construction and Building Materials, V. 251, 2020, p. 119032. doi: 10.1016/j.conbuildmat.2020.119032

32. Tayebani, B.; Hosseinibalam, N.; and Mostofinejad, D., “Influential Effect of Self-Healing Treatment on Water Absorption and Electrical Resistance of Normal and Light Weight Aggregate Concretes,” International Journal of Civil and Environmental Engineering, V. 13, No. 4, 2019, pp. 195-199.

33. Wang, J.; Vandevyvere, B.; Vanhessche, S.; Schoon, J.; Boon, N.; and De Belie, N., “Microbial Carbonate Precipitation for the Improvement of Quality of Recycled Aggregates,” Journal of Cleaner Production, V. 156, 2017, pp. 355-366. doi: 10.1016/j.jclepro.2017.04.051

34. Hosseini Balam, N.; Mostofinejad, D.; and Eftekhar, M., “Use of Carbonate Precipitating Bacteria to Reduce Water Absorption of Aggregates,” Construction and Building Materials, V. 141, 2017, pp. 565-577. doi: 10.1016/j.conbuildmat.2017.03.042

35. Jonkers, H.; Thijssen, A.; Muyzer, G.; Copuroglu, O.; and Schlangen, E., “Application of Bacteria as Self-Healing Agent for the Development of Sustainable Concrete,” Ecological Engineering, V. 36, No. 2, 2010, pp. 230-235. doi: 10.1016/j.ecoleng.2008.12.036

36. Wang, J. Y.; Snoeck, D.; Van Vlierberghe, S.; Verstraete, W.; and De Belie, N., “Application of Hydrogel Encapsulated Carbonate Precipitating Bacteria for Approaching a Realistic Self-Healing in Concrete,” Construction and Building Materials, V. 68, 2014, pp. 110-119. doi: 10.1016/j.conbuildmat.2014.06.018

37. Amidi, S., and Wang, J., “Surface Treatment of Concrete Bricks Using Calcium Carbonate Precipitation,” Construction and Building Materials, V. 80, 2015, pp. 273-278. doi: 10.1016/j.conbuildmat.2015.02.001

38. Parastegari, N.; Mostofinejad, D.; and Poursina, D., “An Investigation on Bacterial Air-Entrained Concrete Permeability using Statistical Modeling,” Advances in Civil Engineering Materials, V. 11, No. 1, 2022, p. 20210010. doi: 10.1520/ACEM20210010

39. Nosouhian, F.; Mostofinejad, D.; and Hasheminejad, H., “Influence of Biodeposition Treatment on Concrete Durability in a Sulphate Environment,” Biosystems Engineering, V. 133, 2015, pp. 141-152. doi: 10.1016/j.biosystemseng.2015.03.008

40. Nosouhian, F.; Mostofinejad, D.; and Hasheminejad, H., “Concrete Durability Improvement in a Sulfate Environment Using Bacteria,” Journal of Materials in Civil Engineering, ASCE, V. 28, No. 1, 2016, p. 04015064 doi: 10.1061/(ASCE)MT.1943-5533.0001337

41. Nosouhian, F., and Mostofinejad, D., “Reducing Permeability of Concrete by Bacterial Mediation on Surface Using Treatment Gel,” ACI Materials Journal, V. 113, No. 3, May-June 2016, pp. 287-293. doi: 10.14359/51688701

42. Tayebani, B., and Mostofinejad, D., “Penetrability, Corrosion Potential, and Electrical Resistivity of Bacterial Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 31, No. 3, 2019, p. 04019002. doi: 10.1061/(ASCE)MT.1943-5533.0002618

43. Persian Type Culture Collection, Tehran, Iran, http://ptcc.irost.org/. (last accessed Nov. 1, 2022)

44. Murahari, K., and Rao, R., “Effects of Polypropylene Fibres on the Strength Properties of Fly Ash Based Concrete,” International Journal of Engineering Science Invention, V. 2, No. 5, 2013, pp. 13-19.

45. Nili, M., and Afroughsabet, V., “Combined Effect of Silica Fume and Steel Fibers on the Impact Resistance and Mechanical Properties of Concrete,” International Journal of Impact Engineering, V. 37, No. 8, 2010, pp. 879-886. doi: 10.1016/j.ijimpeng.2010.03.004

46. ASTM C33/C33M-13, “Standard Specification for Concrete Aggregates,” ASTM International, West Conshohocken, PA, 2013.

47. ACI Committee 211, “Standard Practice for Selecting Proportions for Normal, Heavyweight and Mass Concrete (ACI 211.2-98) (Reapproved 2004),” American Concrete Institute, Farmington Hills, MI, 2002, 20 pp.

48. ASTM C39/C39M-14, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2014.

49. ASTM C642-13, “Standard Test Method for Density, Absorption, and Voids in Hardened Concrete,” ASTM International, West Conshohocken, PA, 2013.

50. ASTM C1760-12, “Standard Test Method for Bulk Electrical Conductivity of Hardened Concrete,” ASTM International, West Conshohocken, PA, 2012.

51. Afroughsabet, V., and Ozbakkaloglu, T., “Mechanical and Durability Properties of High-Strength Concrete Containing Steel and Polypropylene Fibers,” Construction and Building Materials, V. 94, 2015, pp. 73-82. doi: 10.1016/j.conbuildmat.2015.06.051

52. Mondal, S., and Ghosh, A. D., “Spore-Forming Bacillus subtilis Vis-à-Vis Non-Spore-Forming Deinococcus radiodurans, A Novel Bacterium for Self-Healing of Concrete Structures: A Comparative Study,” Construction and Building Materials, V. 266, 2021, p. 121122. doi: 10.1016/j.conbuildmat.2020.121122

53. Monfore, G. E., “The Electrical Resistivity of Concrete,” Portland Cement Association, Research and Development Laboratories, Skokie, IL, 1968.


ALSO AVAILABLE IN:

Electronic Materials Journal