Multi-Laboratory Validation Study of Critical Chloride Threshold Test Method

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Multi-Laboratory Validation Study of Critical Chloride Threshold Test Method

Author(s): Goran Adil, Ceki Halmen, Pavan Vaddey, Jose Pacheco, David Trejo

Publication: Materials Journal

Volume: 119

Issue: 6

Appears on pages(s): 91-100

Keywords: chloride; corrosion; critical chloride threshold; service life prediction; standard test method; threshold

DOI: 10.14359/51737195

Date: 11/1/2022

Abstract:
The critical chloride threshold, Ccrit/, is a value of a reinforced concrete system and the critical parameter that is used to define the initiation of reinforcement corrosion and is used for service life predictions. The published Ccrit/ data in the literature shows significant variability due to the lack of a standardized laboratory test that can consistently be used by the industry and researchers. This paper reports data from a multi-laboratory validation study of a novel Ccrit/ test method, developed based on a framework established by ACI Committee 222. The study was conducted using the same set of materials in three different laboratories, and its repeatability and reproducibility were evaluated. Results indicated that the mean Ccrit/ values were not statistically significantly different. Exhibiting good repeatability and reproducibility, this test method should be further evaluated to be implemented as a standard laboratory Ccrit/ test method.

Related References:

1. Elsener, B., “Macrocell Corrosion of Steel in Concrete–Implications for Corrosion Monitoring,” Cement and Concrete Composites, V. 24, No. 1, 2002, pp. 65-72. doi: 10.1016/S0958-9465(01)00027-0

2. Bertolini, L.; Elsener, B.; Pedeferri, P.; Redaelli, E.; and Polder, R., Corrosion of Steel in Concrete: Prevention, Diagnosis, Repair, Wiley‐VCH Verlag GmbH & Co. KGaA, Weinheim, Germany, V. 392, 2013.

3. Angst, U.; Elsener, B.; Larsen, C. K.; and Vennesland, Ø., “Critical Chloride Content in Reinforced Concrete—A Review,” Cement and Concrete Research, V. 39, No. 12, 2009, pp. 1122-1138. doi: 10.1016/j.cemconres.2009.08.006

4. Poulsen, E., and Mejlbro, L., Diffusion of Chloride in Concrete: Theory and Application, CRC Press, Boca Raton, FL, 2010.

5. Stanish, K. D.; Hooton, R. D.; Thomas, M. D. A., “Testing the Chloride Penetration Resistance of Concrete: A Literature Review,” technical report, Federal Highway Administration, Washington, DC, 2001.

6. Broomfield, J. P., Corrosion of Steel in Concrete: Understanding Investigation and Repair, E&FN Spon, London, UK, 1997, pp. 1-15.

7. Halmen, C., and Trejo, D., “Accelerating Standard Test Method for Assessing Corrosion of Steel in Concrete,” ACI Materials Journal, V. 109, No. 4, July-Aug. 2012, pp. 421-430.

8. Trejo, D., and Pillai, R.G., “Accelerated Chloride Threshold Testing: Part I—ASTM A615 And A706 Reinforcement,” ACI Materials Journal, V. 100, No. 6, Nov.-Dec. 2003, pp. 519-527.

9. Tang, L.; Frederiksen, J. M.; Angst, U. M.; Polder, R.; Alonso, M. C.; Elsener, B.; Hooton, D.; and Pacheco, J., “Experiences from RILEM TC 235-CTC in Recommending a Test Method for Chloride Threshold Values in Concrete,” RILEM Technical Letters, V. 3, 2018, pp. 25-31. doi: 10.21809/rilemtechlett.2018.55

10. Foulkes, F. R., and McGrath, P., “A Rapid Cyclic Voltammetric Method for Studying Cement Factors Affecting the Corrosion of Reinforced Concrete,” Cement and Concrete Research, V. 29, No. 6, 1999, pp. 873-883. doi: 10.1016/S0008-8846(99)00056-3

11. Goñi, S., and Andrade, C., “Synthetic Concrete Pore Solution Chemistry and Rebar Corrosion Rate in the Presence of Chlorides,” Cement and Concrete Research, V. 20, No. 4, 1990, pp. 525-539. doi: 10.1016/0008-8846(90)90097-H

12. Moreno, M.; Morris, W.; Alvarez, M. G.; and Duffo, G. S., “Corrosion of Reinforcing Steel in Simulated Concrete Pore Solutions: Effect of Carbonation and Chloride Content,” Corrosion Science, V. 46, No. 11, 2004, pp. 2681-2699. doi: 10.1016/j.corsci.2004.03.013

13. Flis, J., and Zakroczymski, T., “Impedance Study of Reinforcing Steel in Simulated Pore Solution with Tannin,” Journal of the Electrochemical Society, V. 143, No. 8, 1996, pp. 2458-2464. doi: 10.1149/1.1837031

14. Yuan, Y.; Ji, Y.; and Shah, S. P., “Comparison of Two Accelerated Corrosion Techniques for Concrete Structures,” ACI Structural Journal, V. 104, No. 3, May-June 2007, pp. 344-347.

15. Almusallam, A. A., “Effect of Degree of Corrosion on the Properties of Reinforcing Steel Bars,” Construction and Building Materials, V. 15, No. 8, 2001, pp. 361-368. doi: 10.1016/S0950-0618(01)00009-5

16. El Maaddawy, A. T., and Soudki, K. A., “Effectiveness of Impressed Current Technique to Simulate Corrosion of Steel Reinforcement in Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 15, No. 1, 2003, pp. 41-47. doi: 10.1061/(ASCE)0899-1561(2003)15:1(41)

17. Poursaee, A., and Hansson, C. M., “Potential Pitfalls in Assessing Chloride-Induced Corrosion of Steel in Concrete,” Cement and Concrete Research, V. 39, No. 5, 2009, pp. 391-400. doi: 10.1016/j.cemconres.2009.01.015

18. Angst, U. M., and Polder, R., “Spatial Variability of Chloride in Concrete within Homogeneously Exposed Areas,” Cement and Concrete Research, V. 56, 2014, pp. 40-51. doi: 10.1016/j.cemconres.2013.10.010

19. Warkus, J., and Raupach, M., “Modelling of Reinforcement Corrosion–Geometrical Effects on Macrocell Corrosion,” Materials and Corrosion, V. 61, No. 6, 2010, pp. 494-504.

20. Chalhoub, C.; Francois, R.; and Carcasses, M., “Determination of Chloride Threshold Initiating Corrosion: A New Set-Up Taking the Localized Aspect of Corrosion Into Account,” Cement and Concrete Research, V. 124, 2019, p. 105825. doi: 10.1016/j.cemconres.2019.105825

21. Mammoliti, L. T.; Brown, L. C.; Hansson, C. M.; and Hope, B. B., “The Influence of Surface Finish of Reinforcing Steel and PH of the Test Solution on the Chloride Threshold Concentration for Corrosion Initiation in Synthetic Pore Solutions,” Cement and Concrete Research, V. 26, No. 4, 1996, pp. 545-550. doi: 10.1016/0008-8846(96)00018-X

22. Mohammed, T. U., and Hamada, H., “Corrosion of Steel Bars in Concrete with Various Steel Surface Conditions,” ACI Materials Journal, V. 103, No. 4, July-Aug. 2006, pp. 233-242.

23. Halmen, C., and Adil, G., “A Collaborative Study for the Development of A Standard Critical Chloride Threshold Test Method,” technical report, 2021.

24. Kahrs, J. T.; Darwin, D.; and Locke, C. E., “Evaluation of Corrosion Resistance of Type 304 Stainless Steel-Clad Reinforcing Bars,” SM Report No. 65, The University of Kansas Center for Research, Inc., Lawrence, KS, 2001.

25. Trejo, D.; Vaddey, N. P.; and Halmen, C., “Standardizing Test to Quantify Chloride Threshold of Steel in Concrete,” ACI Materials Journal, V. 118, No. 1, Jan. 2021, pp. 177-187.

26. ASTM C1152/C1152M-20, “Standard Test Method for Acid-Soluble Chloride in Mortar and Concrete,” ASTM International, West Conshohocken, PA, 2020.

27. ASTM A615/A615M-20, “Standard Specification for Deformed and Plain Carbon-Steel Bars for Concrete Reinforcement,” ASTM International, West Conshohocken, PA, 2020.

28. Varner, R. L., “Influences of Cement Source and Sample of Cement Source on Compressive Strength Variability of Gravel Aggregate Concrete,” Report No. FHWA/MS-DOT-RD-13-239, Mississippi Department of Transportation, Jackson, MS, 2013.

29. ASTM C778-17, “Standard Specification for Standard Sand,” ASTM International, West Conshohocken, PA, 2017.

30. ASTM C1437-20, “Standard Test Method for Flow of Hydraulic Cement Mortar,” ASTM International, West Conshohocken, PA, 2020.

31. ASTM C109/C109M-21, “Standard Test Method for Compressive Strength of Hydraulic Cement Mortars (Using 2-in. or [50 mm] Cube Specimens),” ASTM International, West Conshohocken, PA, 2021.

32. Sagüés, A. A.; Moreno, E. I.; and Andrade, C., “Evolution of pH During In-Situ Leaching in Small Concrete Cavities,” Cement and Concrete Research, V. 27, No. 11, 1997, pp. 1747-1759. doi: 10.1016/S0008-8846(97)00177-4

33. ASTM C1760-12, “Standard Test Method for Bulk Electrical Conductivity of Hardened Concrete (Withdrawn 2021),” ASTM International, West Conshohocken, PA, 2012.

34. AASHTO T 358, “Standard Method of Test for Surface Resistivity Indication of Concrete’s Ability to Resist Chloride Ion Penetration,” American Association of State Highway and Transportation Officials, Washington, DC, 2019.

35. Gudimettla, J., and Crawford, G., “Resistivity Tests for Concrete—Recent Field Experience,” ACI Materials Journal, V. 113, No. 4, July-Aug. 2016, pp. 505-512.

36. Lock, R. H.; Lock, P. F.; Morgan, K. L.; Lock, E. F.; and Lock, D. F., Statistics: Unlocking the Power of Data, John Wiley & Sons, New York, 2020.

37. ASTM C670-03, “Standard Practice for Preparing Precision and Bias Statements for Test Methods for Construction Materials,” ASTM International, West Conshohocken, PA, 2003.

38. ASTM C802-96(2002), “Standard Practice for Conducting an Interlaboratory Test Program to Determine the Precision of Test Methods for Construction Materials,” ASTM International, West Conshohocken, PA, 2002.


ALSO AVAILABLE IN:

Electronic Materials Journal