Experimental Study on Activation Energy of Typical Hydraulic Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Study on Activation Energy of Typical Hydraulic Concrete

Author(s): Yaoying Huang, Yong Zhou, Shifa Xia, Xiaofeng Xu

Publication: Materials Journal

Volume: 119

Issue: 6

Appears on pages(s): 35-42

Keywords: activation energy model; curing temperature; fly ash content; hydraulic concrete; Kim’s method

DOI: 10.14359/51737194

Date: 11/1/2022

Abstract:
Existing methods to determine the activation energy of hydraulic concrete generally assume that it is constant, thereby neglecting the fact that it depends on curing temperature and fly ash content. To clarify this issue, this study experimentally investigates the activation energy of typical hydraulic concrete at different curing temperatures (5, 20, and 40°C) and fly ash contents (0, 15, and 35%) and obtains the activation energy of typical hydraulic concrete through a modified optimization algorithm based on Kim’s method. By analyzing the activation energy as a function of either curing temperature or fly ash content, a comprehensive model is developed to accurately predict the activation energy of typical hydraulic concrete for different curing temperatures and fly ash contents. The experiments reveal that the ratio of the hydraulic-concrete activation energy to the gas constant at 5, 20, and 40°C is 4764 to 5251, 4309 to 4874, and 3897 to 4575 K when the fly ash content is 0%, 15%, and 35%, respectively. For a given fly ash content, the hydraulic-concrete activation energy increases as a power law in temperature and, at a given temperature, it decreases quadratically with increasing fly ash content. The results of the proposed model of the activation energy of typical hydraulic concrete are consistent with the experimental results for different curing temperatures and fly ash contents.

Related References:

ASTM C1074-98, 1998, “Standard Practice for Estimating Concrete Strength by the Maturity Method,” ASTM International, West Conshohocken, PA, 8 pp.

ASTM C1074-04, 2004, “Standard Practice for Estimating Concrete Strength by the Maturity Method,” ASTM International, West Conshohocken, PA, 9 pp.

ASTM C1074-11, 2011, “Standard Practice for Estimating Concrete Strength by the Maturity Method,” ASTM International, West Conshohocken, PA, 10 pp.

Bažant, Z. P., and Jirásek, M., 2018, Creep and Hygrothermal Effects in Concrete Structures, Springer, Dordrecht, the Netherlands, 918 pp.

Bentz, D. P., 2014, “Activation Energies of High-Volume Fly Ash Ternary Blends: Hydration and Setting,” Cement and Concrete Composites, V. 53, Oct., pp. 214-223. doi: 10.1016/j.cemconcomp.2014.06.018

Carino, N. J., 1984, “The Maturity Method: Theory and Application,” Cement, Concrete and Aggregates, V. 6, No. 2, pp. 61-73. doi: 10.1520/CCA10358J

Carino, N. J., and Tank, R. C., 1992, “Maturity Functions for Concretes Made with Various Cements and Admixtures,” ACI Materials Journal, V. 89, No. 2, Mar.-Apr., pp. 188-196.

Chengju, G., 1989, “Maturity of Concrete: Method for Predicting Early-Stage Strength,” ACI Materials Journal, V. 86, No. 4, July-Aug., pp. 341-353.

Ezziane, K.; Kadri, E. H.; Hallal, A.; and Duval, R., 2010, “Effect of Mineral Additives on the Setting of Blended Cement by the Maturity Method,” Materials and Structures, V. 43, No. 3, Apr., pp. 393-401. doi: 10.1617/s11527-009-9498-7

Han, S.-H.; Kim, J.-K.; and Park, Y.-D., 2003, “Prediction of Compressive Strength of Fly Ash Concrete by New Apparent Activation Energy Function,” Cement and Concrete Research, V. 33, No. 7, July, pp. 965-971. doi: 10.1016/S0008-8846(03)00007-3

Hansen, P. F., and Pedersen, E. J., 1977, “Maturity Computer for Controlled Curing and Hardening of Concrete,” Nordisk Betong, V. 1, No. 19, pp. 19-34.

Havin, V. P., and Nikol’skij, N. K., 1995, “Complex Methods,” Commutative Harmonic Analysis III: Generalized Functions. Application, V. P. Havin and N. K. Nikol’skij, eds., Springer, Berlin, Germany, pp. 207-252.

Huang, Y.; Zhou, Y.; Liu, Y.; and Xiao, L., 2020, “Tensile Creep Tests of Hydraulic Concrete under Different Curing Conditions,” Journal of Materials in Civil Engineering, ASCE, V. 32, No. 4, Apr., p. 05020004. doi: 10.1061/(ASCE)MT.1943-5533.0003090

JGJ 63-2006, 2006, “Standard of Water for Concrete,” Ministry of Housing and Urban-Rural Development, Beijing, China.

JGJ/T 104-2011, 2011, “Specification for Winter Construction of Building Engineering,” Ministry of Housing and Urban-Rural Development, Beijing, China.

Kada-Benameur, H.; Wirquin, E.; and Duthoit, B., 2000, “Determination of Apparent Activation Energy of Concrete by Isothermal Calorimetry,” Cement and Concrete Research, V. 30, No. 2, Feb., pp. 301-305. doi: 10.1016/S0008-8846(99)00250-1

Kang, S.-T.; Kim, J.-S.; Lee, Y.; Park, Y.-D.; and Kim, J.-K., 2012, “Moisture Diffusivity of Early Age Concrete Considering Temperature and Porosity,” KSCE Journal of Civil Engineering, V. 16, No. 1, Jan., pp. 179-188. doi: 10.1007/s12205-012-1445-4

Kim, J. K.; Han, S. H.; and Lee, K. M., 2001, “Estimation of Compressive Strength by a New Apparent Activation Energy Function,” Cement and Concrete Research, V. 31, No. 2, Feb., pp. 217-225. doi: 10.1016/S0008-8846(00)00481-6

Knudsen, T., 1984, “The Dispersion Model for Hydration of Portland Cement I. General Concepts,” Cement and Concrete Research, V. 14, No. 5, Sept., pp. 622-630. doi: 10.1016/0008-8846(84)90024-3

Lachemi, M.; Hossain, K. M. A.; Anagnostopoulos, C.; and Sabouni, A. R., 2010, “Laboratory and Field Performance of Maturity Functions,” Proceedings of the Institution of Civil Engineers - Construction Materials, V. 163, No. 4, Nov., pp. 211-221. doi: 10.1680/coma.800065

Lee, C. H., and Hover, K. C., 2016, “Compatible Datum Temperature and Activation Energy for Concrete Maturity,” ACI Materials Journal, V. 113, No. 2, Mar.-Apr., pp. 197-206. doi: 10.14359/51688639

Li, X. F.; Wang, H. L.; and Diao, B., 2018, “Prediction of Frost-Resisting Critical Strength of Plateau Concrete Based on Measured Apparent Activation Energy,” Transations of the Chinese Society of Agricultural Engineering, V. 34, No. 8, pp. 117-123. doi: 10.11975/j.issn.1002-6819.2018.08.015

Nokken, M. R., 2016, “Electrical Conductivity to Determine Maturity and Activation Energy in Concretes,” Materials and Structures, V. 49, No. 6, June, pp. 2209-2221. doi: 10.1617/s11527-015-0644-0

Poole, J. L.; Riding, K. A.; Juenger, M. C. G.; Folliard, K.; and Schindler, A., 2010, “Effects of Supplementary Cementitious Materials on Apparent Activation Energy,” Journal of ASTM International, V. 7, No. 9, pp. 1-16. doi: 10.1520/JAI102906

Radlinski, M.; Olek, J.; and Nantung, T., 2010, “Development and Application of Maturity Method for Prediction of Concrete’s Resistance to Chloride Ion Penetration,” Transportation Research Record: Journal of the Transportation Research Board, V. 2164, No. 1, Jan., pp. 105-112. doi: 10.3141/2164-14

Saadoon, T.; Gómez-Meijide, B.; and Garcia, A., 2019, “New Predictive Methodology for the Apparent Activation Energy and Strength of Conventional and Rapid Hardening Concretes,” Cement and Concrete Research, V. 115, Jan., pp. 264-273. doi: 10.1016/j.cemconres.2018.10.020

SL 352-2006, 2006, “Test Code for Hydraulic Concrete,” Ministry of Water Resources and Hydropower Planning and Design, Beijing, China.

Soutsos, M., and Kanavaris, F., 2018, “The Modified Nurse-Saul (MNS) Maturity Function for Improved Strength Estimates at Elevated Curing Temperatures,” Case Studies in Construction Materials, V. 9, Dec., Article No. e00206, 14 pp. doi: 10.1016/j.cscm.2018.e00206

Soutsos, M.; Hatzitheodorou, A.; Kanavaris, F.; and Kwasny, J., 2017, “Effect of Temperature on the Strength Development of Mortar Mixes with GGBS and Fly Ash,” Magazine of Concrete Research, V. 69, No. 15, Aug., pp. 787-801. doi: 10.1680/jmacr.16.00268

Tank, R. C., and Carino, N. J., 1991, “Rate Constant Functions for Strength Development of Concrete,” ACI Materials Journal, V. 88, No. 1, Jan.-Feb., pp. 74-83.

Wang, J.; Yan, P.; and Yu, H., 2007, “Apparent Activation Energy of Concrete in Early Age Determined by Adiabatic Test,” Journal of Wuhan University of Technology-Materials Science Edition, V. 22, No. 3, Sept., pp. 537-541. doi: 10.1007/s11595-006-3537-9

Xu, Y.; Zhang, X.; Liao, X.; and Zhou, Y., 2013, “Determination of Apparent Activation Energy of Concrete by TMC and Mathematical Means,” Journal of Materials in Civil Engineering, ASCE, V. 25, No. 2, Feb., pp. 289-295. doi: 10.1061/(ASCE)MT.1943-5533.0000591

Yang, H.-M.; Kwon, S.-J.; Myung, N. V.; Singh, J. K.; Lee, H.-S.; and Mandal, S., 2020, “Evaluation of Strength Development in Concrete with Ground Granulated Blast Furnace Slag Using Apparent Activation Energy,” Materials, V. 13, No. 2, Jan., Article No. 442, 14 pp. doi: 10.3390/ma13020442

Zhang, Z. M.; Feng, S. R.; Shi, Q. C.; and Wang, J. H., 2004, “Adiabatic Temperature Rise of Concrete Based on Equivalent Time,” Journal of Hohai University, V. 32, No. 5, pp. 573-577.

Zhang, Z. M.; Song, Z. T.; and Huang, H. Y., 2002, “New Theory on Adiabatic Temperature Rise and Heat Conduction Equation of Concrete,” Journal of Hohai University, V. 30, No. 3, pp. 1-6.

Zhang, Z. M.; Zhou, H. J.; and Yin, B., 2005, “Equivalent Time-Based Concrete Creep,” Journal of Hohai University, V. 33, No. 2, pp. 173-176.

Zhu, B., 2012, Thermal Stresses and Temperature Control of Mass Concrete, China Electric Power Press Co., Ltd., Beijing, China, 518 pp.

Zhu, X.; Cai, Y.; Ding, J.; Fu, Q.; and Bai, Y., 2017, “Study on the Effect of Admixtures on the Activation Energy of Abrasion-Resistant Concrete,” Concrete, No. 9, pp. 69-72. doi: 10.3969/j.issn.1002-3550.2017.09.018


ALSO AVAILABLE IN:

Electronic Materials Journal