Penetrating Sealer Effects on Durability Performance of Concrete Joints

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Penetrating Sealer Effects on Durability Performance of Concrete Joints

Author(s): Goran Adil, Seyedhamed Sadati, Yifeng Ling, Peter Taylor, Kejin Wang, John T. Kevern

Publication: Materials Journal

Volume: 119

Issue: 6

Appears on pages(s): 43-52

Keywords: absorption; deterioration; freezing and thawing; hydrophobicity; oxychloride; saturation; scaling; wettability.

DOI: 10.14359/51737184

Date: 11/1/2022

Abstract:
Penetrating sealers are one means to reduce moisture and chemical transport into concrete. However, a large variety of products are available, possessing different functional modes of action. This study investigated representative families of penetrating sealers applied to vertical, sawn faces of properly air-entrained concrete (approximately 6%) to represent field application of sealers to concrete joints. Concrete was characterized for water transport, chloride diffusion, gas permeability, frost resistance in the presence of deicing salts, and potential for oxychloride formation. The results showed that some sealers effectively reduced water absorption, prolonged time to saturation, and reduced chloride penetration. However, delayed time to critical saturation did not always result in improved frost resistance. All sealers significantly reduced the potential of oxychloride formation. The tests used for this study are broadly applicable and provide enhanced characterization for selection and application of new types of sealers and modes of action.

Related References:

1. Arribas-Colón, M. M.; Radliński, M.; Olek, J.; and Whiting, N., “Investigation of Premature Distress around Joints in PCC Pavements: Parts I & II,” Report FHWA/IN/JTRP-2012/25 and FHWA/IN/JTRP-2012/26, Joint Transportation Research Program, Indiana Department of Transportation and Purdue University, West Lafayette, IN, 2012. doi: 10.5703/128828431501910.5703/1288284315019

2. Sutter, L.; Van Dam, T.; Peterson, K. R.; and Johnston, D. P., “Long-Term Effects of Magnesium Chloride and Other Concentrated Salt Solutions on Pavement and Structural Portland Cement Concrete,” Transportation Research Record: Journal of the Transportation Research Board, V. 1979, No. 1, 2006, pp. 60-68. doi: 10.1177/0361198106197900109

3. Panchmatia, P.; Olek, J.; and Whiting, N., “Joint Deterioration in Concrete Pavements,” 4th International Conference on the Durability of Concrete Structures, West Lafayette, IN, 2014, pp. 12-21.

4. de Vries, J., and Polder, R. B., “Hydrophobic Treatment of Concrete,” Construction and Building Materials, V. 11, No. 4, 1997, pp. 259-265. doi: 10.1016/S0950-0618(97)00046-9

5. Basheer, L., and Cleland, D. J., “Freeze–Thaw Resistance of Concretes Treated with Pore Liners,” Construction and Building Materials, V. 20, No. 10, 2006, pp. 990-998. doi: 10.1016/j.conbuildmat.2005.06.010

6. Freitag, S. A., and Bruce, S. M., “The Influence of Surface Treatments on the Service Lives of Concrete Bridges,” New Zealand Transport Agency, Wellington, New Zealand, 2010.

7. Vipulanandan, C.; Parihar, A.; and Issac, M., “Testing and Modeling Composite Coatings with Silanes for Protecting Reinforced Concrete in Saltwater Environment,” Journal of Materials in Civil Engineering, ASCE, V. 23, No. 12, 2011, pp. 1602-1608. doi: 10.1061/(ASCE)MT.1943-5533.0000330

8. Christodoulou, C.; Goodier, C. I.; Austin, S. A.; Webb, J.; and Glass, G. K., “Long-Term Performance of Surface Impregnation of Reinforced Concrete Structures with Silane,” Construction and Building Materials, V. 48, 2013, pp. 708-716. doi: 10.1016/j.conbuildmat.2013.07.038

9. Liu, Z., and Hansen, W., “Effect of Hydrophobic Surface Treatment on Freeze-Thaw Durability of Concrete,” Cement and Concrete Composites, V. 69, 2016, pp. 49-60. doi: 10.1016/j.cemconcomp.2016.03.001

10. Zhang, J.; Taylor, P. C.; and Shi, C., “Investigation of Approaches for Improving Interfacial Transition Zone-Related Freezing-and-Thawing Resistance in Concrete Pavements,” ACI Materials Journal, V. 112, No. 5, Sept.-Oct. 2015, pp. 613-617. doi: 10.14359/51687902

11. Maso, J. C., Interfacial Transition Zone in Concrete, CRC Press, Boca Raton, FL, 1996.

12. Cwirzen, A., and Penttala, V., “Aggregate–Cement Paste Transition Zone Properties Affecting the Salt–Frost Damage of High-Performance Concretes,” Cement and Concrete Research, V. 35, No. 4, 2005, pp. 671-679. doi: 10.1016/j.cemconres.2004.06.009

13. Fu, C.; Ling, Y.; and Wang, K., “An Innovation Study on Chloride and Oxygen Diffusions in Simulated Interfacial Transition Zone of Cementitious Material,” Cement and Concrete Composites, V. 110, 2020, p. 103585. doi: 10.1016/j.cemconcomp.2020.103585

14. Fagerlund, G., “The Critical Degree of Saturation Method of Assessing the Freeze/Thaw Resistance of Concrete,” Materiales de Construcción, V. 10, No. 4, 1977, pp. 217-229.

15. Fagerlund, G., “A Service Life Model for Internal Frost Damage in Concrete,” Report TVBM 3119, Lund University, Lund, Sweden, 2004.

16. Powers, T. C., “A Working Hypothesis for Further Studies of Frost Resistance of Concrete,” ACI Journal Proceedings, V. 41, No. 1, Feb. 1945, pp. 245-272.

17. Powers, T. C., and Helmuth, R. A., “Theory of Volume Changes in Hardened Portland-Cement Paste during Freezing,” Highway Research Board Proceedings, V. 32, 1953.

18. Powers, T. C., and Willis, T. F., “The Air Requirement of Frost Resistant Concrete,” Highway Research Board Proceedings, V. 29, 1950.

19. Valenza, J. J. II, and Scherer, G. W., “A Review of Salt Scaling: I. Phenomenology,” Cement and Concrete Research, V. 37, No. 7, 2007, pp. 1007-1021. doi: 10.1016/j.cemconres.2007.03.005

20. Valenza, J. J. II, and Scherer, G. W., “A Review of Salt Scaling: II. Mechanisms,” Cement and Concrete Research, V. 37, No. 7, 2007, pp. 1022-1034. doi: 10.1016/j.cemconres.2007.03.003

21. Sutter, L.; Peterson, K.; Julio-Betancourt, G.; Hooton, D.; Vam Dam, T.; and Smith, K., “The Deleterious Chemical Effects of Concentrated Deicing Solutions on Portland Cement Concrete,” Technical Report, Office of Research, South Dakota Department of Transportation, Pierre, SD, 2008.

22. Shi, X., and Fu, L., Sustainable Winter Road Operations, John Wiley & Sons, New York, 2018.

23. Farnam, Y.; Dick, S.; Wiese, A.; Davis, J.; Bentz, D.; and Weiss, J., “The Influence of Calcium Chloride Deicing Salt on Phase Changes and Damage Development in Cementitious Materials,” Cement and Concrete Composites, V. 64, 2015, pp. 1-15. doi: 10.1016/j.cemconcomp.2015.09.006

24. Wang, X.; Sadati, S.; Taylor, P.; Li, C.; Wang, X.; and Sha, A., “Material Characterization to Assess Effectiveness of Surface Treatment to Prevent Joint Deterioration from Oxychloride Formation Mechanism,” Cement and Concrete Composites, V. 104, 2019, p. 103394. doi: 10.1016/j.cemconcomp.2019.103394

25. Wiese, A.; Farnam, Y.; Jones, W. A.; Imbrock, P.; Tao, B.; and Weiss, W. J., “Evaluation of Sealers and Waterproofers for Extending the Life Cycle of Concrete,” Joint Transportation Research Program Publication No. FHWA/IN/JTRP-2015/17, Purdue University, West Lafayette, IN, 2015. doi: 10.5703/1288284316002

26. Pfeifer, D. W., and Scali, M. J., “Concrete Sealers for Protection of Bridge Structures,” NCHRP Report 244, 1981.

27. Pan, X.; Shi, Z.; Shi, C.; Ling, T.-C.; and Li, N., “A Review on Concrete Surface Treatment Part I: Types and Mechanisms,” Construction and Building Materials, V. 132, 2017, pp. 578-590. doi: 10.1016/j.conbuildmat.2016.12.025

28. Xiao, D. X.; Adil, G.; Kevern, J. T.; and Owusu-Ababio, S., “Field Performance of Concrete Pavement Joints Protected by Silane Sealer: Case Study,” Journal of Performance of Constructed Facilities, ASCE, V. 35, No. 6, 2021, p. 04021089.

29. Xiao, D. X.; Kevern, J. T.; Owusu-Ababio, S.; and Schmitt, R., “Evaluation of Penetrating Sealers Applied to Saw Cut Faces in Concrete Pavement Joints,” Report No. WHRP 0092-18-01, Wisconsin Department of Transportation, Madison, WI, 2020.

30. Dai, J.-G.; Akira, Y.; Wittmann, F. H.; Yokota, H.; and Zhang, P., “Water Repellent Surface Impregnation for Extension of Service Life of Reinforced Concrete Structures in Marine Environments: The Role of Cracks,” Cement and Concrete Composites, V. 32, No. 2, 2010, pp. 101-109. doi: 10.1016/j.cemconcomp.2009.11.001

31. Hazrati, K.; Abesque, C.; and Pigeon, M., “Efficiency of Sealers on the Scaling Resistance of Concrete in Presence of Deicing Salts,” RILEM Proceedings 30: Freeze-Thaw Durability of Concrete, 1997, pp. 165-196.

32. Al-Rashed, R., and Jabari, M., “Dual-Crystallization Waterproofing Technology for Topical Treatment of Concrete,” Case Studies in Construction Materials, V. 13, 2020, p. e00408. doi: 10.1016/j.cscm.2020.e00408

33. Ibrahim, M.; Al-Gahtani, A. S.; Maslehuddin, M.; and Dakhil, F. H., “Use of Surface Treatment Materials to Improve Concrete Durability,” Journal of Materials in Civil Engineering, ASCE, V. 11, No. 1, 1999, pp. 36-40. doi: 10.1061/(ASCE)0899-1561(1999)11:1(36)

34. Azarsa, P.; Gupta, R.; and Biparva, A., “Crystalline Waterproofing Admixtures Effects on Self-Healing and Permeability of Concrete,” Proceedings of the International Conference on New Horizons in Green Civil Engineering, University of Victoria, Victoria, BC, Canada, 2018, pp. 25-27.

35. Dang, Y.; Xie, N.; Kessel, A.; McVey, E.; Pace, A.; and Shi, X., “Accelerated Laboratory Evaluation of Surface Treatments for Protecting Concrete Bridge Decks from Salt Scaling,” Construction and Building Materials, V. 55, 2014, pp. 128-135. doi: 10.1016/j.conbuildmat.2014.01.014

36. Taylor, P.; Sutter, L.; and Weiss, J., “Investigation of Deterioration of Joints in Concrete Pavements,” InTrans Project 09-361, Institute for Transportation, Iowa State University, Ames, IA, 2012.

37. ASTM C150-05, “Standard Specification for Portland Cement,” ASTM International, West Conshohocken, PA, 2005.

38. ASTM C618-19, “Standard Specification for Coal Fly Ash and Raw or Calcined Natural Pozzolan for Use in Concrete,” ASTM International, West Conshohocken, PA, 2019.

39. ASTM C33/C33M-08, “Standard Specification for Concrete Aggregates,” ASTM International, West Conshohocken, PA, 2008.

40. AASHTO T 259, “Standard Method of Test for Resistance of Concrete to Chloride Ion Penetration,” American Association of State Highway and Transportation Officials, Washington, DC, 2002.

41. Ley, M. T.; Sudbrink, B.; Kotha, H.; Materer, N.; and Apblett, A., “Expected Life of Silane Water Repellant Treatments on Bridge Decks,” Research & Development Division, Oklahoma Department of Transportation, Oklahoma City, OK, 2012.

42. Schneider, C. A.; Rasband, W. S.; and Eliceiri, K. W., “NIH Image to ImageJ: 25 Years of Image Analysis,” Nature Methods, V. 9, No. 7, 2012, pp. 671-675. doi: 10.1038/nmeth.2089

43. Alexander, M. G.; Ballim, Y.; and Mackechnie, J. R., “Durability Index Testing Procedure Manual,” University of Cape Town, Cape Town, South Africa, 2009.

44. ASTM C1585-13, “Standard Test Method for Measurement of Rate of Absorption of Water by Hydraulic Cement Concretes,” ASTM International, West Conshohocken, PA, 2013.

45. ASTM C666/C666M-15, “Standard Test Method for Resistance of Concrete to Rapid Freezing and Thawing,” ASTM International, West Conshohocken, PA, 2015.

46. Taylor, P.; Sadati, S.; Wang, K.; Ling, Y.; Wang, X.; Sun, W.; Kevern, J. T.; and Ryazi, S., “Entrained Air-Void Systems for Durable Highway Concrete,” NCHRP Research Report 961, National Cooperative Highway Research Program, Washington, DC, 2021. doi: 10.17226/26071

47. AASHTO T 260, “Standard Method of Test for Sampling and Testing for Chloride Ion in Concrete and Concrete Raw Materials,” American Association of State Highway and Transportation Officials, Washington, DC, 2005.

48. ASTM C1152/C1152M-03, “Standard Test Method for Acid-Soluble Chloride in Mortar and Concrete,” ASTM International, West Conshohocken, PA, 2003.

49. AASHTO T 365, “Standard Method of Test for Quantifying Calcium Oxychloride Formation Potential of Cementitious Pastes Exposed to Deicing Salts,” American Association of State Highway and Transportation Officials, Washington, DC, 2017.

50. Ley, M. T.; Welchel, D.; Peery, J.; Khatibmasjedi, S.; and LeFlore, J., “Determining the Air-Void Distribution in Fresh Concrete with the Sequential Air Method,” Construction and Building Materials, V. 150, 2017, pp. 723-737. doi: 10.1016/j.conbuildmat.2017.06.037

51. Hall, C., “Water Movement in Porous Building Materials—I. Unsaturated Flow Theory and its Applications,” Building and Environment, V. 12, No. 2, 1977, pp. 117-125. doi: 10.1016/0360-1323(77)90040-3

52. Pigeon, M., Durability of Concrete in Cold Climates, CRC Press, Boca Raton, FL, 2014.

53. Powers, T. C., and Brownyard, T. L., “Studies of the Physical Properties of Hardened Portland Cement Paste,” ACI Journal Proceedings, V. 43, No. 9, Nov. 1946, pp. 101-132.

54. Poursaee, A.; Laurent, A.; and Hansson, C. M., “Corrosion of Steel Bars in OPC Mortar Exposed to NaCl, MgCl2 and CaCl2: Macro- and Micro-Cell Corrosion Perspective,” Cement and Concrete Research, V. 40, No. 3, 2010, pp. 426-430. doi: 10.1016/j.cemconres.2009.09.029

55. Setzer, M. J., “Micro-Ice-Lens Formation in Porous Solid,” Journal of Colloid and Interface Science, V. 243, No. 1, 2001, pp. 193-201. doi: 10.1006/jcis.2001.7828

56. ASTM C672/C672M-12, “Standard Test Method for Scaling Resistance of Concrete Surfaces Exposed to Deicing Chemicals,” ASTM International, West Conshohocken, PA, 2012.

57. Sayama, M.; Sayama, S.; Mitani, K.; Hu, L.; and Yoshitake, I., “Effect of Surface-Penetrants for Concrete under Freeze-Thaw Cycles,” Proceedings of International Structural Engineering and Construction, V. 7, No. 2, 2020. doi: 10.14455/ISEC.2020.7(2).MAT-03


ALSO AVAILABLE IN:

Electronic Materials Journal