Title: Immobilization of Bacterial Cells on Natural Mineral for Developing Self-Healing Cement-Based Mortars

Author(s): Ilgin Sandalci

Publication: Web Session

Volume: ws_S22_IlginSandalci.pdf

Issue:

Appears on pages(s):

Keywords:

DOI:

Date: 3/28/2022

Abstract:
The purpose of this session is to offer authors/speakers an open forum for presentation of recent technical information that does not fit into other sessions scheduled for this convention.