Title: ACI PRC-132.1-22: Responsibility for the Care of Test Specimens for Acceptance of Concrete—TechNote

Author(s): ACI Committee 132

Publication: Technical Documents

Volume:

Issue:

Appears on pages(s): 5

Keywords:

DOI:

Date: 7/1/2022

Abstract:
This TechNote discusses the implications of improper procedures for curing test specimens at the jobsite that result in strength test results that are not reliable for acceptance of concrete. Keywords: contractor; engineer of record (EOR); initial curing; responsibilities; test specimens; testing agency.