Title: A New Reinforcing Configuration for Achieving High-Ductility and High-Strength Rectangular Squat Structural Walls

Author(s): Ghassan Almasabha and Shih-Ho Chao

Publication: Structural Journal

Volume: 120

Issue: 1

Appears on pages(s): 253-268

Keywords: confinement; diagonal compression failure; ductility; post-earthquake functionality; squat walls; strut-and-tie model

DOI: 10.14359/51737144

Date: 1/1/2023

Abstract:
Reinforced concrete squat structural walls (SSWs) are a popular seismic force-resisting system used in low-rise buildings due to their high strength and stiffness. However, extensive studies have shown that rectangular SSWs have limited shear strength and drift ductility, primarily because their deterioration initiates from brittle compression failure of the diagonal concrete struts across the wall’s web. This research investigated a new reinforcing detail for SSWs to achieve substantially improved ductility and strength. While the current ACI Code requires a mesh of steel reinforcing bars to reinforce the SSW web, the new detail presented in this paper fortifies the SSW by multiple steel cages which contain vertical reinforcing bars enclosed by transverse hoops. These steel cages can be easily prefabricated at a shop to minimize on-site assembly work and time. Each steel cage is similar to that in well-confined columns, which increases concrete’s strength and ductility, therefore allowing a higher amount of vertical reinforcement for greater shear strength. Five specimens with an aspect ratio of 0.5 and reinforced according to either the ACI requirements or by the proposed details, and one specimen with an aspect ratio of 0.33 using the proposed details were tested. Similar to prior research results, SSWs using conventional details exhibited a fast strength deterioration at low drift ratios due to severe damage of the diagonal concrete struts under cyclic loading. Conversely, the proposed SSWs provide an increase of approximately 100% in the drift and ductility ratios, as well as a very gradual strength degradation and concrete damage progression. The proposed design allows SSWs to develop a ductile seismic behavior which is essential to safety against collapse, post-earthquake functionality and repairability, and seismic response predictability of structures. The enhanced ductility warrants a higher shear strength reduction factor, ϕ, of greater than 0.6 for SSWs as well as the diaphragms and foundations connected to them. In addition, a seismic response modification coefficient, R, of greater than 6 can be justified, which translates into a smaller seismic design base shear. These adjustments can ultimately lead to a more economical design of structures with SSWs.

Related References:

Almasabha, G. S., 2019, “A New Design Methodology of Reinforced Concrete Squat Shear Walls for Ductile Seismic Behavior and Predictable Shear Strength,” PhD dissertation, The University of Texas at Arlington, Arlington, TX, Aug., 430 pp.

ACI Committee 318, 2019, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 624 pp.

ASCE/SEI 7-22, 2022, “Minimum Design Loads and Associated Criteria for Buildings and Other Structures,” American Society of Civil Engineers, Reston, VA, 888 pp.

Baek, J.-W.; Park, H.-G.; Lee, B.-S.; and Shin, H.-M., 2018, “Shear-Friction Strength of Low-Rise Walls with 550 MPa (80 ksi) Reinforcing Bars under Cyclic Loading,” ACI Structural Journal, V. 115, No. 1, Jan., pp. 65-77. doi: 10.14359/51700915

Baek, J.-W.; Park, H.-G.; Lee, J.-H.; and Bang, C.-J., 2017, “Cyclic Loading Test for Walls of Aspect Ratio 1.0 and 0.5 with Grade 550 MPa (80 ksi) Shear Reinforcing Bars,” ACI Structural Journal, V. 114, No. 4, July-Aug., pp. 969-982. doi: 10.14359/51689680

Cardenas, A. E.; Russell, H. G.; and Corley, W. G., 1980,“Strength of Low-Rise Structural Walls,” Reinforced Concrete Structures Subjected to Wind and Earthquake Forces, SP-63, American Concrete Institute, Farmington Hills, MI, pp. 221-242.

Cheng, M.-Y.; Chou, Y.; and Wibowo, L. S. B., 2020, “Cyclic Response of Reinforced Concrete Squat Walls to Boundary Element Arrangement,” ACI Structural Journal, V. 117, No. 4, July, pp. 15-24.

Cheng, M.-Y.; Hung, S.-C.; Lequesne, R. D.; and Lepage, A., 2016, “Earthquake-Resistant Squat Walls Reinforced with High-Strength Steel,” ACI Structural Journal, V. 113, No. 5, Sept.-Oct., pp. 1065-1076. doi: 10.14359/51688825

Cheng, M.-Y.; Wibowo, L. S. B.; Giduquio, M. B.; and Lequesne, R. D., 2021, “Strength and Deformation of Reinforced Concrete Squat Walls with High-Strength Materials,” ACI Structural Journal, V. 118, No. 1, Jan., pp. 125-137.

Deger, Z. T., and Basdogan, C., 2019, “Empirical Expression for Deformation Capacity of Reinforced Concrete Structural Walls,” ACI Structural Journal, V. 116, No. 6, Nov., pp. 53-61. doi: 10.14359/51716806

Eberhard, M. O., and Meigs, B. E., 1995, “Earthquake-Resisting System Selection Statics for Reinforced Concrete Buildings,” Earthquake Spectra, V. 11, No. 1, pp. 19-36. doi: 10.1193/1.1585801

FEMA, 2020, “Short-Period Building Collapse Performance and Recommendations for Improving Seismic Design, Volume 1 – “Overarching Findings, Conclusions, and Recommendations,” Report No. FEMA P-2139-1, Federal Emergency Management Agency, Washington, DC.

Gebelein, J.; Barnard, M.; Burton, H.; Cochran, M.; Haselton, C.; McLellan, R.; and Porter, K., 2017, “Considerations for a Framework of Resilient Structural Design for Earthquakes,” SEAOC Convention Proceedings, pp. 1-16.

Gulec, C. K., and Whittaker, A. S., 2011, “Empirical Equations for Peak Shear Strength of Low Aspect Ratio Reinforced Concrete Walls,” ACI Structural Journal, V. 108, No. 1, Jan.-Feb., pp. 80-89.

Gulec, C. K.; Whittaker, A. S.; and Stojadinovic, B., 2008, “Shear Strength of Squat Rectangular Reinforced Concrete Walls,” ACI Structural Journal, V. 105, No. 4, July-Aug., pp. 488-497.

Hidalgo, P. A.; Ledezma, C. A.; and Jordan, R. M., 2002, “Seismic Behavior of Squat Reinforced Concrete Shear Walls,” Earthquake Spectra, V. 18, No. 2, pp. 287-308. doi: 10.1193/1.1490353

Kuang, J. S., and Ho, Y. B., 2008, “Seismic Behavior and Ductility of Squat Reinforced Concrete Shear Walls with Nonseismic Detailing,” ACI Structural Journal, V. 105, No. 2, Mar.-Apr., pp. 225-231.

Luna, B. N.; Rivera, J. P.; and Whittaker, A. S., 2015, “Seismic Behavior of Low-Aspect-Ratio Reinforced Concrete Shear Walls,” ACI Structural Journal, V. 112, No. 5, Sept.-Oct., pp. 593-603. doi: 10.14359/51687709

Mander, J. B.; Priestley, M. J. N.; and Park, R., 1988, “Observed Stress‐Strain Behavior of Confined Concrete,” Journal of Structural Engineering, ASCE, V. 114, No. 8, pp. 1827-1849. doi: 10.1061/(ASCE)0733-9445(1988)114:8(1827)

Moehle, J., 2015, Seismic Design of Reinforced Concrete Buildings, McGraw-Hill Education, 760 pp.

Park, H.-G.; Baek, J.-W.; Lee, J.-H.; and Shin, H.-M., 2015, “Cyclic Loading Tests for Shear Strength of Low-Rise Reinforced Concrete Walls with Grade 550 MPa Bars,” ACI Structural Journal, V. 112, No. 3, May-June, pp. 299-310. doi: 10.14359/51687406

Park, R., 1988, “Ductility Evaluation from Laboratory and Analytical Testing,” Proceedings of Ninth World Conference on Earthquake Engineering, V. VIII, pp. 605-616.

Paulay, T., and Priestley, M. J. N., 1992, Seismic Deign of Reinforced Concrete and Masonry Buildings. John Wiley & Sons, Inc., New York, 744 pp.

Paulay, T.; Priestley, M. J. N.; and Synge, A. J., 1982, “Ductility in Earthquake Resisting Squat Shearwalls,” ACI Journal Proceedings, V. 79, No. 4, July-Aug., pp. 257-269.

Priestley, M. J. N., and Park, R., 1987, “Strength and Ductility of Concrete Bridge Columns Under Seismic Loading,” ACI Structural Journal, V. 84, No. 1, Jan.-Feb., pp. 61-76.

Rasoolinejad, M., and Bažant, Z. P., 2019, “Size Effect of Squat Shear Walls Extrapolated by Microplane Model M7,” ACI Structural Journal, V. 116, No. 3, May, pp. 75-84. doi: 10.14359/51714478

Rivera, J. P. and Whittaker, A. S., 2019, “Damage and Peak Shear Strength of Low-Aspect-Ration Reinforced Concrete Shear Walls,” Journal of Structural Engineering, ASCE, V. 145, No. 11, pp. 04019141-1 -04019141-12.

Stevens, N. J.; Uzumeri, S. M.; and Collins, M. P., 1991, “Reinforced Concrete Subjected to Reversed Cyclic Shear—Experiments and Constitutive Model,” ACI Structural Journal, V. 88, No. 2, Mar.-Apr., pp. 135-146.

Terzioglu, T.; Orakcal, K.; and Massone, L. M., 2018, “Cyclic Lateral Load Behavior of Squat Reinforced Concrete Walls,” Engineering Structures, V. 160, pp. 147-160. doi: 10.1016/j.engstruct.2018.01.024

Vecchio, F. J., and Collins, M. P., 1986, “The Modified Compression Field Theory for Reinforced Concrete Elements Subjected to Shear,” ACI Journal Proceedings, V. 83, No. 2, Mar.-Apr., pp. 219-231.

Wallace, J. W., and Orakcal, K., 2002, “ACI 318-99 Provisions for Seismic Design of Structural Walls,” ACI Structural Journal, V. 99, No. 4, July-Aug., pp. 499-508.

Wood, S. L., 1990, “Shear Strength of Low-Rise Reinforced Concrete Walls,” ACI Structural Journal, V. 87, No. 1, Jan.-Feb., pp. 99-107.